CN206204388U - 绿色高效采矿柱浸实验装置 - Google Patents
绿色高效采矿柱浸实验装置 Download PDFInfo
- Publication number
- CN206204388U CN206204388U CN201620815202.6U CN201620815202U CN206204388U CN 206204388 U CN206204388 U CN 206204388U CN 201620815202 U CN201620815202 U CN 201620815202U CN 206204388 U CN206204388 U CN 206204388U
- Authority
- CN
- China
- Prior art keywords
- leaching
- green high
- mother liquor
- efficient mining
- pond
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了绿色高效采矿柱浸实验装置,包括浸淋柱,所述浸淋柱顶部连接有注液井,底部连接有接收池,所述接收池后面依次连接有除杂池和沉淀池,所述沉淀池后面连接有过滤装置,所述过滤装置后接母液池,所述母液池通过浸矿剂回收管线连接在所述注液井上。本实用新型的优点在于:实验步骤基本还原矿上生产的整个工艺流程,根据想要的工艺参数设计实验,能快捷得到实现数据,应用在开采现场中,节省原料,提高效率;浸取完成注入清水能去除土壤中的氨氮离子,有效降低环境污染。
Description
技术领域
本实用新型涉及采矿工艺条件优化技术领域,尤其涉及采矿柱浸实验技术及其装置。
背景技术
现有的开采矿山方式是池浸、堆浸技术,生产需要大量剥离地表土壤,用化学试剂浸取出来。采取原地浸矿工艺的矿山也未对矿山进行专项的选冶工艺试验,未形成有利的开采条件。
现有技术不足和缺点:直接挖出土壤矿体会破坏山体,造成水土流失,破坏植被和生态环境,甚至严重的自然灾害,化学试剂用量大,对环境污染严重,对矿区生态环境造成毁灭性破坏。
每个矿山的开采条件和技术指标都不尽相同,开采前未确定适合的开采工艺方案,不利于浸出,无法控制开采成本,控制不了化学试剂的用量,开采后环境污染严重。
实用新型内容
本实用新型的目的在于提供绿色柱浸采矿柱浸实验装置,能够通过实验获得最合适的采矿方案,减少环境污染,提高采矿效率。
为了达到上述目的本实用新型采用如下技术方案:
绿色高效采矿注浸装置,包括浸淋柱,所述浸淋柱顶部连接有注液井,底部连接有接收池,所述接收池后面依次连接有除杂池和沉淀池,所述沉淀池后面连接有过滤装置,所述过滤装置后接母液池,所述母液池通过浸矿剂回收管线连接在所述注液井上。
进一步地,所述浸淋柱为有机玻璃制造,其上设有刻度。
进一步地,所述除杂池连接一除杂剂储罐,内装有氨水。
进一步地,所述沉淀池连接一沉淀剂储罐,内装有碳铵。
进一步地,还设有一pH调节剂罐,所述pH调节剂为硫酸,所述pH调节剂罐连通所述母液池。
进一步地,所述过滤装置包括过滤槽和抽滤装置,及依次连接在抽滤装置中滤板下方的缓冲罐、真空泵,所述抽滤装置底部和缓冲罐均设有管线连通所述母液池。
进一步地,所述浸淋柱顶部还连接有清水管。
本实用新型主要优点在于:1、实验装置能基本还原矿上生产的整个工艺流程,根据想要的工艺参数设计实验,能快捷得到实验数据,优化开采工艺条件,应用在开采现场中,减少环境污染,节省原料,提高效率;
2、设置有泵设备,免去人工转移溶液的麻烦;
3、设有真空泵抽滤,能够提高过滤效率,把液体彻底与固体分离;
4、在浸淋柱顶部设置清水管,实验结束后能够去除土壤中的氨氮离子,有效降低环境污染。
5、有刻度表的浸淋柱,方便计算矿体的参数。
附图说明
此处所说明的附图用来提供对本实用新型的进一步理解,构成本申请的一部分,并不构成对本实用新型的不当限定,在附图中:
图1是本实用新型实施例结构示意图。
具体实施方式
下面将结合附图以及具体实施例来详细说明本实用新型,在此以本实用新型的示意性实施例及说明用来解释本实用新型,但并不作为对本实用新型的限定。
如图1所示,从矿山上采集矿土样品,装入带有刻度的浸淋柱2中,把浸矿剂从浸淋柱2上部注入,在矿体内铵离子与矿土中金属阳离子发生了置换,矿体中的金属阳离子离子进入到溶液即浸矿剂中,后被下方的接收池3接收。
式中:RE3+—金属阳离子。
实际生产过程中,浸矿剂通过注液井1,在一定的水头压力下,连续不断地注入浸淋柱2内的矿体,首先浸矿剂将矿石中孔隙水和结合水排挤出来,然后浸矿剂中交换势更大的阳离子NH4 +与呈吸附态的金属阳离子发生交换,使金属阳离子进入浸出液(母液),新鲜的浸矿剂不断挤压母液,使离子交换反应不断地由矿石表面向中心发展。整个过程包括:渗透→扩散→交换→再扩散→再渗透,解吸扩散动力是浓度差,不断注入矿体中的浸矿剂(或顶水)挤出已发生交换作用的母液。当浸矿液中有足够的铵离子时,金属阳离子则能被铵离子解吸,进入母液。
接收池中的母液经压力泵泵入除杂池4中,把除杂剂储桶8中的除杂剂泵入除杂池4中,去除Al、Fe、Mn等元素,即令这些离子形成沉淀与上层的溶液分离;除杂后缓慢打开阀门放入下方的沉淀池5,在搅拌下加入沉淀剂沉淀,进一步陈化。
把陈化好的沉淀放入已经装好滤袋的过滤槽6中自然过滤,待滤液基本滴干后把滤饼转移到抽滤装置10中由真空泵12抽滤直至抽干,抽出的滤液在缓冲罐11中暂存,然后回收至母液池中,最后把抽滤后的滤饼进行干燥处理。将硫酸储罐13中的硫酸溶液加入至母液池中调节pH至3-5,作为浸矿剂泵至注液井继续使用。实验结束后,由清水管14注入清水除去柱浸土壤中的氨氮离子,降低对环境的污染。
实验过程中应当记录浸矿剂浓度、浸出时间、浸出液稀土浓度、除杂剂浓度、沉淀剂浓度、pH值、杂质浓度、沉淀量、母液稀土浓度等。
由上可知,本发明的优点在于:
1、实验装置能基本还原矿上生产的整个工艺流程,根据想要的工艺参数设计实验,能快捷得到实验数据,优化开采工艺条件,应用在开采现场中,减少环境污染,节省原料,提高效率;
2、设置有泵设备,免去人工转移溶液的麻烦;
3、设有真空泵抽滤,能够提高过滤效率,把液体彻底与固体分离;
4、在浸淋柱顶部设置清水管,实验结束后能够去除土壤中的氨氮离子,有效降低环境污染。
5、有刻度表的浸淋柱,方便计算矿体的参数。
以上对本实用新型实施例所提供的技术方案进行了详细介绍,本文中应用了具体个例对本实用新型实施例的原理以及实施方式进行了阐述,以上实施例的说明只适用于帮助理解本实用新型实施例的原理;同时,对于本领域的一般技术人员,依据本实用新型实施例,在具体实施方式以及应用范围上均会有改变之处,综上所述,本说明书内容不应理解为对本实用新型的限制。
Claims (7)
1.绿色高效采矿注浸实验装置,其特征在于:
包括浸淋柱,所述浸淋柱顶部连接有注液井,底部连接有接收池,所述接收池后面依次连接有除杂池和沉淀池,所述沉淀池后面连接有过滤装置,所述过滤装置后接母液池,所述母液池通过浸矿剂回收管线连接在所述注液井上。
2.根据权利要求1所述的绿色高效采矿注浸实验装置,其特征在于:
所述浸淋柱为有机玻璃制造,其上设有刻度。
3.根据权利要求2所述的绿色高效采矿注浸实验装置,其特征在于:
所述除杂池连接一除杂剂储罐,内装有氨水。
4.根据权利要求1所述的绿色高效采矿注浸实验装置,其特征在于:
所述沉淀池连接一沉淀剂储罐,内装有碳铵。
5.根据权利要求1所述的绿色高效采矿注浸实验装置,其特征在于:
还设有一pH调节剂罐,所述pH调节剂为硫酸,所述pH调节剂罐连通所述母液池。
6.根据权利要求1所述的绿色高效采矿注浸实验装置,其特征在于:
所述过滤装置包括过滤槽和抽滤装置,及依次连接在抽滤装置中滤板下方的缓冲罐、真空泵,所述抽滤装置底部和缓冲罐均设有管线连通所述母液池。
7.根据权利要求1所述的绿色高效采矿注浸实验装置,其特征在于:
所述浸淋柱顶部还连接有清水管。