CN204825071U - Make balanced face down bonding of current distribution connect I -shaped beam type to collude double anode steel claw in not - Google Patents
Make balanced face down bonding of current distribution connect I -shaped beam type to collude double anode steel claw in not Download PDFInfo
- Publication number
- CN204825071U CN204825071U CN201520525732.2U CN201520525732U CN204825071U CN 204825071 U CN204825071 U CN 204825071U CN 201520525732 U CN201520525732 U CN 201520525732U CN 204825071 U CN204825071 U CN 204825071U
- Authority
- CN
- China
- Prior art keywords
- claw
- girder
- anode steel
- double anode
- auxiliary
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model overcomes it is not enough that prior art exists, provides a structure, simple process, the little make balanced face down bonding of current distribution connect I -shaped beam type to collude double anode steel claw in not of fault rate, in order to solve the technical problem, the utility model discloses a technical scheme do: a make balanced face down bonding of current distribution connect I -shaped beam type to collude double anode steel claw in not, includes crossbeam and claw, the crossbeam is the I shape, includes girder and two auxiliary girders promptly, every the tip both sides of auxiliary girder all are provided with the claw, the claw is the column, and the the central axis who is located four claws of girder one side is on same vertical plane, the top of claw is less than the top of auxiliary girder, the bottom of claw is less than the bottom of auxiliary girder, the utility model discloses but wide application in electrolytic aluminum field.
Description
Technical field
The utility model is a kind of makes the side welding I beam formula of distribution of current equilibrium interior hook double anode steel pawl, belongs to aluminum electrolysis technology field.
Background technology
Anode steel jaw is as a requisite electrical conductor workpiece again of crucial importance in electrolytic aluminium factory production process, and with regard to current anode steel jaw, due in structure formation, ubiquity the unbalanced defect of distribution of current.
If in the production process of electrolytic aluminum, the distribution of current on anode steel jaw can not be balanced, so will have influence on the horizontal current in electrolyzer, and what its result was inevitable will cause pressure drop rise, is also thereupon that power consumption is too much, cost up.For the aluminum electrolysis industry nowadays generally lost, it is also an a difficult problem with overcoming urgently to be resolved hurrily.
More existing anode steel jaw, in order to holding current distributing equilibrium, aluminium guide bar arranges separately wire and is connected with the claw of beam-end, to reaching the distributing equilibrium of electric current on claw, but this mode not only complex process, and failure rate is high.
Utility model content
The utility model overcomes the deficiency that prior art exists, and provides a kind of structure, technique is simple, and failure rate is little makes the side welding I beam formula of distribution of current equilibrium interior hook double anode steel pawl.
In order to solve the problems of the technologies described above, the technical solution adopted in the utility model is: a kind of side welding I beam formula making distribution of current equilibrium in hook double anode steel pawl, comprise crossbeam and claw, described crossbeam is I shape, namely girder and two auxiliary girders are comprised, the both sides, end of each described auxiliary girder are provided with claw, described claw is column, be positioned at the central axis of four claws of girder side at same perpendicular, the top of described claw is lower than the top of auxiliary girder, and the bottom of described claw is lower than the bottom of auxiliary girder.
The top of described claw all cuts out an inclined-plane, and described inclined-plane has a down dip towards auxiliary girder lateral.
Described claw is welded on auxiliary girder.
Described girder top middle portion is vertically connected with aluminium guide bar by blast welding block.
The beneficial effect that the utility model compared with prior art has is: the utility model crossbeam adopts I-shaped crossbeam, in the both sides, auxiliary girder end of crossbeam, all claw is set, form double anode steel pawl, make the blast welding block homogeneous phase of each claw distance girder top middle portion same, such conduction is apart from identical, resistivity is also identical, thus ensure that each claw place distribution of current is balanced, and structure, technique are simple, failure rate is little, in the utility model, claw is symmetricly set on the both sides of auxiliary girder, and thermal contraction variable is consistent, and interior hook phenomenon can not occur.
Accompanying drawing explanation
Below in conjunction with accompanying drawing, the utility model is described further.
Fig. 1 is structural representation of the present utility model.
Fig. 2 is the vertical view of Fig. 1.
In figure: 1 be crossbeam, 11 be girder, 12 be auxiliary girder, 2 for claw.
Embodiment
Solve above-mentioned technical barrier, first where we just must make the reason of its generation current skewness weighing apparatus clear.As everyone knows, electrolytic aluminium factory, when carrying out Aluminum Electrolysis Production process, is take: the electrolysis production technique of " low voltage, big current " and mode, although so the voltage in electrolytic aluminum trough is lower, and its electric current but extremely large.And electric current is in the operational process of conductor, will produce resistivity, therefore, the two ends of steel pawl crossbeam, then the distance apart from crossbeam centre aluminium guide bar and blast welding block due to corresponding is far away, and so the resistivity of top, these two ends is larger.
The such as structure of current electrolysis aluminium manufacturer general multianode steel pawl, be palmation crossbeam and multiple claw, multiple claw evenly arranges the downside being arranged on crossbeam, in the middle, upside of crossbeam, weld a blast welding block be connected with aluminium guide bar.The electric current of anode steel jaw flows through from the blast welding block that steel pawl is middle in other words.
So certainly will cause such situation: the claw in the middle of anode steel jaw, distance blast welding block is nearest, and resistance is minimum, so, electric current just forms big current, and the claw of anode steel jaw beam-end, farthest, resistance is maximum, and so electric current is just corresponding little than middle claw for distance blast welding block.So, just causing the multijaw electron current of anode steel jaw to distribute can not be balanced.
So want the problem solving the equilibrium of anode steel jaw distribution of current, be exactly the beam structure how changing anode steel jaw, allow crossbeam with in the mode of connection of these claws, keep the distance same apart from blast welding block.The utility model is studied around above-mentioned technical barrier expansion just.
As shown in Figure 1 and Figure 2, the utility model is a kind of makes the side welding I beam formula of distribution of current equilibrium interior hook double anode steel pawl, comprise crossbeam 1 and claw 2, described crossbeam 1 is in I shape, namely girder 11 and two auxiliary girders 12 are comprised, the both sides, end of each described auxiliary girder 12 are provided with claw 2, described claw 2 is in column, be positioned at the central axis of four claws 2 of girder 11 side at same perpendicular, the top of described claw 2 is lower than the top of auxiliary girder 12, and the bottom of described claw 2 is lower than the bottom of auxiliary girder 12.
The top of described claw 2 all cuts out an inclined-plane, and described inclined-plane has a down dip towards auxiliary girder 12 lateral.
Described claw 2 is welded on auxiliary girder 12.
Described girder 11 top middle portion is vertically connected with aluminium guide bar by blast welding block.
Described welding process is electroslag welding, or is melting weldering, or is narrow slit weldering, or is induction heating weldering, or is friction welding (FW), or is inert-gas arc welding, or is soldering, or is union-melt weld.
By reference to the accompanying drawings embodiment of the present utility model is explained in detail above, but the utility model is not limited to above-described embodiment, in the ken that those of ordinary skill in the art possess, various change can also be made under the prerequisite not departing from the utility model aim.
Claims (4)
1. one kind makes the side welding I beam formula of distribution of current equilibrium interior hook double anode steel pawl, it is characterized in that: comprise crossbeam (1) and claw (2), described crossbeam (1) is in I shape, namely girder (11) and two auxiliary girders (12) are comprised, the both sides, end of each described auxiliary girder (12) are provided with claw (2), described claw (2) is in column, be positioned at the central axis of four claws (2) of girder (11) side at same perpendicular, the top of described claw (2) is lower than the top of auxiliary girder (12), the bottom of described claw (2) is lower than the bottom of auxiliary girder (12).
2. a kind of side welding I beam formula making distribution of current equilibrium according to claim 1 in hook double anode steel pawl, it is characterized in that: the top of described claw (2) all cuts out an inclined-plane, and described inclined-plane has a down dip towards auxiliary girder (12) lateral.
3. a kind of side welding I beam formula making distribution of current equilibrium according to claim 1 and 2 in hook double anode steel pawl, it is characterized in that: described claw (2) is welded on auxiliary girder (12).
4. a kind of side welding I beam formula making distribution of current equilibrium according to claim 3 in hook double anode steel pawl, it is characterized in that: described girder (11) top middle portion is vertically connected with aluminium guide bar by blast welding block.