CN209010568U - 预应力钢棒淬火、回火保温装置 - Google Patents

预应力钢棒淬火、回火保温装置 Download PDF

Info

Publication number
CN209010568U
CN209010568U CN201820257451.7U CN201820257451U CN209010568U CN 209010568 U CN209010568 U CN 209010568U CN 201820257451 U CN201820257451 U CN 201820257451U CN 209010568 U CN209010568 U CN 209010568U
Authority
CN
China
Prior art keywords
tempering
heating
temperature
furnace
steel bar
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201820257451.7U
Other languages
English (en)
Inventor
吕豫衡
李宁
朱金利
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yingkou North Metal Products Co., Ltd.
Original Assignee
Huludao Beifang Metal Product Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Huludao Beifang Metal Product Co Ltd filed Critical Huludao Beifang Metal Product Co Ltd
Priority to CN201820257451.7U priority Critical patent/CN209010568U/zh
Application granted granted Critical
Publication of CN209010568U publication Critical patent/CN209010568U/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本实用新型提供的是预应力钢棒淬火、回火保温装置。钢棒顺序通过加热炉加热,从加热炉出来后进入淬火装置进行淬火,淬火后钢棒温度降低,然后进入加热炉外保温装置中,以加热炉同等温度进行保温,此时钢棒进入到回火炉内以加热炉一半温度进行回火加热,从回火炉出来后经过回火炉外保温装置继续保温,然后利用牵拉辊将经过热处理的钢棒从生产线上拉出,成为经过热处理的预应力钢棒。由于本实用新型在加热炉和回火炉一侧设置有保温装置,所以不至于加热与回火温度迅速下降,保持足够的温度时间,防止骤冷使预应力钢棒产生内应力以及材质金相组织破坏,具有节能环保的效果。适宜作为预应力钢棒保温装置应用。

Description

预应力钢棒淬火、回火保温装置
技术领域
本实用新型提供的是机械领域使用的预应力钢棒淬火、回火保温装置。
背景技术
目前预应力钢棒淬火与回火通常在敞开的状态下进行,存在的缺点是容易造成热量大部分向环境中散发,导致被加热的钢棒应力不均,而且没有节能的效果。
实用新型内容
为了防止预应力钢棒生产过程热量的散发,本实用新型提供了预应力钢棒淬火、回火保温装置。该装置通过在加热炉和回火炉一侧设置有保温装置,解决预应力钢棒生产过程热量散发的技术问题。
本实用新型解决技术问题所采用的方案是:
钢棒顺序通过加热炉加热,从加热炉出来后进入淬火装置进行淬火,淬火后钢棒温度降低,然后进入加热炉外保温装置中,以加热炉同等温度进行保温,此时钢棒进入到回火炉内以加热炉一半温度进行回火加热,从回火炉出来后经过回火炉外保温装置继续保温,然后利用牵拉辊将经过热处理的钢棒从生产线上拉出,成为经过热处理的预应力钢棒。
所述保温装置结构:中频电流发生器输出导电线上接有超级电容,并连接中频线圈,其中超级电容和中频线圈装在加热管套内。
积极效果,由于本实用新型在加热炉和回火炉一侧设置有保温装置,所以不至于加热与回火温度迅速下降,保持足够的温度时间,防止骤冷使预应力钢棒产生内应力以及材质金相组织破坏,具有节能环保的效果。适宜作为预应力钢棒保温装置应用。
附图说明
图1为本实用新型结构构成图;
图2为本实用新型保温装置结构图。
图中,1.加热炉,1.1.淬火装置,2.加热炉外保温装置,3.回火炉,4.回火炉外保温装置,5.牵拉辊,6.中频电流发生器,6.1.加热管套,6.2.导电线,6.3.超级电容,6.4.中频线圈。
具体实施方式
据图所示:钢棒顺序通过加热炉1加热,从加热炉出来后进入淬火装置1.1进行淬火,淬火后钢棒温度降低,然后进入加热炉外保温装置2中,以加热炉同等温度进行保温,此时钢棒进入到回火炉3内以加热炉一半温度进行回火加热,从回火炉出来后经过回火炉外保温装置4继续保温,然后利用牵拉辊5将经过热处理的钢棒从生产线上拉出,成为经过热处理的预应力钢棒。
所述保温装置结构:中频电流发生器6输出导电线6.2上接有超级电容6.3,并连接中频线圈6.4,其中超级电容和中频线圈装在加热管套6.1内。
技术原理:经过表面加工的钢棒通过加热炉加热到900-950℃,当从加热炉出来后经过淬火装置进行淬火,淬火后钢棒温度降低,此时需要保温,保温使用加热炉外保温装置在900-950℃条件下保温,保温状态时,钢棒内应力消除,结构转化均质,而后进入回火炉在与加热炉一半的温度进行回火加热,回火温度450-475℃,而后进入回火炉外保温装置,以450-475℃温度条件下进行保温,保温的过程使钢棒金相组织转化为马氏体,从而使钢棒结构均匀稳定,所以适宜作预应力钢棒使用。

Claims (2)

1.预应力钢棒淬火、回火保温装置,其特征是:钢棒顺序通过的设备有加热炉(1)、淬火装置(1.1)、加热炉外保温装置(2)、回火炉(3)、回火炉外保温装置(4)和牵拉辊(5),加热炉外保温装置和回火炉外保温装置设置在加热炉和回火炉一侧。
2.根据权利要求1所述的预应力钢棒淬火、回火保温装置,其特征是:
所述保温装置:中频电流发生器(6)输出导电线(6.2)上接有超级电容(6.3),并连接中频线圈(6.4),其中超级电容和中频线圈装在加热管套(6.1)内。
CN201820257451.7U 2018-02-13 2018-02-13 预应力钢棒淬火、回火保温装置 Active CN209010568U (zh)