Prior art keywords
core
ceramic core
hole
centre bore
ceramic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201521064655.1U
Other languages
English (en)
Inventor
郭光�
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shaanxi Mingchen Precision Casting Industry Co.,Ltd.
Original Assignee
Sanyuan Guangda Precision Casting Factory
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sanyuan Guangda Precision Casting Factory filed Critical Sanyuan Guangda Precision Casting Factory
Priority to CN201521064655.1U priority Critical patent/CN205341823U/zh
Application granted granted Critical
Publication of CN205341823U publication Critical patent/CN205341823U/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Molds, Cores, And Manufacturing Methods Thereof (AREA)

Abstract

本实用新型涉及一种精铸用透气陶瓷型芯,其包括:具有内部空腔的陶瓷型芯,设置于陶瓷型芯两端的榫头,设置于榫头中心位置的中心孔,设置于陶瓷型芯的表面上并与陶瓷型芯内部空腔相连通的至少一个芯孔,以及设置于芯孔上的多孔陶瓷芯盖。本实用新型通过在设置芯孔上的多孔陶瓷芯盖,浇筑时气体会通过多孔陶瓷盖上的孔排到内部空腔,再从内部空腔排到中心孔,最后通过中心孔排到大气中,从而避免了铸件气孔的产生,使除芯缩短了一半以后的时间;节约了陶瓷型芯的材料用量;使型壳焙烧的时间缩短,节约了能源。

Description

一种精铸用透气陶瓷型芯
技术领域
本实用新型涉及一种精铸用透气陶瓷型芯。
背景技术
在精密铸造领域,对于较大的铸件在使用陶瓷型芯的时候,总是出现铸件表面产生气孔的问题,从而影响使用性能和外观,导致废品的产生。
一般的陶瓷型芯透气性极低,甚至几乎没有,而为了提高陶瓷型芯的常温强度及高温强度又不能整体做出多孔海绵体状,因此需要对现有的陶瓷型芯进行改进。
实用新型内容
为了克服现有精铸用陶瓷型芯的不足,本实用新型的目的是提供一种精铸用透气陶瓷型芯,不仅能克服在使用现有精铸用陶瓷型芯的时候容易在铸件表面产生气孔的问题,同时避免了将陶瓷型芯柱面整体做成多孔海绵体状而降低了陶瓷型芯强度的问题。
为实现上述技术目的,本实用新型采用如下技术方案予以实现。
一种精铸用透气陶瓷型芯,包括:具有内部空腔的陶瓷型芯,设置于陶瓷型芯两端的榫头,设置于榫头中心位置的中心孔,设置于陶瓷型芯的表面上并与陶瓷型芯内部空腔相连通的至少一个芯孔,以及设置于芯孔上的多孔陶瓷芯盖。
作为优选的,所述中心孔的一端与陶瓷型芯内部空腔相连通,另一端与大气相连通的通孔。
作为优选的,所述的设置于芯孔上的多孔陶瓷芯盖上的孔均为通孔。
本实用新型的有益效果为:本实用新型通过在设置芯孔上的多孔陶瓷芯盖,浇筑时气体会通过多孔陶瓷盖上的孔排到内部空腔,再从内部空腔排到中心孔,最后通过中心孔排到大气中,从而避免了铸件气孔的产生,使除芯缩短了一半以后的时间;节约了陶瓷型芯的材料用量;使型壳焙烧的时间缩短,节约了能源。
附图说明
图1为本实用新型的结构示意图;
图中:1-榫头;2-多孔陶瓷芯盖;3-陶瓷型芯;4-中心孔;5-柱体表面;6-内部空腔。
具体实施方式
下面结合附图对本实用新型作进一步说明:
一种精铸用透气陶瓷型芯,包括:具有内部空腔6的陶瓷型芯3,设置于陶瓷型芯3两端的榫头1,设置于榫头1中心位置的中心孔4,设置于陶瓷型芯3柱体表面5上并与陶瓷型芯3内部空腔6相连通的至少一个芯孔7和设置于芯孔7上的多孔陶瓷芯盖2。
所述的设置于榫头1中心位置的中心孔4为一端与陶瓷型芯3内部空腔6相连通,另一端与大气相连通的通孔。多孔陶瓷芯盖2上的孔均为通孔。
本实用新型的使用方法:在芯孔7上用多孔陶瓷芯盖2覆盖,然后放入焙烧炉焙烧(1200℃)1~2小时,后随炉冷却到常温备用,将陶瓷型芯3装入模具中压制蜡型,在涂料前应将榫头1两端的中心孔4用蜡堵上,在制壳完成脱蜡前将两端涂料层去除(切除,磨除),然后再脱蜡,型壳正常焙烧浇筑即可。浇筑时气体会通过多孔陶瓷盖2上的孔排到内部空腔6,再从内部空腔6排到中心孔4,最后通过中心孔4排到大气中,从而避免了铸件气孔的产生。
显然,本领域的技术人员可以对本实用新型进行各种改动和变型而不脱离本实用新型的精神和范围。这样,倘若本实用新型的这些修改和变型属于本实用新型权利要求及其等同技术的范围之内,则本实用新型也意图包含这些改动和变型在内。

Claims (3)

1.一种精铸用透气陶瓷型芯,其特征在于,包括:具有内部空腔的陶瓷型芯,设置于陶瓷型芯两端的榫头,设置于榫头中心位置的中心孔,设置于陶瓷型芯的表面上并与陶瓷型芯内部空腔相连通的至少一个芯孔,以及设置于芯孔上的多孔陶瓷芯盖。
2.根据权利要求1所述的一种精铸用透气陶瓷型芯,其特征在于,所述中心孔的一端与陶瓷型芯内部空腔相连通,另一端与大气相连通的通孔。
3.根据权利要求1所述的一种精铸用透气陶瓷型芯,其特征在于,所述的设置于芯孔上的多孔陶瓷芯盖上的孔均为通孔。
CN201521064655.1U 2015-12-18 2015-12-18 一种精铸用透气陶瓷型芯 Active CN205341823U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201521064655.1U CN205341823U (zh) 2015-12-18 2015-12-18 一种精铸用透气陶瓷型芯

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201521064655.1U CN205341823U (zh) 2015-12-18 2015-12-18 一种精铸用透气陶瓷型芯

Publications (1)

Publication Number Publication Date
CN205341823U true CN205341823U (zh) 2016-06-29

Family

ID=56169746

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201521064655.1U Active CN205341823U (zh) 2015-12-18 2015-12-18 一种精铸用透气陶瓷型芯

Country Status (1)

Country Link
CN (1) CN205341823U (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108080575A (zh) * 2016-11-23 2018-05-29 中国科学院金属研究所 一种硅基陶瓷型芯的固定方法

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108080575A (zh) * 2016-11-23 2018-05-29 中国科学院金属研究所 一种硅基陶瓷型芯的固定方法
CN108080575B (zh) * 2016-11-23 2019-12-03 中国科学院金属研究所 一种硅基陶瓷型芯的固定方法

Similar Documents

Publication Publication Date Title
CN104907492B (zh) 一种面向双层壁空心涡轮叶片的制造方法
CN203737936U (zh) 纤维增强熔模铸造复合型壳
CN105855468A (zh) 陶瓷型壳制备方法及制备透平叶片的陶瓷型壳的制造方法
CN105834363B (zh) 一种低压失蜡精密铸造系统
CN105127374B (zh) 一种钛及钛合金铸造用复合型芯及其制备方法
CN104399882B (zh) 采用v法铸造工艺生产箱体类铝合金铸件的二次造型方法
CN104128561A (zh) 一种耐热钢带孔篦板消失模铸造方法
CN110143819A (zh) 一种复杂陶瓷结构件的间接自由成型方法
CN109530630A (zh) 一种五辐轮毂铸型及五辐轮毂制造方法
CN205732814U (zh) 一种熔模铸造用的浇注系统蜡模
CN205341823U (zh) 一种精铸用透气陶瓷型芯
CN110640085A (zh) 一种空心铸件熔模铸造工艺
CN202207774U (zh) 浇铸细长孔铸件的熔模型壳
CN104741530A (zh) 复杂零件快速精密铸造方法
CN102601305B (zh) 实体制壳熔模铸造方法
CN102380581A (zh) 一种壳体铸件芯撑间隔层叠多组芯工艺方法
CN105945258B (zh) 一种低压熔模精密铸造工艺
CN103639396A (zh) 利用陶瓷型制备金属钛及钛合金铸件的方法
CN204430192U (zh) 增强铸件冒口补缩能力的冒口油砂芯组件
CN104513056A (zh) 钧瓷的生产方法
CN101716649A (zh) 基于光固化快速成型的消失法砂型铸造工艺
CN101733816B (zh) 一种异形匣钵的制作方法、异形匣钵及异形陶瓷
CN107030256A (zh) 一种金属器物的精密铸造方法
CN208555911U (zh) 一种真空干砂造型砂箱
CN108297242A (zh) 陶瓷坯料注塑制品及其烧结方法、陶瓷坯料注塑模具

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
TR01 Transfer of patent right

Effective date of registration: 20210827

Address after: 713804 room 02, southwest, first floor, Sanyuan Everbright Precision Foundry, east section of metallurgical Avenue, Xianyang City, Shaanxi Province

Patentee after: Shaanxi Mingchen Precision Casting Industry Co.,Ltd.

Address before: 713800 eastern section of metallurgical Road, Sanyuan County, Xianyang, Shaanxi

Patentee before: SANYUAN GUANGDA PRECISION CASTING FACTORY

TR01 Transfer of patent right