CN204277301U - Steel cord ends welding forming mould - Google Patents

Steel cord ends welding forming mould Download PDF

Info

Publication number
CN204277301U
CN204277301U CN201420668666.XU CN201420668666U CN204277301U CN 204277301 U CN204277301 U CN 204277301U CN 201420668666 U CN201420668666 U CN 201420668666U CN 204277301 U CN204277301 U CN 204277301U
Authority
CN
China
Prior art keywords
mould
left mould
embedded groove
steel cord
cord ends
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201420668666.XU
Other languages
Chinese (zh)
Inventor
刘彬国
何京辉
曹祥瑞
刘钦
陈铁蛋
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xingtai Jinglong Electronic Material Co Ltd
Original Assignee
Xingtai Jinglong Electronic Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xingtai Jinglong Electronic Material Co Ltd filed Critical Xingtai Jinglong Electronic Material Co Ltd
Priority to CN201420668666.XU priority Critical patent/CN204277301U/en
Application granted granted Critical
Publication of CN204277301U publication Critical patent/CN204277301U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a kind of steel cord ends welding forming mould, relate to single crystal growing furnace hoisting mechanism.The utility model comprises the left mould of chimeric use in pairs and right mould, described left mould is identical with the structure of right mould, a semicircle die cavity is respectively provided with on the die joint of left mould and on the die joint of right mould, the circular die cavity of described two halves is closely sealed when left mould and right mould are fitting for one is forming cavity, described forming cavity be diameter can with the straight hole of wirerope diameter matched in clearance, on the die joint of left mould, the both sides of semicircle die cavity are provided with the embedded groove of recessed left mould and protrude the insertion wedge of die joint, the die joint of right mould be provided with the embedded groove on left mould and insert wedge and embed the insertion wedge and embedded groove that coordinate.Utilize this mould, steel cord ends one-shot forming can be made, greatly improve treatment effect and the treatment effeciency of steel cord ends, reduce labour intensity.

Description

Steel cord ends welding forming mould
Technical field
The utility model relates to single crystal growing furnace hoisting mechanism, particularly a kind of steel cord ends welding forming mould.
Background technology
The hoisting mechanism of single crystal growing furnace is soft axle transmission, mostly all adopt steel wire rope as flexible axle, a rotation cable car mechanism is had at the top of stove, one end of steel wire rope is connected with rotation cable car, the other end connects monocrystal rod, during crystal pulling, cable car ceaselessly rotates and scrolling rope hoisting monocrystal rod slowly, and steel wire rope wants coaxial with the rotation of stove.Crucible is supported by a hard axle and is rotated under the effect of hoisting mechanism and rises, and liquation is contained in crucible, and graphite crucible bar is screwed on the lower shaft of single crystal growing furnace, and hard axle is fixed on the hoisting mechanism of crucible; Crucible lifting mechanism guide rail and leading screw smooth-going, drive hard axle to rotate and want steadily, crucible lifting mechanism runs to be wanted steadily.As can be seen here, steel wire rope plays a part very important in the growth course of single crystal growing furnace, the particularly two ends that are connected with cable car and monocrystal rod of steel wire rope, if process bad, the normal use of hoisting mechanism can be affected, when connecting steel wire ropes, first the steel wire rope of rolling is needed to block, the jag burr of steel cord ends is processed, could be connected with miscellaneous part after polishing rounding, at present, the mode of manual polishing is adopted to carry out steel cord ends process, this processing mode compares to waste time and energy, also easily hurt sb.'s feelings, the more important thing is, steel cord ends after grinding process not rounding, rough, diameter is also not of uniform size, do not meet use standard.
Utility model content
Technical problem to be solved in the utility model is to provide a kind of steel cord ends welding forming mould, utilizes this mould, can make steel cord ends one-shot forming, greatly improves treatment effect and the treatment effeciency of steel cord ends, reduces labour intensity.
For solving the problems of the technologies described above, technical solution adopted in the utility model is: a kind of steel cord ends welding forming mould, comprise the left mould of chimeric use in pairs and right mould, described left mould is identical with the structure of right mould, a semicircle die cavity is respectively provided with on the die joint of left mould and on the die joint of right mould, the circular die cavity of described two halves is closely sealed when left mould and right mould are fitting for one is forming cavity, described forming cavity be diameter can with the straight hole of wirerope diameter matched in clearance, on the die joint of left mould, the both sides of semicircle die cavity are provided with the embedded groove of recessed left mould and protrude the insertion wedge of die joint, the die joint of right mould be provided with the embedded groove on left mould and insert wedge and embed the insertion wedge and embedded groove that coordinate.
Further, the upper surface of described insertion wedge and the upper surface of left mould or right mould are in same level, and corresponding embedded groove is positioned on the same upper surface of left mould and right mould.
Further, described embedded groove and insertion wedge are positioned at the centre of left mould and right mould height.
Further, described embedded groove and insertion wedge are square.
Further, described embedded groove and insertion wedge also can be triangle.
Preferably, described left mould and right mould are copper material.
The beneficial effect adopting technique scheme to produce is: forming cavity one end of steel wire rope being put into this mould, argon arc welding is utilized to be melted by steel cord ends, in the liquation insert molding chamber of fusing, due to the restriction by forming cavity, liquation can form the steel cord ends that rounding is smooth together with being set in the steel wire rope in forming cavity, save manual polishing operation, simplify the operation operation greatly, reduces labour intensity, greatly improve treatment effect and the treatment effeciency of steel cord ends.
Accompanying drawing explanation
Fig. 1 is the structural representation of the utility model embodiment one;
Fig. 2 is the structural representation utilizing embodiment one melting welding steel cord ends;
Fig. 3 is the structural representation of the utility model embodiment two;
Fig. 4 is the structural representation utilizing embodiment two melting welding steel cord ends;
In figure: 1, Zuo Mo; 2, semicircle die cavity; 3, wedge is inserted; 4, right mould; 5, embedded groove; 6, steel wire rope.
Detailed description of the invention
Below in conjunction with the drawings and specific embodiments, the utility model is described in further detail.
In single crystal growth process, the process of steel cord ends used is lack of standardization nonstandard, namely with jagged or due to the problem such as the steel cord ends of manual grinding process is rough, also certain impact can be brought on the overall transmission of hoisting mechanism, such as manual polishing is wasted time and energy, be difficult to be connected with miscellaneous part, therefore, a kind of method of fast processing steel cord ends is needed.
Utilize the utility model to solve the problem, make steel wire rope 6 end one-shot forming, and without the need to polishing.
As embodiment one wherein, see Fig. 1, Fig. 2, the utility model specifically comprises left mould 1 and the right mould 4 of chimeric use in pairs, described left mould 1 is identical with the structure of right mould 4, a semicircle die cavity 2 is respectively provided with on the die joint of left mould 1 and on the die joint of right mould 4, the circular die cavity 2 of described two halves is closely sealed when left mould 1 and right mould 4 are fitting for one is forming cavity, described forming cavity is the straight hole that diameter can coordinate with steel wire rope 6 diametric clearance, on the die joint of left mould 1, the both sides of semicircle die cavity 2 are provided with the embedded groove 5 of recessed left mould 1 and protrude the insertion wedge 3 of die joint, the die joint of right mould 4 be provided with the embedded groove 5 on left mould 1 and insert wedge 3 and embed the insertion wedge and embedded groove that coordinate.
The upper surface of insertion wedge 3 wherein and the upper surface of left mould 1 or right mould 4 are in same level, on the same upper surface that corresponding embedded groove 5 is positioned at left mould 1 and right mould 4 and embedded groove 5 and insert wedge 3 for square.
The structure of embodiment two is: see Fig. 3, Fig. 4, comprise left mould 1 and the right mould 4 of chimeric use in pairs, described left mould 1 is identical with the structure of right mould 4, a semicircle die cavity 2 is respectively provided with on the die joint of left mould 1 and on the die joint of right mould 4, the circular die cavity 2 of described two halves is closely sealed when left mould 1 and right mould 4 are fitting for one is forming cavity, described forming cavity is the straight hole that diameter can coordinate with steel wire rope 6 diametric clearance, on the die joint of left mould 1, the both sides of semicircle die cavity 2 are provided with the embedded groove 5 of recessed left mould 1 and protrude the insertion wedge 3 of die joint, the die joint of right mould 4 be provided with the embedded groove 5 on left mould 1 and insert wedge 3 and embed the insertion wedge and embedded groove that coordinate.Described embedded groove 5 and insertion wedge 3 are positioned at the centre of left mould 1 and right mould 4 height.Described embedded groove 5 and insertion wedge are triangle.
Wherein, the embedded groove 5 in embodiment one on left mould 1 and right mould 4 and insert the structure of wedge 3, compares the structure of embodiment two, more left mould 1 and right mould 4, pulls down steel wire rope 6 and compares simply more convenient.But all can select adopt square or leg-of-mutton embedded groove 5 and insert wedge 3.Wherein leg-of-mutton embedded groove 5 is compared square with insertion wedge 3, and grafting is chimeric more firm.
When steel wire rope 6 needs to block, steel wire rope 6 is placed in the semicircle die cavity 2 of left mould 1, then right mould 4 is inserted left mould 1, steel wire rope 6 is blocked, fuses with welding.
When needs process steel wire rope 6 end, first steel wire rope 6 is embedded in one of them semicircle die cavity 2, then another mould chimeric, and make steel wire rope 6 end expose left mould 1 upper surface 5-6 millimeter, argon arc welding is used to be melted steel wire rope 6 end, the liquation of fusing flows in forming cavity, and is solidified as one with the part steel wire rope 6 in forming cavity, takes out after cooling.
Steel wire rope 6 plumb joint of different model can be made according to the different type of furnaces, convenient, easy to operate.
The chimera of the left mould of the utility model 1 and right mould 4 is cylinder, and also can be square cylinder, wherein left mould 1 and right mould 4 adopt copper material to make, and after welding completes, because copper is different from the fusing point of steel, can not cause adhesion phenomenon, steel wire rope is easy to take off.

Claims (6)

1. a steel cord ends welding forming mould, it is characterized in that, comprise left mould (1) and the right mould (4) of chimeric use in pairs, described left mould (1) is identical with the structure of right mould (4), a semicircle die cavity (2) is respectively provided with on the die joint of left mould (1) and on the die joint of right mould (4), described two semicircle die cavitys (2) are closely sealed when left mould (1) and right mould (4) are fitting for one is forming cavity, described forming cavity is the straight hole that diameter can coordinate with steel wire rope (6) diametric clearance, on the die joint of left mould (1), the both sides of semicircle die cavity (2) are provided with the embedded groove (5) of recessed left mould (1) and protrude the insertion wedge (3) of die joint, the die joint of right mould (4) be provided with the embedded groove (5) on left mould (1) and insert wedge (3) and embed the insertion wedge and embedded groove that coordinate.
2. steel cord ends welding forming mould according to claim 1, it is characterized in that, the upper surface of described insertion wedge (3) and the upper surface of left mould (1) or right mould (4) are in same level, and corresponding embedded groove (5) is positioned on the same upper surface of left mould (1) and right mould (4).
3. steel cord ends welding forming mould according to claim 1, is characterized in that, described embedded groove (5) and insertion wedge (3) are positioned at the centre of left mould (1) and right mould (4) height.
4. the steel cord ends welding forming mould according to Claims 2 or 3, is characterized in that, described embedded groove (5) and insertion wedge (3) are for square.
5. the steel cord ends welding forming mould according to Claims 2 or 3, is characterized in that, described embedded groove (5) and insertion wedge (3) are triangle.
6. steel cord ends welding forming mould according to claim 1, is characterized in that, described left mould (1) and right mould (4) are copper material.
CN201420668666.XU 2014-11-11 2014-11-11 Steel cord ends welding forming mould Expired - Fee Related CN204277301U (en)