CN206480516U - 石墨烯活性炭超级电容电极 - Google Patents
石墨烯活性炭超级电容电极 Download PDFInfo
- Publication number
- CN206480516U CN206480516U CN201621345697.7U CN201621345697U CN206480516U CN 206480516 U CN206480516 U CN 206480516U CN 201621345697 U CN201621345697 U CN 201621345697U CN 206480516 U CN206480516 U CN 206480516U
- Authority
- CN
- China
- Prior art keywords
- electrode
- porous
- activated carbon
- graphene
- barrier film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及电容电机技术领域,尤其是一种石墨烯活性炭超级电容电极,包括引出电极、多孔化电极、电解液存储空间和隔膜,所述引出电极作为外壳,多孔化电极作为内壳,多孔化电极内部形成电解液存储空间,电解液存储空间内设有隔膜,所述多孔化电极外层附有石墨烯层,引出电极内部设有防水膜层。所述隔膜为石墨烯、活性炭混合成型。所述防水膜层由乙炔和聚四氟乙烯混合压制而成。本实用新型可以防止石墨烯层的腐蚀,延长电极的使用寿命,增大电极的容量。
Description
技术领域
本实用新型涉及电容电机技术领域,尤其是一种石墨烯活性炭超级电容电极。
背景技术
现有的超级电容主要由电极、电解液和隔离体组成。作为电能储存元件的电极和隔离体多浸入在电解液中,长期处于电离状态,电极会在电解液的长期浸泡下发生腐蚀现象,减短使用寿命。
实用新型内容
为了克服现有的技术的不足,本实用新型提供了一种石墨烯活性炭超级电容电极。
本实用新型解决其技术问题所采用的技术方案是:一种石墨烯活性炭超级电容电极,包括引出电极、多孔化电极、电解液存储空间和隔膜,所述引出电极作为外壳,多孔化电极作为内壳,多孔化电极内部形成电解液存储空间,电解液存储空间内设有隔膜,所述多孔化电极外层附有石墨烯层,引出电极内部设有防水膜层。
根据本实用新型的另一个实施例,进一步包括,所述隔膜为石墨烯、活性炭混合成型。
根据本实用新型的另一个实施例,进一步包括,所述防水膜层由乙炔和聚四氟乙烯混合压制而成。
本实用新型的有益效果是,本实用新型可以防止石墨烯层的的腐蚀,延长电极的使用寿命,增大电极的容量。
附图说明
下面结合附图和实施例对本实用新型进一步说明。
图1是本实用新型的结构示意图;
图中1、引出电极,2、多孔化电极,3、电解液存储空间,4、隔膜,5、石墨烯层,6、防水膜层。
具体实施方式
如图1所示,一种石墨烯活性炭超级电容电极,包括引出电极1、多孔化电极2、电解液存储空间3和隔膜4,引出电极1作为外壳,多孔化电极2作为内壳,多孔化电极2内部形成电解液存储空间3,电解液存储空间3内设有隔膜4,多孔化电极2外层附有石墨烯层5,引出电极1内部设有防水膜层。
隔膜4为石墨烯、活性炭混合成型。防水膜层6由乙炔和聚四氟乙烯混合压制而成。
在使用时,外层的石墨烯层5可以扩大多孔的密度与接触面。防水膜层6可以防止电解液对电极的腐蚀,延长电极的使用寿命。隔膜4可以提高电极液的活性,扩大电容。
本实用新型可以防止石墨烯层的的腐蚀,延长电极的使用寿命,增大电极的容量。
Claims (3)
1.一种石墨烯活性炭超级电容电极,其特征是,包括引出电极(1)、多孔化电极(2)、电解液存储空间(3)和隔膜(4),所述引出电极(1)作为外壳,多孔化电极(2)作为内壳,多孔化电极(2)内部形成电解液存储空间(3),电解液存储空间(3)内设有隔膜(4),所述多孔化电极(2)外层附有石墨烯层(5),引出电极(1)内部设有防水膜层(6)。
2.根据权利要求1所述的石墨烯活性炭超级电容电极,其特征是,所述隔膜(4)为石墨烯、活性炭混合成型。
3.根据权利要求1所述的石墨烯活性炭超级电容电极,其特征是,所述防水膜层(6)由乙炔和聚四氟乙烯混合压制而成。