CN206487210U - Anti-corrosion concrete chimney in granite - Google Patents
Anti-corrosion concrete chimney in granite Download PDFInfo
- Publication number
- CN206487210U CN206487210U CN201720164716.4U CN201720164716U CN206487210U CN 206487210 U CN206487210 U CN 206487210U CN 201720164716 U CN201720164716 U CN 201720164716U CN 206487210 U CN206487210 U CN 206487210U
- Authority
- CN
- China
- Prior art keywords
- granite
- slabstone
- concrete chimney
- corrosion
- chimney
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Anti-corrosion concrete chimney in a kind of granite, including concrete chimney body, side is provided with granite anticorrosive coat in described concrete chimney body, described granite anticorrosive coat is rearranged by the granite slabstone of rectangle, two adjacent edges of the granite slabstone are provided with gomphosis groove, other two adjacent edge of the granite slabstone is provided with chimeric chimb, and the chimeric chimb of the granite slabstone of arranged adjacent is embedded in relative gomphosis groove and passes through the gluing docking for realizing each granite slabstone.The utility model is using corrosion-proof lining of the granite slabstone as concrete chimney, with excellent acid-alkali-corrosive-resisting performance, while the effective slabstone seam that solves easily occurs to leak and influence chimney intensity, and stone material is easy to fall off causes the problem of corrosion-proof lining fails.The utility model uses brick plate building construction different from the past, completes interior anticorrosive coat construction simultaneously during concrete chimney body moulding by casting, and short construction period, engineering cost is low, and the overall performance of concrete chimney and corrosion-proof lining is good, and intensity is high.
Description
Technical field
The utility model is related to chimney, and in particular to anti-corrosion concrete chimney in a kind of granite.
Background technology
Glass flake or fiberglass and line with rubber technique, its resistance to elevated temperatures being used the interior anti-corrosion of current concrete chimney more
Difference, the easily carbonization failure in hot environment.Have high temperature resistant and decay resistance strong as the interior anti-corrosion of chimney using titanium plate
The characteristics of, but it involves great expense.The characteristics of brick plate inside lining anti-corrosive has high temperature resistant and relatively low cost, but its brick plate seam
Easily occur leakage and influence chimney intensity, cause corrosion-proof lining to fail while brick plate is easy to fall off, brick plate liner is hindered as current
The widely used main cause of anti-corrosion.
The content of the invention
The purpose of this utility model is in view of the above-mentioned problems, improving anti-corrosion concrete chimney in a kind of granite, the flower
Anti-corrosion concrete chimney is rotten with excellent acid and alkali-resistance using corrosion-proof lining of the granite slabstone as concrete chimney in the rock of hilllock
Corrosion energy, while the effective slabstone seam that solves easily occurs to leak and influence chimney intensity, and stone material is easy to fall off causes to prevent
The problem of rotten liner fails.
Realizing the technical scheme of above-mentioned purpose is:Anti-corrosion concrete chimney in a kind of granite, including concrete chimney body,
Side is provided with granite anticorrosive coat in described concrete chimney body, and described granite anticorrosive coat is arranged by the granite slabstone of rectangle
Row composition, two adjacent edges of the granite slabstone are provided with gomphosis groove, and other two adjacent edge of the granite slabstone is provided with chimeric
Chimb, the chimeric chimb of the granite slabstone of arranged adjacent is embedded in relative gomphosis groove and realizes each granite by gluing
The docking of slabstone.
Anti-corrosion concrete chimney in above-mentioned granite, the back side of the granite slabstone it is gluing be connected with it is embedded described
Granite embedded block in concrete chimney body, the granite embedded block is rectangle slabstone of four sides in inclined-plane.
Outer reinforcement skeleton is provided with anti-corrosion concrete chimney in above-mentioned granite, described concrete chimney body and interior
Layer framework of steel reinforcement.
The beneficial effects of the utility model:
1st, using corrosion-proof lining of the granite building material as concrete chimney, with excellent acid-alkali-corrosive-resisting performance, and
By the Qian He and gluing docking of granite slabstone chimb and groove, effectively solve granite slabstone seam and easily let out
Leak and influence chimney intensity, and slabstone is easy to fall off causes the problem of corrosion-proof lining fails.
2nd, by the back side of granite slabstone it is gluing connection granite embedded block, further increase granite slabstone with
The being firmly combined with property of concrete chimney body.
The 3rd, inside and outside double steel bar skeleton is set in concrete chimney body, can be improved while reinforcing bar usage amount is reduced
The intensity of chimney.
4th, using brick plate building construction different from the past, completed simultaneously during concrete chimney body moulding by casting
Anticorrosive coat is constructed in stone material, and short construction period, engineering cost is low, and the overall performance of concrete chimney and corrosion-proof lining is good.
5th, granite anticorrosive coat of the present utility model is not only applicable to columnar structure, is equally applicable to square, trapezoidal
The internal layer anti-corrosion of uiform section body.
Brief description of the drawings
Fig. 1 is anti-corrosion concrete stack cross section schematic diagram in this granite.
Fig. 2 is the granite slabstone front view of anti-corrosion concrete chimney in this granite.
Fig. 3 is Fig. 2 top view.
Fig. 4 is the granite slabstone front view that the back side is adhesive with granite embedded block.
Fig. 5 is Fig. 4 top view.
In figure:1st, concrete chimney body;2nd, granite anticorrosive coat;3rd, granite embedded block;4th, outer reinforcement skeleton;5th, it is interior
Layer framework of steel reinforcement;21st, granite slabstone;22nd, gomphosis groove;23rd, it is fitted together to chimb.
Embodiment
Embodiment of the present utility model is illustrated with reference to the accompanying drawings and examples.
As shown in Figure 1, Figure 2 and Fig. 3, anti-corrosion concrete chimney includes concrete chimney body 1, the concrete chimney in this granite
It is provided with body 1 close to the outer reinforcement skeleton 4 of the outer surface of concrete chimney body 1 and close to the interior of the inner surface of concrete chimney body 1
Layer framework of steel reinforcement 5.The outer reinforcement skeleton 4 and internal layer framework of steel reinforcement 5 of Fig. 1 embodiments are respectively by horizontally disposed annular reinforcing bar
Constituted with the mat reinforcement cylinder that vertical reinforcing bar is combined, the inside and outside double steel bar skeleton structure is reducing the same of reinforcing bar usage amount
When can improve the intensity of chimney.Concrete chimney body 1 inwall be provided with granite anticorrosive coat 2, the granite anticorrosive coat 2 by
The granite slabstone 21 of rectangle is rearranged along the circumferential and axial of chimney, and two adjacent edges of the granite slabstone 21 are provided with chimeric
Groove 22, other two adjacent edge of the granite slabstone 21 is provided with the chimeric chimb 23 being coincide with described gomphosis groove 22, attached
Figure embodiment is the gomphosis groove 22 and chimeric chimb 23 of square-section.The chimeric chimb 23 of the granite slabstone 21 of arranged adjacent
Bonded in embedded relative gomphosis groove 22 and by adhesive glue and realize that the circumferential and axial of each granite slabstone 21 are docked.This glues
The preferred high-temperature-resistant epoxy resin glue of gum deposit.Granite has excellent acid-alkali-corrosive-resisting as the corrosion-proof lining of concrete chimney
Can, while by the Qian He and gluing docking of granite slabstone chimb and groove, granite slabstone seam can be prevented effectively from
Generation is leaked and slabstone comes off, and the service life for being used in the concrete chimney of acid and alkali corrosion fume emission is greatly improved.
The granite anticorrosive coat 2 of anti-corrosion concrete chimney is provided with embedded concrete chimney body 1 in such as Fig. 1, this granite
Granite embedded block 3, for further improving the fastness that granite anticorrosive coat 2 is combined with concrete chimney body 1.Such as Fig. 4
And Fig. 5, one granite embedded block 3 bonded by adhesive glue at the middle part at the back side of granite slabstone 21, the granite embedded block 3 is
Four sides are arranged to the rectangle granite chippings material of inside side inclined ramp.The adhesive glue bonded used in granite embedded block 3 is preferably resistance to
High temperature epoxy resinses glue.
In this granite the length of the granite slabstone 21 of anti-corrosion concrete chimney and it is wide be adapted to selection for 120mm ~ 150mm,
Thickness is 20mm ~ 30mm.The length of granite embedded block 3 and wide to be adapted to selection be that 40mm ~ 50mm, thickness are 10mm ~ 15mm.It is chimeric
The width and depth of groove 22 may be selected to be 1/3rd of the thickness of granite slabstone 21.
Claims (3)
1. anti-corrosion concrete chimney in a kind of granite, including concrete chimney body(1), it is characterized in that:Described concrete cigarette
Chimney body(1)Inner side is provided with granite anticorrosive coat(2), described granite anticorrosive coat(2)By the granite slabstone of rectangle(21)Row
Row composition, the granite slabstone(21)Two adjacent edges be provided with gomphosis groove(22), the granite slabstone(21)Other two-phase
Adjacent side is provided with chimeric chimb(23), the granite slabstone of arranged adjacent(21)Chimeric chimb(23)Embedded relative gomphosis groove
(22)It is interior and realize each granite slabstone by gluing(21)Docking.
2. anti-corrosion concrete chimney in granite according to claim 1, it is characterized in that:In the granite slabstone(21)
The back side gluing be connected with the embedded concrete chimney body(1)Interior granite embedded block(3), the granite embedded block(3)
It is in the rectangle slabstone on inclined-plane for four sides.
3. anti-corrosion concrete chimney in granite according to claim 1 or 2, it is characterized in that:Described concrete chimney
Body(1)It is interior to be provided with outer reinforcement skeleton(4)With internal layer framework of steel reinforcement(5).