- CN205465036U CN205465036U CN201620014693.4U CN201620014693U CN205465036U CN 205465036 U CN205465036 U CN 205465036U CN 201620014693 U CN201620014693 U CN 201620014693U CN 205465036 U CN205465036 U CN 205465036U
- Authority
- CN
- China
- Prior art keywords
- steel pipe
- welding
- additional
- submerged arc
- main steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Arc Welding In General (AREA)
Abstract
本实用新型属于螺旋焊管埋弧焊接钢管封口焊接结构的改进,特别是一种埋弧焊接钢管封口的焊接结构,包括主钢管和与主钢管端口相配合的封头侧板,在封头侧板的外侧配合安装着加装钢管,加装钢管的直径与主钢管的直径相等,加装钢管的长度为40-60mm,焊接枪嘴和焊丝直对主钢管与封头侧板之间的焊缝,焊剂设置在封头侧板、主钢管和加装钢管上。本实用新型结构合理,焊剂可以有效覆盖焊道,焊道成型好,保证焊接质量,可以减少焊剂浪费,降低焊接费用。
Description
技术领域
本实用新型属于螺旋焊管埋弧焊接钢管封口焊接结构的改进,特别是一种埋弧焊接钢管封口的焊接结构。
背景技术
在螺旋焊管生产企业中,焊管焊接采用自动埋弧焊焊接技术,自动埋弧焊接技术焊接质量好,焊缝强度大,埋弧焊焊接技术在螺旋焊管生产中各项工艺参数成熟。市场上常见的蓄水罐本体为卷筒机卷圆筒,焊缝为直缝,承压不及螺旋焊管,且直缝蓄水罐受卷筒机设备及板材宽度影响,罐体长度受限,长度过长就需对接,管端封口焊接一般采用CO2气体保护焊。
蓄水罐制作过程中端头密封采用埋弧焊焊接,而埋弧焊焊接过程中最主要的是利用焊剂将焊接熔池覆盖,焊剂对焊接熔池覆盖的好坏直接影响焊接质量。螺旋焊管生产过程中无论是板带头尾对接还是成型焊接,都能很好的承载焊剂,从而保护熔池,保证焊接质量。
在钢管端头密封焊接过程中,焊道据钢管封头端面较近,焊剂撒在焊道上后大部分顺着钢管封头端面流失,无法有效覆盖焊道,一方面在焊接过程中造成明弧,另一方面焊接后铁水容易流失,焊道成型差,焊接质量差。
实用新型内容
本实用新型的目的在于提供一种埋弧焊接钢管封口的焊接结构,其结构合理,焊剂可以有效覆盖焊道,焊道成型好,保证焊接质量,可以减少焊剂浪费,降低焊接费用。
本实用新型的目的是这样实现的:一种埋弧焊接钢管封口的焊接结构,包括主钢管和与主钢管端口相配合的封头侧板,在封头侧板的外侧配合安装着加装钢管,加装钢管的直径与主钢管的直径相等,加装钢管的长度为40-60mm,焊接枪嘴和焊丝直对主钢管与封头侧板之间的焊缝,焊剂设置在封头侧板、主钢管和加装钢管上。
本实用新型的主要实施方式:
1、对钢管端头进行平头处理,在平头时下料50mm长钢管。
2、钢管封头侧板下料,在下料时可先下比所需侧板直径大30mm的圆盘,圆盘下好后紧贴钢管端头点焊固定,根据钢管圆度对侧板进行仿形切割,使侧板与钢管端头匹配。
3、将前期平头下料50mm长钢管固定于钢管封头侧板,可采用点焊固定、磁铁固定等多种固定模式。
4、调整焊点及焊接工艺参数进行焊接。
本实用新型结构合理,实现了焊剂有效覆盖焊道,焊道成型好,保证了焊接质量,减少了焊剂浪费,降低了焊接费用。
附图说明
下面将结合附图对本实用新型做进一步的描述,图1为本实用新型剖视结构示意图。
具体实施方式
一种埋弧焊接钢管封口的焊接结构,如图1所示, 包括主钢管1和与主钢管1端口相配合的封头侧板5,在封头侧板5的外侧配合安装着加装钢管6,加装钢管6的直径与主钢管1的直径相等,加装钢管6的长度为40-60mm,焊接枪嘴3和焊丝2直对主钢管1与封头侧板5之间的焊缝,焊剂4设置在封头侧板5、主钢管1和加装钢管6上。
Claims (1)
1.一种埋弧焊接钢管封口的焊接结构,包括主钢管(1)和与主钢管(1)端口相配合的封头侧板(5),其特征是:在封头侧板(5)的外侧配合安装着加装钢管(6),加装钢管(6)的直径与主钢管(1)的直径相等,加装钢管(6)的长度为40-60mm,焊接枪嘴(3)和焊丝(2)直对主钢管(1)与封头侧板(5)之间的焊缝,焊剂(4)设置在封头侧板(5)、主钢管(1)和加装钢管(6)上。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201620014693.4U CN205465036U (zh) | 2016-01-08 | 2016-01-08 | 埋弧焊接钢管封口的焊接结构 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201620014693.4U CN205465036U (zh) | 2016-01-08 | 2016-01-08 | 埋弧焊接钢管封口的焊接结构 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN205465036U true CN205465036U (zh) | 2016-08-17 |
Family
ID=56664251
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201620014693.4U Expired - Fee Related CN205465036U (zh) | 2016-01-08 | 2016-01-08 | 埋弧焊接钢管封口的焊接结构 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN205465036U (zh) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN106624292A (zh) * | 2016-11-25 | 2017-05-10 | 中国海洋石油总公司 | 组块及模块化工厂节点盖板的焊接工艺 |
-
2016
- 2016-01-08 CN CN201620014693.4U patent/CN205465036U/zh not_active Expired - Fee Related
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN106624292A (zh) * | 2016-11-25 | 2017-05-10 | 中国海洋石油总公司 | 组块及模块化工厂节点盖板的焊接工艺 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN103264209A (zh) | 不锈钢焊件的组合焊接方法 | |
CN103612001B (zh) | 一种基于r形坡口的双金属复合管管端封焊工艺 | |
CN104889527A (zh) | 一种管线钢制管焊接工艺 | |
CN110576245A (zh) | 双相不锈钢管道环焊缝全自动氩弧焊接方法 | |
CN105983755A (zh) | 长输管道封闭连接堆焊免补口方法 | |
CN205465036U (zh) | 埋弧焊接钢管封口的焊接结构 | |
CN208644343U (zh) | 一种无气体保护金属管对接焊结构 | |
CN108213663A (zh) | 大厚度筒体与接管的全焊透焊接方法 | |
CN105710549A (zh) | 一种变压器用风冷却器不锈钢冷却管和管板焊接工艺 | |
CN106944725B (zh) | 一种局部干法水下气体保护焊焊枪喷嘴 | |
CN204673127U (zh) | 一种采用水溶性纸保护膜的气体保护焊结构 | |
CN102513657A (zh) | 一种适用管体焊接的氩弧焊焊接方法及该方法使用的辅助装置 | |
CN205008806U (zh) | 用于圆管钢柱精确对焊的内衬管 | |
CN106624274A (zh) | 一种钢管与法兰焊接方法 | |
CN203585612U (zh) | 一种双金属复合管窄间隙对接焊坡口 | |
CN107676520A (zh) | 全焊接管线球阀阀体及其焊接装配工艺 | |
CN103418899A (zh) | 一种用于管道内部打底焊接的等离子焊机 | |
CN107297558A (zh) | 一种耐蚀合金复合弯头堆焊工艺 | |
CN208132176U (zh) | 一种用于氩弧焊的氩气保护装置 | |
CN207394181U (zh) | 一种可以调节长度的带内衬管道接头 | |
CN202356775U (zh) | 管体氩弧焊焊接辅助装置 | |
CN203304743U (zh) | 采用co2气体保护焊的大直径法兰堆焊设备 | |
CN105618901A (zh) | 一种管道焊接用左挡板及气体保护装置和焊接工装 | |
CN207377687U (zh) | 一种高压油管端部焊接结构 | |
CN104625553A (zh) | 一种用于调整焊口组对错边量的工具 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C14 | Grant of patent or utility model | ||
GR01 | Patent grant | ||
CF01 | Termination of patent right due to non-payment of annual fee |
Granted publication date: 20160817 Termination date: 20170108 |
|
CF01 | Termination of patent right due to non-payment of annual fee |