CN207047083U - Glass furnace Flow-rate adjustment flashboard electric smelting tile assembly - Google Patents

Glass furnace Flow-rate adjustment flashboard electric smelting tile assembly Download PDF

Info

Publication number
CN207047083U
CN207047083U CN201720762338.XU CN201720762338U CN207047083U CN 207047083 U CN207047083 U CN 207047083U CN 201720762338 U CN201720762338 U CN 201720762338U CN 207047083 U CN207047083 U CN 207047083U
Authority
CN
China
Prior art keywords
fused cast
cast refractories
flashboard
axle
axle sleeve
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201720762338.XU
Other languages
Chinese (zh)
Inventor
褚刚
马菘
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhengzhou City Sheng Wei Fused Material Co Ltd
Original Assignee
Zhengzhou City Sheng Wei Fused Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhengzhou City Sheng Wei Fused Material Co Ltd filed Critical Zhengzhou City Sheng Wei Fused Material Co Ltd
Priority to CN201720762338.XU priority Critical patent/CN207047083U/en
Application granted granted Critical
Publication of CN207047083U publication Critical patent/CN207047083U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

Glass furnace Flow-rate adjustment flashboard electric smelting tile assembly, including flashboard fused cast refractories, pull bar and two axle sleeve fused cast refractories, flashboard fused cast refractories include square plate, the top both sides of square plate have been respectively fixedly connected with left gudgeon and auris dextra axle, left gudgeon and auris dextra axle is rotatably connected in the mounting hole on the furnace wall of both sides by axle sleeve fused cast refractories respectively, axle sleeve fused cast refractories coordinate with left gudgeon and auris dextra shaft clearance, axle sleeve fused cast refractories and the mounting hole tight fit on furnace wall, the front side surface of square plate is fixedly connected with two spaced contiguous blocks in the horizontal direction, a connecting hole is offered in two contiguous blocks in the horizontal direction, a connecting rod is equipped with two connecting holes, described pull bar one end is between two contiguous blocks and is rotatably connected in connecting rod.The utility model can control the flow that glass metal is entered in molten tin bath by runner, and axle sleeve fused cast refractories and rotary axle box only change broken parts when the utility model is safeguarded, maintenance cost is low.

Description

Glass furnace Flow-rate adjustment flashboard electric smelting tile assembly
Technical field
It the utility model is related to a kind of refractory brick, more particularly to a kind of glass furnace Flow-rate adjustment flashboard electric smelting tile assembly.
Background technology
Glass furnace is the equipment of fusion cast glass, is typically built into by refractory brick, and the damage of glass furnace kiln lining is mainly invaded with chemistry Based on erosion.In float glass, Flow-rate adjustment flashboard is the key equipment on production line, and its effect is by adjusting flashboard Aperture, the flow for controlling the glass metal melted to be entered by runner in molten tin bath, wanting for different-thickness glass product is produced to realize Ask.
But after the Flow-rate adjustment flashboard on furnace wall uses a period of time, due to frequently adjusting flashboard aperture, The rotatable connecting portion heavy wear of Flow-rate adjustment flashboard and furnace wall, while the life-span of Flow-rate adjustment flashboard and furnace wall is influenceed, because This, can be in the glass metal runner in glass furnace the utility model proposes a kind of glass furnace Flow-rate adjustment flashboard electric smelting tile assembly The rotatable connecting portion of middle use, the flow that control glass metal is entered in molten tin bath by runner, flow path adjustment flashboard and furnace wall passes through Axle sleeve fused cast refractories connect, wear-resistant, service life length.
Utility model content
The utility model is in order to solve weak point of the prior art, there is provided a kind of glass furnace Flow-rate adjustment flashboard Electric smelting tile assembly, the flow that can control glass metal to be entered by runner in molten tin bath, pass through axle between the mounting hole on gudgeon and furnace wall Fused cast refractories connection is covered, wear-resistant, service life is grown, and maintenance cost is low.
In order to solve the above technical problems, the utility model adopts the following technical scheme that:Glass furnace Flow-rate adjustment flashboard electricity Molten tile assembly, including flashboard fused cast refractories, pull bar and two axle sleeve fused cast refractories, flashboard fused cast refractories and two axle sleeve fused cast refractories are zirconium Corundum refractory brick, flashboard fused cast refractories include square plate, and the top both sides of square plate have been respectively fixedly connected with left gudgeon and auris dextra axle, Left gudgeon and auris dextra axle is rotatably connected in the mounting hole on the furnace wall of glass metal runner both sides by axle sleeve fused cast refractories respectively, axle sleeve The inwall of fused cast refractories coordinates with the outer circumference surface gap of left gudgeon and auris dextra axle, axle sleeve fused cast refractories outer wall and the installation on furnace wall Hole inwall tight fit, the front side surface of square plate are fixedly connected with two spaced contiguous blocks, two companies in the horizontal direction Connect and offer a connecting hole in block in the horizontal direction, the center line of two connecting holes overlaps, and is equipped with two connecting holes A piece connecting rod, described pull bar one end is between two contiguous blocks and is rotatably connected in connecting rod.
The pull bar both ends are respectively equipped with rotation hole and drive hole, and rotary axle box is provided with rotation hole, and pull bar passes through Rotary axle box is rotatably connected in connecting rod.
When the flashboard fused cast refractories hang naturally, the bottom of square plate contacts with the bottom surface of glass metal runner, square plate The width of width and glass metal runner matches.
Using above-mentioned technical proposal, left gudgeon and the auris dextra axle of flashboard fused cast refractories is rotatably connected on by axle sleeve fused cast refractories In mounting hole on the furnace wall of glass metal runner both sides, axle sleeve fused cast refractories can prevent from installing caused by flashboard fused cast refractories frequently rotate Hole is worn, and prevents furnace wall from damaging, and after flashboard fused cast refractories use a period of time, only need to change flashboard fused cast refractories and axle sleeve fused cast refractories It can be safeguarded, without dismantling or repairing furnace wall, reduce maintenance cost.Pull bar is rotatably connected on company by rotary axle box On extension bar, rotary axle box can prevent because pull bar pull flashboard fused cast refractories when frequently around connecting rod rotate and caused by damage, work as drawing After bar uses a period of time, only need to change rotary axle box can be safeguarded, reduce maintenance cost.Produced according to different-thickness glass The requirement of product, pull bar is pulled by external force, pull bar passes in succession through connecting rod and contiguous block drives gate rotation, flashboard fused cast refractories Rotational angle is bigger, then the aperture of flashboard fused cast refractories is bigger, and the flow that the glass metal melted is entered in molten tin bath by runner is also It is more, you can to complete the Flow-rate adjustment to glass metal in glass furnace.The drive hole set on pull bar can connect other drive devices, To be exerted a force to flashboard fused cast refractories.
To sum up, the utility model can control the flow that glass metal is entered in molten tin bath by runner, and flashboard fused cast refractories installation side Just, rotary axle box is set to cause between the axle sleeve fused cast refractories and pull bar and connecting rod that are set between the mounting hole on gudgeon and furnace wall The utility model is wear-resistant, service life length, broken parts need to be only changed when safeguarding, maintenance cost is low.
Brief description of the drawings
Fig. 1 is the dimensional structure diagram of flashboard fused cast refractories in the utility model;
Fig. 2 is the dimensional structure diagram of the utility model bottom bracket axle fused cast refractories;
Fig. 3 is scheme of installation of the present utility model;
Fig. 4 is the connection diagram of pull bar and connecting rod in the utility model.
Embodiment
As shown in Figures 1 to 4, the left-hand using Fig. 3 left side as the following content, using Fig. 3 right side to be following described The dextrad of content, glass furnace Flow-rate adjustment of the present utility model flashboard electric smelting tile assembly, including flashboard fused cast refractories, the and of pull bar 7 Two axle sleeve fused cast refractories 6, flashboard fused cast refractories and two axle sleeve fused cast refractories 6 are zirconia-corundum refractory brick, and flashboard fused cast refractories include side Shape plate 1, the top both sides of square plate 1 have been respectively fixedly connected with left gudgeon 2 and auris dextra axle 3, and left gudgeon 2 and auris dextra axle 3 lead to respectively Cross in the mounting hole 12 that axle sleeve fused cast refractories 6 are rotatably connected on glass metal runner both sides furnace wall 13, the inwall of axle sleeve fused cast refractories 6 is equal Coordinate with the outer circumference surface gap of left gudgeon 2 and auris dextra axle 3, the outer wall of axle sleeve fused cast refractories 6 and the inwall of mounting hole 12 on furnace wall 13 Tight fit, axle sleeve fused cast refractories 6 are set to prevent that mounting hole 12 wears caused by flashboard fused cast refractories frequently rotate, and prevents furnace wall 13 Damage, after flashboard fused cast refractories use a period of time, only need to change flashboard fused cast refractories and axle sleeve fused cast refractories 6 can be safeguarded, Without dismantling or repairing furnace wall 13, maintenance cost is reduced, the front side surface of square plate 1 is fixedly connected with two in the horizontal direction Spaced contiguous block 4, offers a connecting hole 5 in two contiguous blocks 4 in the horizontal direction, in two connecting holes 5 Heart line overlaps, and a connecting rod 7 is equipped with two connecting holes 5, described one end of pull bar 7 is between two contiguous blocks 4 and turns It is dynamic to be connected in connecting rod 7.
The both ends of pull bar 7 are respectively equipped with rotation hole 9 and drive hole 11, and rotary axle box 10 is provided with rotation hole 9, draw Bar 7 is rotatably connected in connecting rod 7 by rotary axle box 10.Rotary axle box 10 is set to prevent because pull bar 7 pulls flashboard electric smelting During brick frequently around connecting rod 7 rotate and caused by damage, when pull bar 7 using a period of time after, only need to change rotary axle box 10 i.e. It can be safeguarded, reduce maintenance cost.
When the flashboard fused cast refractories hang naturally, the bottom of square plate 1 contacts with the bottom surface of glass metal runner, square plate 1 The width of width and glass metal runner match.
In use, the left gudgeon 2 of flashboard fused cast refractories and auris dextra axle 3 are rotatably connected on glass metal by axle sleeve fused cast refractories 6 In mounting hole 12 on runner both sides furnace wall 13, pull bar 7 is rotatably connected in connecting rod 7 by rotary axle box 10, according to not The requirement of stack pile glass product, the aperture of flashboard fused cast refractories is adjusted, pull bar 7 is pulled by external force, pull bar 7 passes in succession through connection Bar 7 and contiguous block 4 drive gate rotation, and the rotational angle of flashboard fused cast refractories is bigger, then the aperture of flashboard fused cast refractories is bigger, fusing The flow that good glass metal is entered in molten tin bath by runner is also more, in this way, the flow to glass metal in glass furnace can be completed Regulation.
The present embodiment not makees any formal limitation, every foundation to shape of the present utility model, material, structure etc. Any simple modification, equivalent change and modification that the technical essence of the utility model is made to above example, belongs to this reality With the protection domain of new technique scheme.

Claims (3)

1. glass furnace Flow-rate adjustment flashboard electric smelting tile assembly, it is characterised in that:Including flashboard fused cast refractories, pull bar and two axle sleeves Fused cast refractories, flashboard fused cast refractories and two axle sleeve fused cast refractories are zirconia-corundum refractory brick, and flashboard fused cast refractories include square plate, square plate Top both sides be respectively fixedly connected with left gudgeon and auris dextra axle, left gudgeon and auris dextra axle passes through axle sleeve fused cast refractories and rotated respectively to be connected Be connected in the mounting hole on the furnace wall of glass metal runner both sides, the inwalls of axle sleeve fused cast refractories with left gudgeon and the excircle of auris dextra axle Face gap coordinates, axle sleeve fused cast refractories outer wall and the inner wall of the hole installing tight fit on furnace wall, the front side surface edge level side of square plate To two spaced contiguous blocks are fixedly connected with, a connecting hole is offered in two contiguous blocks in the horizontal direction, two The center line of individual connecting hole overlaps, and is equipped with a connecting rod in two connecting holes, described pull bar one end is located at two contiguous blocks Between and be rotatably connected in connecting rod.
2. glass furnace Flow-rate adjustment according to claim 1 flashboard electric smelting tile assembly, it is characterised in that:The pull bar two End is respectively equipped with rotation hole and drive hole, and rotary axle box is provided with rotation hole, and pull bar is rotatably connected on by rotary axle box In connecting rod.
3. glass furnace Flow-rate adjustment according to claim 1 flashboard electric smelting tile assembly, it is characterised in that:The flashboard electricity When molten brick hangs naturally, the bottom of square plate contacts with the bottom surface of glass metal runner, width and the glass metal runner of square plate Width matches.
CN201720762338.XU 2017-06-28 2017-06-28 Glass furnace Flow-rate adjustment flashboard electric smelting tile assembly Expired - Fee Related CN207047083U (en)