CN204278187U - Ripple bent limit ecosystem emulation furring tile makes bed die core - Google Patents

Ripple bent limit ecosystem emulation furring tile makes bed die core Download PDF

Info

Publication number
CN204278187U
CN204278187U CN201420504256.1U CN201420504256U CN204278187U CN 204278187 U CN204278187 U CN 204278187U CN 201420504256 U CN201420504256 U CN 201420504256U CN 204278187 U CN204278187 U CN 204278187U
Authority
CN
China
Prior art keywords
ripple
bed die
bent limit
die core
ecosystem
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN201420504256.1U
Other languages
Chinese (zh)
Inventor
胡洪容
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SICHUAN MINGZHU CERAMIC Co Ltd
Original Assignee
SICHUAN MINGZHU CERAMIC Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SICHUAN MINGZHU CERAMIC Co Ltd filed Critical SICHUAN MINGZHU CERAMIC Co Ltd
Priority to CN201420504256.1U priority Critical patent/CN204278187U/en
Application granted granted Critical
Publication of CN204278187U publication Critical patent/CN204278187U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

The utility model discloses a kind of ripple bent limit ecosystem emulation furring tile and make bed die core; It is characterized in that: there is outside described bed die core more than one ripple bent limit shape.The design in ecosystem emulation face is the application of building decoration material on ceramic tile meeting ecosystem, and all ecosystem shapes such as stone, bamboo wood, flowers and plants, animal are transferred on ceramic tile surface; For meeting the integrality of ceramic tile surface pattern, ripple bent limit shape on each side of the continuity of pattern after paving uses and the design of mating surface line pattern characteristics; Ripple bent limit profile design constructability reduces paving difficulty, and the occlusion that interlocks of ripple limit also allows wall brick more firmly prevent from coming off.For solve ceramic tile blank compacting and sintering procedure in base substrate unequal power distribution occur cracking and deformation defect design bed die supercharging and decompression zone, be embodied in reduce pressure and degree of boost ± 30%; For meeting the adobe side plate step surface that the demoulding and production technology needs are arranged in compacting; For meet die cavity the side plate larger pressure that bears and wearability in adobe compacting require selected by specific alloy material etc.

Description

Ripple bent limit ecosystem emulation furring tile makes bed die core
Technical field
The utility model relates to a kind of mould for processing ceramic tile, is specifically that a kind of line limit ecosystem emulation furring tile makes bed die core.
Background technology
As everyone knows, ceramic tile is with fire-resistant metal oxide and half-metal oxide, via the process of grinding, mixing, compacting, glazing, sintering, and the building of the porcelain of a kind of acid and alkali-resistance of formation or Shi Zhi etc. or the material of decoration, be always referred to as ceramic tile.Its raw material are many to be mixed by clay, quartz sand etc.The use of ceramic tile is seen everywhere, and stretches into daily life, and the processing of ceramic tile is normally prepared from by supporting mould; Along with ceramic tile is applied gradually widely, the making mould of ceramic tile is also focused on by technical staff thereupon.
The utility model of the patent No. 201120415185.4 provides a kind of tile mould of high-strength adhesion isostatic mould-core, multiple anyhow staggered stripe shape groove is evenly distributed with above the matrix of a tile mould, the rubber cushion glue head that arrange corresponding to stripe shape groove in top is pasted onto in corresponding stripe shape groove, seal oil chamber in matrix passes to the buffering space formed above matrix between matrix and rubber cushion, is provided with and the corresponding sealing strip groove of rubber cushion periphery for pasting in matrix surrounding.During use, Seal Oil in matrix can regulate pressurized space in the buffering space between stripe shape groove voluntarily, make the overall pressed density of the ceramic tile of processing consistent, to reduce ceramic tile sintering warpage, because the glue head entirety of rubber cushion is pasted onto in stripe shape groove, constantly repeatedly suppressing in knockout course, rubber cushion and matrix is there will not be to come off or rubber cushion fracture phenomena, there is long service life, the distinguishing feature such as wait the large and static pressure of quiet area effective.
The utility model patent of the patent No. 00237114.6 discloses a kind of pressing-forming mould for ceramic tile, comprise and lay respectively at upper mold core in upper and lower mould side plate and lower mold core, be characterized at least having exhaust passage at one of upper and lower core rod, the powder between described exhaust passage and upper and lower core rod loads cavity UNICOM.The utility model shortens evacuation time, improves the shaping speed of pressing unfired brick, and can improve uniformity and the compactness of adobe density.
The utility model of patent No. 01233880.X discloses a kind of mould of arced ceramic tile, include the outer mold for placing adobe, outer mold is formed with the face of cylinder of indent, also increase and have an inner mould core, inner mould core has the external cylindrical surface with indent face of cylinder corresponding matching, inner mould core can be put into outer mold and adobe is sandwiched in centre and exerts pressure, such mould, the overall uniformity of the radial brick produced, radian deviation is little, and production efficiency is high, quality is good, be easy to adjustment, overcome the high shaping defect of traditional moulds large, the inconsistent rate of distortion.
The utility model of the patent No. 201410197466.5 discloses a kind of ripple limit ecosystem emulation furring tile and makes mould, comprises bed die core, face mould core and die cavity side plate; 1. the design in ecosystem emulation face is the application of building decoration material on ceramic tile meeting ecosystem, and all ecosystem shapes such as stone, bamboo wood, flowers and plants, animal are transferred on ceramic tile surface; For the integrality and paving that meet ceramic tile surface pattern use the ripple glaze bent limit shape of the continuity design of rear pattern; Stressed shape is cut for what solve because of adobe effect of stress, product causes that blank cracking designs in shape on the bent limit of product and die side plate in high-temperature firing process; For solve ceramic tile blank compacting and sintering procedure in base substrate unequal power distribution occur cracking and deformation defect design bed die supercharging and decompression zone, be embodied in reduce pressure and degree of boost ± 30%; For meeting the adobe side plate step surface that the demoulding and production technology needs are arranged in compacting; For meet die cavity the side plate larger pressure that bears and wearability in adobe compacting require selected by specific alloy material etc.But the outside of this mould is ripple glaze bent limit shape.
But the analysis found that, the existing tile product be widely used is all straight flange right-angle design, is formed in paving uses like this and significantly split lines, not nature of looking ill at ease.Another straight flange right angle product can cause seam crossing to occur height step because of deformation of products or construction wrong, affects result of use.Wall brick the more important thing is that straight flange right-angle design paving construction difficulty is comparatively large, and the wall brick after paving is also easily insecure and come off.
Utility model content
The purpose of this utility model is to provide a kind of ripple bent limit ecosystem emulation furring tile to make bed die core at this; For meeting the integrality of ceramic tile surface pattern, ripple bent limit shape on each side that paving uses the continuity of rear pattern and designs; Ripple bent limit profile design constructability reduces paving difficulty, and the occlusion that interlocks of ripple limit also allows wall brick more firmly prevent from coming off.
The utility model carries out in the following manner: construct a kind of ripple bent limit ecosystem emulation furring tile and make bed die core; It is characterized in that: there is outside described bed die core more than one ripple bent limit shape; The design constructability of ripple bent limit shape reduces paving difficulty, and ripple limit interlocks to be engaged and also allows prepared wall brick more firmly prevent from coming off.
Make bed die core according to ripple described in the utility model bent limit ecosystem emulation furring tile, it is characterized in that: with concavo-convex embossment region 11,12 in bed die core.
Make bed die core according to ripple described in the utility model bent limit ecosystem emulation furring tile, it is characterized in that: the wavelength of the bent limit of the ripple on each side of described bed die core shape is from 1mm to 600mm, and wave amplitude is from 1mm to 300mm.
Make bed die core according to ripple described in the utility model bent limit ecosystem emulation furring tile, it is characterized in that: ripple bent limit shape is trapezoidal wave, square wave, sine wave, triangular wave or staircase waveform.
Make bed die core according to ripple described in the utility model bent limit ecosystem emulation furring tile, it is characterized in that: bed die core is that alloy material is made.
In sum, ripple described in the utility model bent limit ecosystem emulation furring tile makes bed die core, and its bed die core side is one and above ripple bent limit shape; Simultaneously in bed die core with concavo-convex anaglyph.Mould described in the utility model: 1, the design in ecosystem emulation face is the application of building decoration material on ceramic tile meeting ecosystem, and all ecosystem shapes such as stone, bamboo wood, flowers and plants, animal are transferred on ceramic tile surface; 2, for meeting integrality and the shape facility requirement of ceramic tile surface pattern, (square-wave form is from one to multiple for the ripple bent limit shape that paving uses the continuity of rear pattern and designs, wavelength is from 1mm to 600mm, wave amplitude from 1mm to 300mm, waveform covers trapezoidal wave, square wave, sine wave, triangular wave, staircase waveform, various ripple are combined into composite wave-shape or other irregular waveform etc.); 3, ripple bent limit profile design constructability reduces paving difficulty and increases work efficiency, and the occlusion that interlocks of ripple limit also allows wall brick more firmly prevent from coming off.4, for solve ceramic tile blank compacting and sintering procedure in base substrate unequal power distribution occur cracking and deformation defect design bed die supercharging and decompression zone, be embodied in decompression and degree of boost ± 30%; 5, for meeting the adobe side plate step surface that the demoulding and production technology needs are arranged in compacting; 6, for meet die cavity the side plate larger pressure that bears and wearability in adobe compacting require selected by specific alloy material etc.
The advantage of this novel practical is: this novel practical provides a kind of ripple bent limit ecosystem emulation furring tile to make bed die core at this; 1, by the square corrugated limit male and fomale(M&F) ceramic tile that this face mould core makes, can meet the application of building decoration material on ceramic tile of ecosystem, all ecosystem shapes such as stone, bamboo wood, flowers and plants, animal are transferred on ceramic tile surface; 2, for meeting integrality and the shape facility requirement of ceramic tile surface pattern, (square-wave form is from one to multiple for the square corrugated bent limit shape that paving uses the continuity of rear pattern and designs, wavelength is from 1mm to 600mm, wave amplitude from 1mm to 300mm, waveform covers trapezoidal wave, square wave, sine wave, triangular wave, staircase waveform, various ripple are combined into composite wave-shape or other irregular waveform etc.); 3, square corrugated bent limit profile design constructability reduces paving difficulty and increases work efficiency, and the occlusion that interlocks of ripple limit also allows wall brick more firmly prevent from coming off.4, for solve ceramic tile blank compacting and sintering procedure in base substrate unequal power distribution occur cracking and deformation defect design bed die supercharging and decompression zone, be embodied in decompression and degree of boost ± 30%; 5, for meeting the adobe side plate step surface that the demoulding and production technology needs are arranged in compacting; 6, for meet die cavity the side plate larger pressure that bears and wearability in adobe compacting require selected by specific alloy material etc.
Accompanying drawing explanation
Fig. 1 is bed die core schematic diagram described in the utility model
Fig. 2 is the utility model face mould core schematic diagram
Fig. 3 A, Fig. 3 B, Fig. 3 C, Fig. 3 D are several form schematic diagrames of ripple bent limit ecosystem emulation furring tile respectively
Fig. 4 is A-A profile in the utility model Fig. 3 A
Fig. 5 is square corrugated limit ecosystem emulation furring tile die assembly floor map
Fig. 6 is square corrugated limit ecosystem emulation furring tile die assembly generalized section
Fig. 7 is square corrugated limit ecosystem emulation furring tile die assembly perspective diagram
Wherein: bed die core 10, concavo-convex embossment region 11,12, face mould core 20, inner concavity region 21, die cavity side plate 30, cavity 31, step surface 32, ripple bent limit shape 40, step 50 that emulation furring tile is corresponding.
Detailed description of the invention
Below in conjunction with accompanying drawing 1-7, the utility model is described in detail, technical scheme in the utility model embodiment is clearly and completely described, obviously, described embodiment is only the utility model part embodiment, instead of whole embodiments.Based on the embodiment in the utility model, those of ordinary skill in the art are not making the every other embodiment obtained under creative work prerequisite, all belong to the scope of the utility model protection.
The utility model provides a kind of square corrugated bent limit ecosystem emulation furring tile to make bed die core (finishing die size covers length of side 600mm and following all specification product sizes); Mainly solve wall brick and the more important thing is that straight flange right-angle design paving construction difficulty is comparatively large, the wall brick after paving is also easily insecure and the problem that comes off.
Form ripple limit ecosystem by bed die core 10, face mould core 20 and die cavity side plate 30 and emulate furring tile assembling die; With inner concavity region 21 in face mould core 20; Outside described bed die core 10 and face mould core 20, there is more than one ripple bent limit shape 40; In the cavity 31 that the ripple corresponding with bed die core 10, face mould core 20 bent limit shape 40 matches in the middle part of described die cavity side plate 30; The design constructability of ripple bent limit shape reduces paving difficulty, and the occlusion that interlocks of ripple limit also allows wall brick more firmly prevent from coming off.
Bed die core 10 is upper with concavo-convex embossment region 11,12; Make it with concavo-convex anaglyph; Concavo-convex embossment region is also corresponding simultaneously forms pressurizing area 11 and reduced pressure zone 12.For solving bed die supercharging and the decompression zone of the ceramic tile blank cracking that base substrate unequal power distribution occurs in compacting and sintering procedure and deformation defect design, be embodied in degree of pressure reduction about 30%.
Ripple on outside described bed die core 10 and face mould core 20 bent limit shape 40; Its waveform shape is from one to multiple, and wavelength is from 1mm to 600mm, and wave amplitude is from 1mm to 300mm.For meeting the integrality of ceramic tile surface pattern, square corrugated bent limit shape (, to multiple, wavelength is from 1mm to 600mm for square-wave form, and wave amplitude is from 1mm to 300mm) on each side that paving uses the continuity of rear pattern and designs.Waveform covers trapezoidal wave, square wave, sine wave, triangular wave, staircase waveform, various ripple are combined into composite wave-shape or other irregular waveform etc.).After improving, such as square corrugated bent limit profile design constructability reduces paving difficulty, and the occlusion that interlocks of ripple limit also allows wall brick more firmly prevent from coming off.
A step surface 32 is had in the cavity side plate mated with bed die core, face mould core in the middle part of described die cavity side plate 30.Its objective is as meeting the adobe side plate step surface that the demoulding and production technology needs are arranged in compacting.
Bed die core 10, face mould core 20 and die cavity side plate 30 form a set of square corrugated limit ecosystem emulation furring tile and make mould, and bed die core 10, face mould core 20 and die cavity side plate 30 can be made for alloy material.
To the above-mentioned explanation of the disclosed embodiments, product professional and technical personnel in the field being realized or uses the utility model mould and this mould to produce.To be apparent for those skilled in the art to the multiple amendment of these embodiments, General Principle as defined herein when not departing from spirit or scope of the present utility model, can realize in other embodiments.Therefore, the utility model can not be restricted to these embodiments shown in this article, also be not limited to the square corrugated size of product side that exemplifies and quantity, but will meet the widest scope consistent with principle disclosed herein and features of novelty.

Claims (5)

1. a ripple bent limit ecosystem emulation furring tile makes bed die core (10), it is characterized in that: described bed die core (10) outside has bent limit shape (40) of more than one ripple.
2. ripple bent limit ecosystem emulation furring tile makes bed die core (10) according to claim 1, it is characterized in that: with concavo-convex embossment region (11,12) in bed die core (10).
3. ripple bent limit ecosystem emulation furring tile makes bed die core (10) according to claim 1, it is characterized in that: the wavelength of bent limit shape (40) of the ripple on each side of described bed die core (10) is from 1mm to 600mm, and wave amplitude is from 1mm to 300mm.
4. according to claim 1 or 3, ripple bent limit ecosystem emulation furring tile makes bed die core, it is characterized in that: bent limit shape (40) of ripple is trapezoidal wave, square wave, sine wave, triangular wave or staircase waveform.
5. ripple bent limit ecosystem emulation furring tile makes bed die core (10) according to claim 1, it is characterized in that: bed die core (10) is made for alloy material.
CN201420504256.1U 2014-09-03 2014-09-03 Ripple bent limit ecosystem emulation furring tile makes bed die core Expired - Lifetime CN204278187U (en)