CN203361506U - 防潮阻燃轻质装饰板 - Google Patents
防潮阻燃轻质装饰板 Download PDFInfo
- Publication number
- CN203361506U CN203361506U CN 201320321908 CN201320321908U CN203361506U CN 203361506 U CN203361506 U CN 203361506U CN 201320321908 CN201320321908 CN 201320321908 CN 201320321908 U CN201320321908 U CN 201320321908U CN 203361506 U CN203361506 U CN 203361506U
- Authority
- CN
- China
- Prior art keywords
- damp
- paper layer
- melamine
- inflaming retarding
- decorative
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型提供了一种防潮阻燃轻质装饰板,包括从上至下依次设置的三聚氰胺浸渍耐磨纸层、三聚氰胺浸渍装饰纸层、防潮阻燃纤维板和三聚氰胺浸渍平衡纸层。本实用新型不但质量轻,节约了物流成本,还大大减少了森林资源的浪费。
Description
技术领域
本实用新型涉及一种装饰板,尤其涉及一种防潮阻燃轻质装饰板。
背景技术
公安部和建设部于1992年颁布实施了《建筑内部装修设计防火规范》,国家质量监督检验检疫总局于2006发布了GB8624-2006《建筑材料及制品燃烧性能分级》、GB/T20284-2006《建筑材料或制品的单体燃烧试验》、GB/T20285-2006《材料产烟毒性危险分级》及GB20286-2006《公共场所阻燃制品及组件燃烧性能要求及标识》等五项强制性标准,对建筑装饰装修材料、家具的阻燃性能做了具体规定,要求应用于公共建筑和高层民用建筑的材料燃烧性能不低于GB8624-2006的C级或GB8624-1997的B1级。
为了达到防潮效果,国家标准GB/T18102-2007《浸渍纸层压木质地板》中规定吸水厚度膨胀率必须≤18%。
目前,市场上的装饰板阻燃性能、力学性能、甲醛释放量、吸水厚度膨胀率、产烟量和烟毒性能达到国家标准要求的只有中、高密度装饰板。而中、高密度装饰板的缺点为:浪费森林资源、质量重、生产效率低、物流成本高。因为生产中、高密度纤维板的木片消耗为≥1700kg/m3,即每立方米中、高密度纤维板需消耗1700公斤以上木片;密度越高所消耗的木片就越多,反之则越少。
实用新型内容
本实用新型所要解决的技术问题在于提供一种防潮阻燃轻质装饰板,质量轻,大大减少了森林资源的浪费。
本实用新型是通过以下技术方案解决上述技术问题的:一种防潮阻燃轻质装饰板,包括从上至下依次设置的三聚氰胺浸渍耐磨纸层、三聚氰胺浸渍装饰纸层、防潮阻燃纤维板和三聚氰胺浸渍平衡纸层。
较佳地,所述防潮阻燃纤维板的厚度为6-18mm。
本实用新型的有益效果在于:不但质量轻,节约了物流成本,还大大减少了森林资源的浪费。
附图说明
下面参照附图结合实施例对本实用新型作进一步的描述。
图1为本实用新型防潮阻燃轻质装饰板的结构示意图。
具体实施方式
请参阅图1,一种防潮阻燃轻质装饰板,包括从上至下依次设置的三聚氰胺浸渍耐磨纸层1、三聚氰胺浸渍装饰纸层2、防潮阻燃纤维板3和三聚氰胺浸渍平衡纸层4;所述防潮阻燃纤维板3的厚度为6-18mm;所述防潮阻燃纤维板3为0.4~0.65g/cm3。
所述防潮阻燃轻质装饰板的生产方法如下:
(1)在铺装台上从下而上依次铺上三聚氰胺浸渍平衡纸、防潮阻燃纤维板3、三聚氰胺浸渍装饰纸和三聚氰胺浸渍耐磨纸,组成坯板。
(2)在热压机上,分别将上钢板固定于热压机的上热平板之下,将下钢板固定于热压机的下热平板上;接着在上钢板和上热平板之间、下钢板和下热平板之间分别铺设硅胶缓冲垫,使压贴过程中钢板不直接与热平板接触,缓解了热平板与钢板间的冲击力;然后启动热压机,将所述坯板安装于所述上钢板和下钢板之间。
(3)设定好压贴参数后闭合热压机,待热压机加压至设定的压力后开始计时,待达到压贴时间后打开压机完成压贴;压贴参数设置为:上钢板温度175℃~190℃,下钢板温度170℃~185℃,压力6MPa~13MPa,压贴时间15s~25s。
本实用新型的防潮阻燃轻质装饰板,按照《GB/T17657人造板及饰面人造板理化性能试验方法》GB/T18102-2007《浸渍纸层压木质地板》及GB8624-2006B级检测该装饰板的内结合强度、表面结合强度、吸水厚度膨胀率、甲醛释放量、燃烧性能,其检测结果如下表中所示:
Claims (2)
1.一种防潮阻燃轻质装饰板,其特征在于:包括从上至下依次设置的三聚氰胺浸渍耐磨纸层、三聚氰胺浸渍装饰纸层、防潮阻燃纤维板和三聚氰胺浸渍平衡纸层。
2.如权利要求1所述的防潮阻燃轻质装饰板,其特征在于:所述防潮阻燃纤维板的厚度为6-18mm。