CN206404383U - Solution agitating device in part blind hole Ni-Speed - Google Patents

Solution agitating device in part blind hole Ni-Speed Download PDF

Info

Publication number
CN206404383U
CN206404383U CN201621471820.XU CN201621471820U CN206404383U CN 206404383 U CN206404383 U CN 206404383U CN 201621471820 U CN201621471820 U CN 201621471820U CN 206404383 U CN206404383 U CN 206404383U
Authority
CN
China
Prior art keywords
filter
blind hole
branch pipe
solution
nickel plating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201621471820.XU
Other languages
Chinese (zh)
Inventor
曹元�
李方勇
王峥
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuhan Hangda Aero Science & Technology Development Co Ltd
Original Assignee
Wuhan Hangda Aero Science & Technology Development Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuhan Hangda Aero Science & Technology Development Co Ltd filed Critical Wuhan Hangda Aero Science & Technology Development Co Ltd
Priority to CN201621471820.XU priority Critical patent/CN206404383U/en
Application granted granted Critical
Publication of CN206404383U publication Critical patent/CN206404383U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses the solution agitating device in a kind of part blind hole Ni-Speed.It includes filter, branch pipe;There is filter to be arranged on the outside of coating bath;There is nickel plating by amino sulphonate solution to be located in the coating bath, there is part to be located in the nickel plating by amino sulphonate solution;There is filter tank liquor inlet pipeline to be arranged at the filter side wall upper part, there is filter inlet valve to be arranged on the filter tank liquor inlet pipeline;There is filter tank liquor outlet conduit to be arranged at the filter lower sidewall, there is filter outlet valve to be arranged on the filter tank liquor outlet conduit;The branch pipe is arranged on the filter tank liquor outlet conduit, has branch pipe valve to be arranged on the branch pipe;There is PVC elastic hoses one end to be fixedly connected on the branch pipe, the PVC elastic hoses other end is connected to stainless steel impressed current anode upper end.Prior art gas residue generation bubble, blind hole depths root is overcome not stir dynamics, the shortcoming of pin hole can not be avoided.

Description

Solution agitating device in part blind hole Ni-Speed
Technical field
The utility model is related to ultrahigh strength steel part blind hole and repairs field, and more specifically it is part blind hole nickel plating Solution agitating device in journey.
Background technology
Undercarriage ultrahigh strength steel part is in use due to for a long time by mechanical shock and abrasion, stress corrosion etc. There is the phenomenon of overheat and corrosion in situation, local matrix, be typically mainly distributed at sealing cooperation and piston like motion stress Concentrated area, such as bushing mounting holes, inner cylinder endoporus obturage mating surface, are required according to the servicing manual of parts, these defects It must be completely removed, then size is repaired by electroplating technology, and electronickelling is primarily adapted for use in the reparation of thicker size, it is high to ensure The quality safety of strength steel, generally uses sulfamate electronickelling to obtain the coating of low stress.
There is pin hole on nickel coating is most incident defect during nickel plating by amino sulphonate, especially for for a long time Plating, it is difficult to avoid;So-called pin hole, is the pore that visually can directly be seen that, can be divided into three types according to feature:
One, matrix deficiencies
Such pin hole is non-circular shrinkage pool, is mostly because metal base surface has micropore, pit, corrosion and surface Field trash is formed;
Two, gas evolution types
The shape of pin hole is similar " tadpole ", be due to part in electroplating process as negative electrode, and cathode surface separates out hydrogen Gas, when wetting agent is inadequate, the tension force of solution becomes big, the adhesion strength of bubble becomes strong, and hydrogen is because of the buoyancy by itself, solution Stirring (being typically all upward air stirring) is floated up, but can not be shaken off, and forms pin hole, this kind of pin hole is entirely being electroplated Area distribution is more uniform;
Three, gas detention types
Pin hole is larger, generally local distribution, mostly because parts locally oil removing is not thorough enough, or because some solids suspend Thing is adsorbed on surface, causes the region hydrophobic, the gas of generation is easily detained generation pin hole;
For pin hole Producing reason, in addition to above description, also several factors:Such as plate front activating state and nickel plating is molten Metal impurities, pH value in liquid, current density, chemical composition, as long as not controlled on one side wherein having, pin hole will be produced It is raw, and for high-duty steel part obturage face for, a pin hole does not allow to exist.
Because the delay of bubble is the common cause of generation pin hole, traditional electro-nickel process and modern relatively advanced electricity Nickel plating technology is required to be reduced or avoided using two ways:One, air or mechanical agitation solution;Two, negative electrode (drive part) It is mobile, cause the bubble that piece surface is produced to be difficult to be detained by both modes, but for undercarriage heavy parts, negative electrode is moved It is dynamic to realize, even if being driven using high power large-size machine, do not reach the travel frequency of requirement, it is impossible to obtain good effect yet Really, and for deep blind hole region, mechanical agitation (bottom land uses mechanical device agitating solution) is not applied to completely, and air stirring can be with Operation, but supplement slower because solution solution outside hole is inside in blind hole, the air being passed through can aggravate the office of part inwall on the contrary The hollow phenomenon in portion, makes more gas residues produce bubble in inwall, while this mode is difficult to stir, especially blind hole Dynamics is not stirred in depths root substantially, and pin hole can not still be avoided.
The content of the invention
The purpose of this utility model is to provide the solution agitating device in a kind of part blind hole Ni-Speed, simple in construction, It is easily operated, it is adaptable to the blind hole of all size, the problem of fundamentally solving bubble residence.
To achieve these goals, the technical solution of the utility model is:Solution stirring in part blind hole Ni-Speed Device, including filter, it is characterised in that:Also include branch pipe;There is filter to be arranged on the outside of coating bath;There is nickel plating by amino sulphonate Solution is located in the coating bath, has part to be located in the nickel plating by amino sulphonate solution;There is filter tank liquor inlet pipeline to set The filter side wall upper part is placed in, has filter inlet valve to be arranged on the filter tank liquor inlet pipeline;There is filtering trough Liquid outlet conduit is arranged at the filter lower sidewall, has filter outlet valve to be arranged at the filter tank liquor outlet conduit On;The branch pipe is arranged on the filter tank liquor outlet conduit, has branch pipe valve to be arranged on the branch pipe;There are PVC bullets Property flexible pipe one end is fixedly connected on the branch pipe, and the PVC elastic hoses other end is connected to stainless steel impressed current anode upper end, The stainless steel impressed current anode top is by being fixed on the fluoroplastics anode tool locating of the part upper end;The stainless steel is auxiliary Supporing yang pole is in hollow type structure, and the stainless steel impressed current anode lower end is by fluoroplastics Seat Seal and positioned at the part Blind via bottom, the part is hung by row and hung in the coating bath;There are Small Inclined Holes to be arranged at the stainless steel impressed current anode Bottom and by inwall lead directly to outer wall, the Small Inclined Holes be located at the fluoroplastics bearing above;In the stainless steel impressed current anode The nickel plating by amino sulphonate solution in portion is flowed out by Small Inclined Holes and forms angle of inclination with part blind hole inwall tangent line.
In the above-mentioned technical solutions, nickel plating by amino sulphonate solution by Small Inclined Holes reflect outflow and with part blind hole The angle of inclination of the tangent line formation of inwall is less than 80 °.Because the sealing of stainless steel impressed current anode lower port is blocked, impressed current anode is passed through The nickel plating by amino sulphonate solution of hollow region can only lead to Small Inclined Holes, be sprayed onto part blind hole inner wall surface, amino through refraction Sulfonate nickel plating solution forces nickel plating by amino sulphonate solution in inwall quick rotation while being hit with part blind hole inwall, Simultaneously because the lasting supplement of solution causes solution to be discharged to part upper-end anode fixing tool aperture, finally cause part blind hole The tendency for rotating and constantly climbing is presented in inwall solution, so as to take away the bubble for being attached to part blind hole inwall, fundamentally solves Certainly pin hole produced problem.
Hole height, aperture, blowing angle and the quantity in hole of Small Inclined Holes are determined according to the actual conditions of product, it is adaptable to The part blind hole of all size.
The utility model has the following advantages that:
(1) nickel plating by amino sulphonate solution is delivered directly to the stainless steel used in part blind hole nickel plating by PVC hose The hollow region of impressed current anode, because the sealing of stainless steel impressed current anode lower port is blocked, nickel plating by amino sulphonate solution can only lead to Part blind hole inner wall surface is sprayed onto to Small Inclined Holes, through refraction, the oblique design of Small Inclined Holes makes the sulfamate reflected There is certain angle of inclination in nickel plating solution, amino sulphur is forced while being hit with part blind hole inwall with part blind hole inwall Hydrochlorate nickel plating solution is in inwall quick rotation and rises, and takes away the bubble for being attached to part blind hole inwall, so as to fundamentally solve Certainly pin hole produced problem;
(2) stainless steel anode is used, dissolving and the deposition of nickel dam with anode, the metallic nickel ions in blind hole region The quick supplement of reduction, iron ion increase, but nickel plating by amino sulphonate solution ensure that the quality of solution;
(3) for strong-current electroplating, the solution heating in blind hole is very fast, and nickel plating by amino sulphonate solution in time take away by supplement Enough heats, it is ensured that the temperature homogeneity of solution;
(4) filter continuous service, the nickel plating by amino sulphonate solution of branch pipe shunting continues into stainless steel impressed current anode It is flowed into inside part blind hole, is flowed out finally by the fluoroplastics fixed anode frock of part upper end, in blind hole again after portion's supplement Nickel plating by amino sulphonate solution form a kind of spiralling liquid form, it is ensured that nickel plating by amino sulphonate solution purity, Realize that bubble and suspended contamination are taken away the purpose of part blind hole in time;
(5) the utility model can be used for the nickel plating of all kinds of part blind holes to repair field, especially on undercarriage The nickel plating reparation of ultrahigh strength steel part, with extensive;The utility model is applicable not only to the plating of part blind hole groove, applies also for cup Plating (part does not descend groove, and solution i.e. electrodepositable is only filled up in blind hole, reduces shielding workload and hanging security risk, it is adaptable to Small blind hole plating on big part).
Brief description of the drawings
Fig. 1 is the utility model structural representation.
Fig. 2 is the utility model part blind hole inwall, stainless steel impressed current anode A-A to structural representation.
1- filters in figure, 2- filter tank liquor inlet pipelines, 3- filter tank liquor outlet conduits, 4- branch pipes, 5- filterings Machine inlet valve, 6- filter outlet valves, 7- branch pipe valves, 8-PVC elastic hoses, 9- stainless steel impressed current anodes, 10- parts, 11- Fluoroplastics bearing, 12- fluoroplastics fixed anode frocks, 13- Small Inclined Holes, 14- coating baths, 15- nickel plating by amino sulphonate solution, 16- part blind hole inwalls, a- angles of inclination.
Embodiment
Describe performance of the present utility model in detail below in conjunction with the accompanying drawings, but they are not constituted to of the present utility model Limit, it is only for example.Make advantage of the present utility model more clear by explanation simultaneously and be readily appreciated that.
Understood refering to accompanying drawing:Solution agitating device in part blind hole Ni-Speed, including filter, it is characterised in that: Also include branch pipe 4;There is filter 1 to be arranged at the outside of coating bath 14;There is nickel plating by amino sulphonate solution 15 to be located in the coating bath 14, There is part 10 to be located in the nickel plating by amino sulphonate solution 15;There is filter tank liquor inlet pipeline 2 to be arranged at the side of filter 1 Wall top, has filter inlet valve 5 to be arranged on the filter tank liquor inlet pipeline 2;There is filter tank liquor outlet conduit 3 to set The lower sidewall of filter 1 is placed in, has filter outlet valve 6 to be arranged on the filter tank liquor outlet conduit 3;The branch pipe 4 are arranged on the filter tank liquor outlet conduit 3, have branch pipe valve 7 to be arranged on the branch pipe 4;There are PVC elastic hoses 8 One end is fixedly connected on the branch pipe 4, and the other end of PVC elastic hoses 8 is connected to the upper end of stainless steel impressed current anode 9, institute State the top of stainless steel impressed current anode 9 and positioned by being fixed on the fluoroplastics anode frock 12 of the upper end of part 10;It is described stainless Steel impressed current anode 9 is in hollow type structure, and the lower end of stainless steel impressed current anode 9 is sealed by fluoroplastics bearing 11 and positioned at institute The blind via bottom of part 10 is stated, the part 10 is hung by row and hung in the coating bath 14;There are Small Inclined Holes 13 to be arranged at institute State the bottom of stainless steel impressed current anode 9 and outer wall is led directly to by inwall, the Small Inclined Holes 13 are located on the fluoroplastics bearing 11 Side;The nickel plating by amino sulphonate solution 15 inside the stainless steel impressed current anode 9 is flowed out by Small Inclined Holes 13 and with zero The tangent line of part blind hole inwall 16 formation angle of inclination a (as shown in Figure 1).Nickel plating by amino sulphonate solution 15 passes through the folding of Small Inclined Holes 13 Jet goes out and is less than 80 ° (as shown in Figure 2) with the angle of inclination a of the tangent line formation of part blind hole inwall 16.
The course of work of solution agitating device in part blind hole Ni-Speed described in the utility model is as follows:Plating Before, operation filter 1 is opened, nickel plating by amino sulphonate solution 15 enters branch pipe 4, branch pipe flow by filter outlet conduit 3 Individually controlled by branch pipe valve 7;Nickel plating by amino sulphonate solution 15 in branch pipe 4 is auxiliary into stainless steel along PVC elastic hoses 8 The hollow wall of supporing yang pole 9, the upper-end part of driving fluoroplastics fixed anode frock 12 of stainless steel impressed current anode 9 is fixed, and stainless steel is auxiliary The supporing yang lower port fluoroplastics bearing 11 of pole 9 sealing is blocked;Up certain altitude opens oblique small to the lower port of stainless steel impressed current anode 9 Hole 13;Nickel plating by amino sulphonate solution 15 inside stainless steel impressed current anode 9 is reflected by the inwall of Small Inclined Holes 13 to be ejected, with zero The tangent line shape of part blind hole inwall 16 is at a certain angle, is driven while collision part blind hole inwall 16 of nickel plating by amino sulphonate solution 15 Nickel plating by amino sulphonate solution 15 is set to be rotated on part blind hole inwall 16, so as to drive the amino sulphur in the whole blind hole of part 10 Hydrochlorate nickel plating solution 15 is rotated;Nickel plating by amino sulphonate solution 15 constantly enters again to after supplementing inside stainless steel impressed current anode 9 The nickel plating by amino sulphonate solution 15 entered in the blind hole of part 10, the blind hole of part 10 flows in the form of rapid spiral rises, will be attached The bubble and suspended particle impurity in part blind hole inwall 16 take away the blind hole of part 10, it is ensured that coating is uniform, smooth needleless Hole.
In order to be better described the solution agitating device in part blind hole Ni-Speed described in the utility model with it is existing Technology air or mechanical agitation solution containment are compared and had the advantage that with negative electrode (drive part) mobile device, and staff will This two kinds of technical schemes are compared, concrete outcome such as following table:
As can be known from the above table, the solution agitating device and prior art in part blind hole Ni-Speed described in the utility model Air or mechanical agitation solution containment are compared with negative electrode (drive part) mobile device, stirred great efforts, are taken away piece surface production Raw bubble effect substantially, can reach 99%.9, can fundamentally solve coating pin hole problems, it is adaptable to all size it is blind Hole, and cost is relatively low.
Other unaccounted parts belong to prior art.

Claims (2)

1. the solution agitating device in part blind hole Ni-Speed, including filter (1), it is characterised in that:Also include branch pipe (4);The filter (1) is arranged on the outside of coating bath (14);There is nickel plating by amino sulphonate solution (15) to be located at the coating bath (14) It is interior, there is part (10) to be located in the nickel plating by amino sulphonate solution (15);There is filter tank liquor inlet pipeline (2) to be arranged at institute Filter (1) side wall upper part is stated, has filter inlet valve (5) to be arranged on the filter tank liquor inlet pipeline (2);There is filter Tank liquor outlet conduit (3) is arranged at the filter (1) lower sidewall, has filter outlet valve (6) to be arranged at the filtering trough On liquid outlet conduit (3);The branch pipe (4) is arranged on the filter tank liquor outlet conduit (3), has branch pipe valve (7) to set It is placed on the branch pipe (4);There is PVC elastic hoses (8) one end to be fixedly connected on the branch pipe (4), the PVC elastic hoses (8) other end is connected to stainless steel impressed current anode (9) upper end, and stainless steel impressed current anode (9) top is described by being fixed on Fluoroplastics anode frock (12) positioning of part (10) upper end;The stainless steel impressed current anode (9) be in hollow type structure, it is described not Steel impressed current anode (9) lower end become rusty by fluoroplastics bearing (11) sealing and positioned at the blind via bottom of the part (10), described zero Part (10) is hung by row and hung in the coating bath (14);There are Small Inclined Holes (13) to be arranged at the stainless steel impressed current anode (9) Bottom and by inwall lead directly to outer wall, the Small Inclined Holes (13) be located at the fluoroplastics bearing (11) above;The stainless steel is auxiliary The internal nickel plating by amino sulphonate solution (15) of supporing yang pole (9) flowed out by Small Inclined Holes (13) and with part blind hole Wall (16) tangent line formation angle of inclination (a).
2. the solution agitating device in part blind hole Ni-Speed according to claim 1, it is characterised in that:Sulfamic acid The inclination angle that salt nickel plating solution (15) is formed by Small Inclined Holes (13) refraction outflow and with the tangent line of part blind hole inwall (16) Spend (a) and be less than 80 °.
CN201621471820.XU 2016-12-30 2016-12-30 Solution agitating device in part blind hole Ni-Speed Expired - Fee Related CN206404383U (en)