CN208266064U - The gradual change glass cover-plate of one type of metal - Google Patents
The gradual change glass cover-plate of one type of metal Download PDFInfo
- Publication number
- CN208266064U CN208266064U CN201820843638.5U CN201820843638U CN208266064U CN 208266064 U CN208266064 U CN 208266064U CN 201820843638 U CN201820843638 U CN 201820843638U CN 208266064 U CN208266064 U CN 208266064U
- Authority
- CN
- China
- Prior art keywords
- film
- gradual change
- plate
- site
- glass substrate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses the gradual change glass cover-plates of a type of metal, comprising: glass substrate, the glass substrate have the first surface and second surface being oppositely arranged;Gradual change site layer, is set to the first surface of the glass substrate;Metallic luster effect layer is set to the second surface of the glass substrate;Diamond-film-like is set on the metallic luster effect layer;Fingerprint proof membrane is set on the diamond-film-like.Gradual change site layer and metallic luster effect layer are provided on the glass cover-plate of the utility model, it can be realized the effect for having metallic luster gradual change by the gradual change of the size of site, keep its appearance more beautiful, also it is suitble to the aesthetic conceptions of social people now, consumer demand is preferably met, market value is huge.
Description
Technical field
The utility model relates to electronic equipment accessory technical field more particularly to the gradual change glass cover-plates of a type of metal.
Background technique
With the continuous improvement of people's living standards, the electronic products such as mobile phone, tablet computer, camera, laptop
Gradually popularize.The cover board of electronic product is mostly plastics or metal at this stage, and this single pattern cannot expire now
Pursuit of the sufficient people to fashion and individual character.Plastic cover plate and metal cover board are there is shortcomings, the wherein homogeneity of plastic cover plate
Change seriously, and is influenced for a long time using easily fading using beauty;Metal cover board is although specious, but metal has to letter
Number interference it is strong, easily scratch the disadvantages of.Interference in order to avoid metal to signal, most metals cover board product have to use
Three-stage design, design is complicated, affects its integraty and aesthetic feeling.
With the development of the electronic products such as smart phone, the style and material gradual perfection of product, material quality is also gradually
It improves, wherein glass cover-plate has many advantages, such as to the noiseless of signal, and hardness is high after tempering is liked by a large amount of consumers.But
Be existing glass cover-plate color it is single, eye appeal is not strong, it is difficult to product be made to have stronger competitiveness.
Utility model content
In order to solve above-mentioned the deficiencies in the prior art, the utility model provides the gradual change glass cover-plate of a type of metal.
Technical problem to be solved in the utility model is achieved by the following technical programs:
The gradual change glass cover-plate of one type of metal, comprising:
Glass substrate, the glass substrate have the first surface and second surface being oppositely arranged;
Gradual change site layer, is set to the first surface of the glass substrate;
Metallic luster effect layer is set to the second surface of the glass substrate;
Diamond-film-like is set on the metallic luster effect layer;
Fingerprint proof membrane is set on the diamond-film-like.
Further, the gradual change site layer is set on the glass substrate using screen printing mode.
Further, gradual change site layer includes the site of multiple gradual changes arrangement, the shape of the site be it is round or
Polygon.
Further, the size of the site is gradually increased on the first surface of the glass substrate from center to edge
Or reduce.
Further, the size of the site is incremented by or passs to the other side from a side of the first surface of the glass substrate
Subtract.
Further, the size of the site is first successively decreased from a side of the first surface of the glass substrate to the other side,
It is incremented by again.
Further, the metallic luster effect layer is made of 5-10 layers of compound film.
Further, the compound film is CuO film, TiN film, ZnO film, TiO2Film, Fe2O3Film, Nb2O5Film, Si3N4
Film, SiO2Film, Al2O3Film, MgF2Film, CaF2At least two in film.
The utility model has the following beneficial effects:
It is provided with gradual change site layer and metallic luster effect layer on the glass cover-plate of the utility model, passes through the size of site
Gradual change can be realized the effect for having metallic luster gradual change, keep its appearance more beautiful, be also suitble to examining for social people now
Beauty, preferably meets consumer demand, and market value is huge.
Detailed description of the invention
Fig. 1 is the structural schematic diagram of the utility model;
Fig. 2 is the effect picture of the utility model gradual change site layer.
In figure: 1, glass substrate, 2, metallic luster effect layer, 3, diamond-film-like, 4, fingerprint proof membrane, 5, gradual change site
Layer.
Specific embodiment
The utility model is described in detail with reference to the accompanying drawings and examples.
The gradual change glass cover-plate of one type of metal, including glass substrate, gradual change site layer, diamond-film-like, fingerprint proof membrane
With metallic luster effect layer.
The glass substrate has the first surface and second surface being oppositely arranged.Glass substrate is used in the utility model
The interference to signal of communication can be reduced, thus overcome in the prior art metal cover board to signal interference by force caused by back shroud
The problem of complex structural designs.Deck design can be structure as a whole in the utility model, moreover, without increasing anti-tampering letter
Number structure, so as to simplify the design of cover board.In addition the difficulty of processing of glass substrate is small, at low cost.
The gradual change site layer is set to the first surface of the glass substrate.Preferably, the gradual change site layer uses
Screen printing mode is set on the glass substrate.By setting gradual change site layer, so as to realize the natural gradual change of light,
It realizes fade effect, so that appearance is more beautiful, there is larger difference with the cover board of other electronic products, it is existing to avoid homogeneity
As.
The gradual change site layer includes the site of multiple gradual changes arrangement.
The shape of the site is round or polygon, naturally it is also possible to be other shapes, this is not restricted.
In the utility model, the gradual change can be surrounding gradual change, and specifically, the size of the site is in the glass base
It is gradually increased or reduces from center to edge on the first surface of plate
In the utility model, the gradual change can also be gradual change up and down, and specifically, the size of the site is from the glass
One side of the first surface of substrate is to other side increasing or decreasing.It is highly preferred that the size of the site is from the glass substrate
A side of first surface first successively decrease to the other side, then be incremented by.
The metallic luster effect layer is set to the second surface of the glass substrate, for rendering metallic luster.
In the present solution, metallic luster effect layer can be formed by coating process processing.Specifically, metallic luster effect
Layer can form the metallic luster effect layer by way of evaporation plating, sputtering plating color film layer.
The metallic luster effect layer is made of 5-10 layers of compound film.Preferably, the compound film be CuO film,
TiN film, ZnO film, TiO2Film, Fe2O3Film, Nb2O5Film, Si3N4Film, SiO2Film, Al2O3Film, MgF2Film, CaF2In film at least
Two kinds.
The thickness range of the metallic luster effect layer is 0.1 micron to 2.0 microns.
It should be noted that the thickness range suits production reality and product effect, if too thin cannot be achieved metallochrome
Pool, and it is too thick if then cost it is too high.
The diamond-film-like is set on the metallic luster effect layer.By introducing diamond-like carbon film layer, so that institute
The surface hardness for stating glass cover-plate can reach 8H or more, to increase its wearability, substantially increase the anti-scratch of the glass cover-plate
Flower ability.
Diamond-film-like can be coated with using modes such as chemical vapor deposition, physical vapour deposition (PVD)s, wherein chemistry
Vapor deposition includes but is not limited to hot-wire chemical gas-phase deposition, plasma enhanced chemical vapor deposition etc..Physical vapour deposition (PVD)
Including but not limited to magnetron sputtering, vacuum evaporation, ion plating (such as arc ion plating, RF ion plating) etc..Preferably, it adopts
The diamond-film-like, the film surface of appearance uniform densification available in this way are formed with magnetron sputtering plating mode.
Wherein, the diamond-film-like with a thickness of 1-50nm.Further, the thickness of diamond-film-like is preferably 5-
20nm.The diamond-film-like of the thickness range may make the surface hardness of the glass cover-plate to can reach 8H or more, in addition, should
The diamond-like carbon film layer of thickness range is relatively easy to be coated with, and the uniformity of film layer, consistency preferably control.
The fingerprint proof membrane is set on the diamond-film-like.Fingerprint proof membrane can reduce fingerprint and various substances in institute
Stating the attachment on glass cover-plate and attached spot can also remove easily.
It should also be noted that, herein, relational terms such as first and second and the like are used merely to one
Entity or operation are distinguished with another entity or operation, without necessarily requiring or implying between these entities or operation
There are any actual relationship or orders.Moreover, the terms "include", "comprise" or its any other variant are intended to contain
Lid non-exclusive inclusion, so that article or equipment including a series of elements not only include those elements, but also
It including other elements that are not explicitly listed, or further include for this article or the intrinsic element of equipment.Do not having
In the case where more limitations, the element that is limited by sentence "including a ...", it is not excluded that in the article including above-mentioned element
Or there is also other identical elements in equipment.
The above-mentioned embodiments merely express the embodiments of the present invention, and the description thereof is more specific and detailed, but simultaneously
Therefore it cannot be interpreted as that a limitation on the scope of the patent of the present invention, as long as using the form institute of equivalent substitution or equivalent transformation
The technical solution of acquisition, shall fall within the scope of the present invention.
Claims (9)
1. the gradual change glass cover-plate of a type of metal, comprising:
Glass substrate, the glass substrate have the first surface and second surface being oppositely arranged;
Gradual change site layer, is set to the first surface of the glass substrate;
Metallic luster effect layer is set to the second surface of the glass substrate.
2. the gradual change glass cover-plate of metalloid as described in claim 1, which is characterized in that on the metallic luster effect layer also
Equipped with diamond-film-like, fingerprint proof membrane is additionally provided on the diamond-film-like.
3. the gradual change glass cover-plate of metalloid as described in claim 1, which is characterized in that the gradual change site layer uses silk screen
Mode of printing is set on the glass substrate.
4. the gradual change glass cover-plate of metalloid as described in claim 1, which is characterized in that the gradual change site layer includes multiple
The site of gradual change arrangement, the shape of the site are round or polygon.
5. the gradual change glass cover-plate of metalloid as claimed in claim 4, which is characterized in that the size of the site is in the glass
It is gradually increased or reduces from center to edge on the first surface of glass substrate.
6. the gradual change glass cover-plate of metalloid as claimed in claim 4, which is characterized in that the size of the site is from the glass
One side of the first surface of glass substrate is to other side increasing or decreasing.
7. the gradual change glass cover-plate of metalloid as claimed in claim 4, which is characterized in that the size of the site is from the glass
One side of the first surface of glass substrate is first successively decreased to the other side, then is incremented by.
8. the gradual change glass cover-plate of metalloid as described in claim 1, which is characterized in that the metallic luster effect layer is by 5-
10 layers of compound film composition.
9. the gradual change glass cover-plate of metalloid as claimed in claim 8, which is characterized in that the compound film be CuO film,
TiN film, ZnO film, TiO2Film, Fe2O3Film, Nb2O5Film, Si3N4Film, SiO2Film, Al2O3Film, MgF2Film, CaF2In film at least
Two kinds.