CN204269526U - 一种实现在高温高压状态下对挂片腐蚀试验的装置 - Google Patents
一种实现在高温高压状态下对挂片腐蚀试验的装置 Download PDFInfo
- Publication number
- CN204269526U CN204269526U CN201420844913.7U CN201420844913U CN204269526U CN 204269526 U CN204269526 U CN 204269526U CN 201420844913 U CN201420844913 U CN 201420844913U CN 204269526 U CN204269526 U CN 204269526U
- Authority
- CN
- China
- Prior art keywords
- tank body
- gland bonnet
- coupon
- pressure state
- test under
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种实现在高温高压状态下对挂片腐蚀试验的装置,包括罐体,所述罐体设有密封盖,所述密封盖的底部设有挂片吊钩,所述挂片吊钩上设有腐蚀挂片;所述的罐体和密封盖的外周设有相对应的压紧螺孔,所述压紧螺孔内设有压紧螺栓,实现罐体和密封盖的密封;所述密封盖上设有减压阀,并设有压力表,从而实现对罐体内部压力的调控;本实用新型的优点在于:能够耐压、耐温,满足不同条件的缓蚀实验,实验得出数据准确度较高,外部影响因素少,结构简单,使用方便。
Description
技术领域
本实用新型涉及一种挂片腐蚀试验的装置,具体地说是一种实现在高温高压状态下对挂片腐蚀试验的装置,属于挂片腐蚀试验装置领域。
背景技术
目前,在化工厂、油田、炼化行业,所有流体介质都是通过管道输送,而管道主要材质为普通碳钢,由于所输送的介质大部分都为酸性或弱酸性介质,因此随着时间的增加,管道会被内部介质不断腐蚀,最终导致损坏。另外,在炼化过程中由于还经常伴有高温高压的环境,因此,对设备的腐蚀愈发严重。为了减缓介质对设备的腐蚀速度,延长设备使用时限,缓蚀剂产品便孕育而生,不同的环境条件下会有不同种类的缓蚀剂,其效果也各不相同。而对于一种缓蚀剂在某一工艺上缓蚀效果的好坏的确定,必须要进行相应的缓蚀评价实验,其最基本的实验就是用腐蚀挂片法来确定,然而现有的实验设备几乎都是常压装置,且实验温度也不高(100℃以内),做出的实验结果只能是相对数值的好坏,如果想更真实的反应其好坏程度,就需要尽可能的来模拟现场环境,如高温高压状态下的效果。
实用新型内容
本实用新型的目的在于,设计了一种实现在高温高压状态下对挂片腐蚀试验的装置,能够耐压、耐温,满足不同条件的缓蚀实验,实验得出数据准确度较高,外部影响因素少,结构简单,使用方便。
本实用新型的技术方案为:
一种实现在高温高压状态下对挂片腐蚀试验的装置,包括罐体,所述罐体设有密封盖,所述密封盖的底部设有挂片吊钩,所述挂片吊钩上设有腐蚀挂片;所述的罐体和密封盖的外周设有相对应的压紧螺孔,所述压紧螺孔内设有压紧螺栓,实现罐体和密封盖的密封;所述密封盖上设有减压阀,并设有压力表,从而实现对罐体内部压力的调控,使得整套装置能够满足不同条件的缓蚀实验,实验得出数据准确度较高,外部影响因素少
进一步地,所述罐体的顶部周围设有密封槽,所述密封盖的一部分位于所述密封槽内,进一步地提高了罐体的密封性;
进一步地,所述罐体的内壁为聚四氟乙烯内壁,能耐压、耐温。
本实用新型的优点在于:罐体设有内衬,密封性良好,能耐压、耐温,使得整套装置能够满足不同条件的缓蚀实验,实验得出数据准确度较高,外部影响因素少。
下面结合附图和实施例对本实用新型作进一步说明。
附图说明
图1为本实用新型实施例的结构示意图;
图中:1-罐体、2-密封盖、3-压紧螺孔、4-挂片吊钩、5-压力表、6-减压阀、7-内壁、8-腐蚀挂片、9-密封槽。
具体实施方式
以下对本实用新型的优选实施例进行说明,应当理解,此处所描述的优选实施例仅用于说明和解释本实用新型,并不用于限定本实用新型。
实施例1
如图1所示,一种实现在高温高压状态下对挂片腐蚀试验的装置,包括罐体1,所述罐体1的顶部设有密封盖2,所述密封盖2的底部设有挂片吊钩4,所述挂片吊钩4上设有腐蚀挂片8;所述的罐体1和密封盖2的外周设有相对应的压紧螺孔3,所述压紧螺孔3内设有压紧螺栓,实现罐体1和密封盖2的密封;所述罐体1的顶部周围设有密封槽9,所述密封盖2的一部分位于所述密封槽9内,进一步地提高了罐体1的密封性;所述密封盖2上设有减压阀6,并设有压力表5,从而实现对罐体1内部压力的调控;所述罐体1的内壁为聚四氟乙烯内壁,能耐压、耐温,使得整套装置能够满足不同条件的缓蚀实验,实验得出数据准确度较高,外部影响因素少。
Claims (3)
1.一种实现在高温高压状态下对挂片腐蚀试验的装置,其特征在于:包括罐体,所述罐体设有密封盖,所述密封盖的底部设有挂片吊钩,所述挂片吊钩上设有腐蚀挂片;所述的罐体和密封盖的外周设有相对应的压紧螺孔,所述压紧螺孔内设有压紧螺栓,实现罐体和密封盖的密封;所述密封盖上设有减压阀,并设有压力表。
2.根据权利要求1所述的一种实现在高温高压状态下对挂片腐蚀试验的装置,其特征在于:所述罐体的顶部周围设有密封槽,所述密封盖的一部分位于所述密封槽内。
3.根据权利要求1或2所述的一种实现在高温高压状态下对挂片腐蚀试验的装置,其特征在于:所述罐体的内壁为聚四氟乙烯内壁,能耐压、耐温。