- Prior art keywords
- plate
- wood
- block
- flattening
- long
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
- 239000002023 wood Substances 0.000 title claims abstract description 105
- 235000017166 Bambusa arundinacea Nutrition 0.000 title claims abstract description 104
- 235000017491 Bambusa tulda Nutrition 0.000 title claims abstract description 104
- 241001330002 Bambuseae Species 0.000 title claims abstract description 104
- 235000015334 Phyllostachys viridis Nutrition 0.000 title claims abstract description 104
- 239000011425 bamboo Substances 0.000 title claims abstract description 104
- 239000011120 plywood Substances 0.000 title abstract description 4
- 150000001875 compounds Chemical class 0.000 title abstract 3
- -1 phenolic aldehyde Chemical class 0.000 claims abstract description 18
- 239000002131 composite material Substances 0.000 claims description 23
- 239000003292 glue Substances 0.000 claims description 18
- 238000007731 hot pressing Methods 0.000 claims description 13
- 239000005011 phenolic resin Substances 0.000 claims description 6
- 229920001568 phenolic resin Polymers 0.000 claims description 6
- 238000001035 drying Methods 0.000 claims description 5
- KXGFMDJXCMQABM-UHFFFAOYSA-N 2-methoxy-6-methylphenol Chemical compound [CH]OC1=CC=CC([CH])=C1O KXGFMDJXCMQABM-UHFFFAOYSA-N 0.000 claims description 3
- 238000007598 dipping method Methods 0.000 claims description 3
- 210000002489 tectorial membrane Anatomy 0.000 abstract 1
- 238000004519 manufacturing process Methods 0.000 description 9
- 230000008676 import Effects 0.000 description 8
- 230000005587 bubbling Effects 0.000 description 5
- 238000005470 impregnation Methods 0.000 description 5
- 230000006835 compression Effects 0.000 description 3
- 238000007906 compression Methods 0.000 description 3
- 230000002950 deficient Effects 0.000 description 3
- 238000005516 engineering process Methods 0.000 description 3
- 238000005187 foaming Methods 0.000 description 3
- 238000004026 adhesive bonding Methods 0.000 description 2
- 239000000463 material Substances 0.000 description 2
- 239000002994 raw material Substances 0.000 description 2
- 238000003854 Surface Print Methods 0.000 description 1
- 238000010411 cooking Methods 0.000 description 1
- 230000007547 defect Effects 0.000 description 1
- 238000010586 diagram Methods 0.000 description 1
- 238000007688 edging Methods 0.000 description 1
- 230000000694 effects Effects 0.000 description 1
- 230000007613 environmental effect Effects 0.000 description 1
- 238000005304 joining Methods 0.000 description 1
- 238000012856 packing Methods 0.000 description 1
Abstract
The utility model discloses a compound container of flattening -out bamboo wood plywood for bottom plate, flattening -out bamboo clapper, bamboo screen or curtain brachymedial board in phenolic aldehyde tectorial membrane paper, the long medium plate of wood, wooden brachymedial board, length, follow between the terminal surface under and at this up end the up end has set gradually the long medium plate of first piece wood in the orientation of lower terminal surface, the wooden brachymedial board of first piece, flattening -out bamboo clapper in the first block length, the long medium plate of second piece wood, first piece bamboo screen or curtain brachymedial board, the long medium plate of third piece wood, second piece wood brachymedial board, the long medium plate of fourth piece wood, flattening -out bamboo clapper in the second block length, the 5th long medium plate of wood, third piece wood brachymedial board, the 6th long medium plate of wood, second piece bamboo screen or curtain brachymedial board, the 7th long medium plate of wood, flattening -out bamboo clapper in the third block length, fourth piece wood brachymedial board and the 8th long medium plate of wood. The utility model discloses compound container of flattening -out bamboo wood plywood for bottom plate intensity is high, long service life.
Description
Technical field
The utility model relates to technical field of board processing, particularly relates to a kind of flattening-out bamboo wood composite container baseboard glued board.
Background technology
Existing plate of joining used for bottom plate of container is full bamboo mat structure or bamboo-wood structure, and these two kinds of structural plywood production technologies are loaded down with trivial details, and glue quantity is large, need impregnation, and to material moisture content require too high, production board is yielding, bubbling, layering, floor strength is not high, and service life is not long.
Utility model content
Based on this, be necessary for prior art defect, provide that intensity is high, the flattening-out bamboo wood composite container baseboard glued board of long service life and production technology thereof.
Its technical scheme is as follows.
A kind of flattening-out bamboo wood composite container baseboard glued board, comprise phenolic aldehyde tectorial paper, wood long in plate, wooden brachymedial plate, long in flattening-out bamboo clappers, bamboo curtain splint brachymedial plate, its upper surface is provided with the first phenolic aldehyde tectorial paper, and lower surface is provided with Ah must, and plate or flattening-out bamboo stay blue or green panel in the east, on the direction of lower surface, be disposed with plate in first piece of wood length along described upper surface between this upper surface and lower surface, first block of wooden brachymedial plate, flattening-out bamboo clappers in first block length, plate during second block of wood is long, first block of bamboo curtain splint brachymedial plate, plate during 3rd block of wood is long, second block of wooden brachymedial plate, plate during 4th block of wood is long, flattening-out bamboo clappers in second block length, plate during 5th block of wood is long, 3rd block of wooden brachymedial plate, plate during 6th block of wood is long, second block of bamboo curtain splint brachymedial plate, plate during 7th block of wood is long, flattening-out bamboo clappers in 3rd block length, 4th block of wooden brachymedial plate and the 8th block of wood long in plate.
Rational in infrastructure, the impregnation operation of the technical program flattening-out bamboo wood composite container baseboard glued board new product is simple and save glue, Functionality, quality and appealing design, intensity is high, good springiness, panel and base plate are all indeformable, surface is non-foaming, anti-pressure ability is strong, cost is low, the life-span is long, applied range, both can be applicable to container, can be applicable to again the various aspects such as door and window, furniture, automobile, vessel, both effectively range of application can be expanded, effectively can reduce again the import of container plate, also can effectively reduce cost.Plate during wooden brachymedial plate in its structure, wood are long, not only can use import weedtree, but also can apply domestic weedtree, not only convenient, but also the import of corresponding minimizing raw material of selection.
Below the technical program is further described:
Wherein in an embodiment, described first phenolic aldehyde tectorial paper, Ah must in the east plate or flattening-out bamboo stays blue or green panel, plate during first block of wood is long, first block of wooden brachymedial plate, flattening-out bamboo clappers in first block length, plate during second block of wood is long, first block of bamboo curtain splint brachymedial plate, plate during 3rd block of wood is long, second block of wooden brachymedial plate, plate during 4th block of wood is long, flattening-out bamboo clappers in second block length, plate during 5th block of wood is long, 3rd block of wooden brachymedial plate, plate during 6th block of wood is long, second block of bamboo curtain splint brachymedial plate, plate during 7th block of wood is long, flattening-out bamboo clappers in 3rd block length, 4th block of wooden brachymedial plate and the 8th block of wood long in glue coated between plate, be interconnected by hot pressing.
Wherein in an embodiment, described glue is phenolic resins, and its glue-spread is every square metre of two-sided 380g-420g, and it is coated on the both sides of flattening-out bamboo clappers, bamboo curtain splint brachymedial plate in plate, wooden brachymedial plate, length in wood length by glue spreader.
Wherein in an embodiment, during described hot pressing, the temperature of hot press is 125-150 DEG C, the pressure of hot pressing is 2.0-4.0mpa/cm
2, hot pressing time be 50-70min.
Wherein in an embodiment, plate during described phenolic aldehyde tectorial paper, wood are long, wooden brachymedial plate, long in flattening-out bamboo clappers, be laminated structure, bamboo curtain splint brachymedial plate is horizontal bamboo curtain splint structure.
Wherein in an embodiment, the width of flattening-out bamboo wood composite container baseboard glued board is 600-1300mm, length is 1000-2500mm, thickness is 18-35mm.
Wherein in an embodiment, plate during described wood is long, wooden brachymedial plate, long in the thickness of flattening-out bamboo clappers is 4.0-6.0mm, the thickness of bamboo curtain splint brachymedial plate is 1.0-2.5mm.
Wherein in an embodiment, described phenolic aldehyde tectorial paper is paper is put into phenolic resin glue drying after dipping to make.
Accompanying drawing explanation
Fig. 1 is the structural representation of flattening-out bamboo wood composite container baseboard glued board described in the utility model embodiment;
Fig. 2 is the manufacturing process flow diagram of flattening-out bamboo wood composite container baseboard glued board described in the utility model embodiment;
Description of reference numerals:
10, phenolic aldehyde tectorial paper, 20, wood long in plate, 30, wooden brachymedial plate, 40, long in flattening-out bamboo clappers, 50, bamboo curtain splint brachymedial plate.
Detailed description of the invention
Below in conjunction with accompanying drawing, the utility model embodiment is described in detail.
Refer to Fig. 1, flattening-out bamboo wood composite container baseboard glued board comprise phenolic aldehyde tectorial paper 10, wood long in plate 20, wooden brachymedial plate 30, long in flattening-out bamboo clappers 40, bamboo curtain splint brachymedial plate 50.The upper surface of flattening-out bamboo wood composite container baseboard glued board is provided with the first phenolic aldehyde tectorial paper 10, and lower surface is provided with Ah must, and plate or flattening-out bamboo stay blue or green panel in the east.On the direction of lower surface, be disposed with plate 20 in first piece of wood length along described upper surface between this upper surface and lower surface, first block of wooden brachymedial plate 30, flattening-out bamboo clappers 40 in first block length, plate 20 during second block of wood is long, first block of bamboo curtain splint brachymedial plate 50, plate 20 during 3rd block of wood is long, second block of wooden brachymedial plate 30, plate 20 during 4th block of wood is long, flattening-out bamboo clappers 40 in second block length, plate 20 during 5th block of wood is long, 3rd block of wooden brachymedial plate 30, plate 20 during 6th block of wood is long, second block of bamboo curtain splint brachymedial plate 50, plate 20 during 7th block of wood is long, flattening-out bamboo clappers 40 in 3rd block length, 4th block of wooden brachymedial plate 30 and the 8th block of wood long in plate 20.Ah must in the east plate, by A Bidong timber (a kind of imported log is also known as clone's wood), through being peeled into the thick veneer of 1-1.5mm, can do container table deck panels.Flattening-out bamboo stays blue or green panel to be flattening-out bamboo stays blue or green one side.
Rational in infrastructure, the impregnation operation of the technical program flattening-out bamboo wood composite container baseboard glued board new product is simple and save glue, Functionality, quality and appealing design, intensity is high, good springiness, panel and base plate are all indeformable, surface is non-foaming, anti-pressure ability is strong, cost is low, the life-span is long, applied range, both can be applicable to container, can be applicable to again the various aspects such as door and window, furniture, automobile, vessel, both effectively range of application can be expanded, effectively can reduce again the import of container plate, also can effectively reduce cost.Plate 20 during wooden brachymedial plate 30 in its structure, wood are long, not only can use import weedtree, but also can apply domestic weedtree, not only convenient, but also the import of corresponding minimizing raw material of selection.Significantly reduce production board yielding, layering, the phenomenon of bubbling, compression strength and elastic modelling quantity add 10%-30%, increase the service life, and decrease defective products and the cost of product, improve quality.
Described first phenolic aldehyde tectorial paper 10, Ah must in the east plate or flattening-out bamboo stays blue or green panel, plate 20 during first block of wood is long, first block of wooden brachymedial plate 30, flattening-out bamboo clappers 40 in first block length, plate 20 during second block of wood is long, first block of bamboo curtain splint brachymedial plate 50, plate 20 during 3rd block of wood is long, second block of wooden brachymedial plate 30, plate 20 during 4th block of wood is long, flattening-out bamboo clappers 40 in second block length, plate 20 during 5th block of wood is long, 3rd block of wooden brachymedial plate 30, plate 20 during 6th block of wood is long, second block of bamboo curtain splint brachymedial plate 50, plate 20 during 7th block of wood is long, flattening-out bamboo clappers 40 in 3rd block length, 4th block of wooden brachymedial plate 30 and the 8th block of wood long in glue coated between plate 20, be interconnected by hot pressing.Described glue is phenolic resins, and its glue-spread is every square metre of two-sided 380g-420g, and it is coated on the both sides of flattening-out bamboo clappers 40, bamboo curtain splint brachymedial plate 50 in plate 20, wooden brachymedial plate 30, length in wood length by glue spreader.
Use glue spreader gluing, decrease the use amount of glue and eliminate the loaded down with trivial details operation of impregnation, suitably improve the moisture content of veneer, reduce drying cost.Significantly reduce production board yielding, layering, the phenomenon of bubbling, compression strength and elastic modelling quantity add 10%-30%, increase the service life, and decrease defective products and the cost of product, improve quality.
During described hot pressing, the temperature of hot press is 125-150 DEG C, the pressure of hot pressing is 2.0-4.0mpa/cm
2, hot pressing time be 50-70min.Adopt that hot-forming to significantly reduce production board yielding, layering, the phenomenon of bubbling.Plate 20 during described phenolic aldehyde tectorial paper 10, wood are long, wooden brachymedial plate 30, long in flattening-out bamboo clappers 40, be laminated structure, bamboo curtain splint brachymedial plate 50 be horizontal bamboo curtain splint structure.The width of flattening-out bamboo wood composite container baseboard glued board is 600-1300mm, length is 1000-2500mm, thickness is 18-35mm.
During described wood is long, in plate 20, wooden brachymedial plate 30, length, the thickness of flattening-out bamboo clappers 40, bamboo curtain splint brachymedial plate 50 is 1.0-2.5mm.In the present embodiment, preferably, in wood length, in plate 20, wooden brachymedial plate 30, length, the thickness of flattening-out bamboo clappers is the equal 1.7mm of thickness of 4.0-6.0mm40, bamboo curtain splint brachymedial plate 50.Described phenolic aldehyde tectorial paper 10 is dry and make after the dipping for paper being put into phenolic resin glue in the present embodiment.
Refer to Fig. 2, the present embodiment additionally provides a kind of manufacturing process of flattening-out bamboo wood composite container baseboard glued board, comprises the following steps: and log, former bamboo cross cut saw → log cooking → rotary cut venner → former bamboo hack → and drying → sorting → supporting → gluing → assembly → precompressed → hot pressing → thermal reactor puts → edging → sanding → fluting → packing.
Present embodiments provide a kind of flattening-out bamboo wood composite container baseboard glued board new product, make glued board new product of the present utility model scientific and reasonable for structure, impregnation operation is simple and save glue, Functionality, quality and appealing design, intensity is high, good springiness, panel and base plate are all indeformable, not stratified, surface is non-foaming, anti-pressure ability is strong, effect stability is reliable, cost is low, life-span is long, applied range, both can be applicable to container, can be applicable to door and window again, furniture, automobile, the various aspects such as vessel, both effectively range of application can be expanded, effectively can reduce again the import of container plate, also cost can be effectively reduced, particularly can various pattern required for its surface printing client and elegant in appearance, there is good resistance to impact simultaneously, wearability, resistance tocrocking, environmental protection and wholesome outstanding feature, because the utility model suitably improves the moisture content of veneer, reduce drying cost, more effectively reduce that production board is yielding, layering, bubbling phenomenon, compression strength and elastic modelling quantity add 10%-30%, extend service life, decrease defective products and the cost of product, improve quality, due to the wooden brachymedial plate 30 in its structure of the utility model, wood long in plate 20, not only can use import weedtree, but also domestic weedtree can have been applied, not only convenient, but also the corresponding minimizing material inlet of selection.
The above embodiment only have expressed several embodiment of the present utility model, and it describes comparatively concrete and detailed, but therefore can not be interpreted as the restriction to the utility model the scope of the claims.It should be pointed out that for the person of ordinary skill of the art, without departing from the concept of the premise utility, can also make some distortion and improvement, these all belong to protection domain of the present utility model.
Claims (8)
1. a flattening-out bamboo wood composite container baseboard glued board, is characterized in that, comprise phenolic aldehyde tectorial paper, wood long in plate, wooden brachymedial plate, long in flattening-out bamboo clappers, bamboo curtain splint brachymedial plate, its upper surface is provided with Ah must's plate or the first phenolic aldehyde tectorial paper in the east, and lower surface is provided with Ah must, and plate or flattening-out bamboo stay blue or green panel in the east, on the direction of lower surface, be disposed with plate in first piece of wood length along described upper surface between this upper surface and lower surface, first block of wooden brachymedial plate, flattening-out bamboo clappers in first block length, plate during second block of wood is long, first block of bamboo curtain splint brachymedial plate, plate during 3rd block of wood is long, second block of wooden brachymedial plate, plate during 4th block of wood is long, flattening-out bamboo clappers in second block length, plate during 5th block of wood is long, 3rd block of wooden brachymedial plate, plate during 6th block of wood is long, second block of bamboo curtain splint brachymedial plate, plate during 7th block of wood is long, flattening-out bamboo clappers in 3rd block length, 4th block of wooden brachymedial plate and the 8th block of wood long in plate.
2. flattening-out bamboo wood composite container baseboard glued board according to claim 1, it is characterized in that, described first phenolic aldehyde tectorial paper, second phenolic aldehyde tectorial paper, plate during first block of wood is long, first block of wooden brachymedial plate, flattening-out bamboo clappers in first block length, plate during second block of wood is long, first block of bamboo curtain splint brachymedial plate, plate during 3rd block of wood is long, second block of wooden brachymedial plate, plate during 4th block of wood is long, flattening-out bamboo clappers in second block length, plate during 5th block of wood is long, 3rd block of wooden brachymedial plate, plate during 6th block of wood is long, second block of bamboo curtain splint brachymedial plate, plate during 7th block of wood is long, flattening-out bamboo clappers in 3rd block length, 4th block of wooden brachymedial plate and the 8th block of wood long in glue coated between plate, be interconnected by hot pressing.
3. flattening-out bamboo wood composite container baseboard glued board according to claim 2, it is characterized in that, described glue is phenolic resins, its glue-spread is every square metre of two-sided 380g-420g, and it is coated on the both sides of flattening-out bamboo clappers, bamboo curtain splint brachymedial plate in plate, wooden brachymedial plate, length in wood length by glue spreader.
4. flattening-out bamboo wood composite container baseboard glued board according to claim 3, is characterized in that, during described hot pressing, the temperature of hot press is 125-150 DEG C, the pressure of hot pressing is 2.0-4.0mpa/cm
2, hot pressing time be 50-70min.
5. flattening-out bamboo wood composite container baseboard glued board according to claim 4, is characterized in that, plate during described phenolic aldehyde tectorial paper, wood are long, wooden brachymedial plate, long in flattening-out bamboo clappers, be laminated structure, bamboo curtain splint brachymedial plate is horizontal bamboo curtain splint structure.
6. flattening-out bamboo wood composite container baseboard glued board according to claim 5, is characterized in that, the width of flattening-out bamboo wood composite container baseboard glued board is 600-1300mm, length is 1000-2500mm, thickness is 18-35mm.
7. flattening-out bamboo wood composite container baseboard glued board according to claim 6, is characterized in that, plate during described wood is long, wooden brachymedial plate, long in the thickness of flattening-out bamboo clappers is 4.0-6.0mm, the thickness of bamboo curtain splint brachymedial plate is 1.0-2.5mm.
8. flattening-out bamboo wood composite container baseboard glued board according to claim 7, is characterized in that, described phenolic aldehyde tectorial paper is paper is put into phenolic resin glue drying after dipping to make.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| CN201520301644.4U CN204869122U (en) | 2015-05-11 | 2015-05-11 | Compound container of flattening -out bamboo wood plywood for bottom plate |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| CN201520301644.4U CN204869122U (en) | 2015-05-11 | 2015-05-11 | Compound container of flattening -out bamboo wood plywood for bottom plate |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| CN204869122U true CN204869122U (en) | 2015-12-16 |
Family
ID=54813543
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| CN201520301644.4U Expired - Fee Related CN204869122U (en) | 2015-05-11 | 2015-05-11 | Compound container of flattening -out bamboo wood plywood for bottom plate |
Country Status (1)
| Country | Link |
|---|---|
| CN (1) | CN204869122U (en) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN104827528A (en) * | 2015-05-11 | 2015-08-12 | 佛山市正森木业有限公司 | Plywood used for flattened bamboo-wood composite container bottom plate and production technology thereof |
-
2015
- 2015-05-11 CN CN201520301644.4U patent/CN204869122U/en not_active Expired - Fee Related
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN104827528A (en) * | 2015-05-11 | 2015-08-12 | 佛山市正森木业有限公司 | Plywood used for flattened bamboo-wood composite container bottom plate and production technology thereof |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN104963481A (en) | Anti-cracking floor heating solid wood composite floor and production method thereof | |
| CN103640066B (en) | A kind of composite artificial board for container soleplate and manufacture method thereof | |
| CN102990759B (en) | Dipping compression strengthened floor and manufacturing method thereof | |
| CN102390065A (en) | Plywood for bamboo/wood hybrid structured container baseboard | |
| CN109808011A (en) | A kind of impregnating by pressure fire retardant formula cemented bamboo component and preparation method thereof | |
| CN102773887B (en) | Recombined bamboo wood and oriented strand board composite structural board and manufacturing method thereof | |
| CN204869122U (en) | Compound container of flattening -out bamboo wood plywood for bottom plate | |
| CN102294723A (en) | Non-degreased masson pine solid wood composite floor and production method thereof | |
| CN201020766Y (en) | Composite container floor with particle board as core material for structure | |
| CN103692502B (en) | As the manufacture method of the non-woven fabrics enhancement mode laminated veneer lumber of decoration bar section base material | |
| CN203198012U (en) | Plywood for shipbuilding | |
| CN104827528A (en) | Plywood used for flattened bamboo-wood composite container bottom plate and production technology thereof | |
| CN2894989Y (en) | bamboo plywood | |
| CN101712167B (en) | Composite bottom board for container | |
| CN204296150U (en) | Transparent wear dalle | |
| CN103522373A (en) | Low-carbon method for manufacturing environmental friendly deformation-prevention fireproof sheet material | |
| CN104552495A (en) | Manufacturing method for low-carbon and environmental-protection anti-deformation solid wood composite board | |
| CN202685039U (en) | A composite structure board of recombined bamboo and medium density fiberboard | |
| CN2362808Y (en) | Bamboo composite container base board | |
| CN201178806Y (en) | Dining-table top with frame edging lamination structure | |
| CN204054256U (en) | A kind of container bottom board | |
| CN202540419U (en) | Bamboo-wood composite container bottom plate | |
| CN210173799U (en) | Novel composite board | |
| CN202556511U (en) | A kind of plywood for bamboo and wood container | |
| CN201058449Y (en) | Lumber-core board |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| C14 | Grant of patent or utility model | ||
| GR01 | Patent grant | ||
| CF01 | Termination of patent right due to non-payment of annual fee |
Granted publication date: 20151216 Termination date: 20160511 |
|