CN202849573U - Anode oxidation device - Google Patents

Anode oxidation device Download PDF

Info

Publication number
CN202849573U
CN202849573U CN201220492370.8U CN201220492370U CN202849573U CN 202849573 U CN202849573 U CN 202849573U CN 201220492370 U CN201220492370 U CN 201220492370U CN 202849573 U CN202849573 U CN 202849573U
Authority
CN
China
Prior art keywords
anodic oxidation
main body
anode oxidation
oxidation device
overarm
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN201220492370.8U
Other languages
Chinese (zh)
Inventor
欧阳江林
孙学通
陈贤帅
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Jianchi Biotechnology Co ltd
Original Assignee
Guangzhou Institute of Advanced Technology of CAS
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangzhou Institute of Advanced Technology of CAS filed Critical Guangzhou Institute of Advanced Technology of CAS
Priority to CN201220492370.8U priority Critical patent/CN202849573U/en
Application granted granted Critical
Publication of CN202849573U publication Critical patent/CN202849573U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

The utility model discloses an anode oxidation device. The device comprises an anode oxidation pond and a rotary motor, wherein a hanging rack main body is arranged at the front end of the rotary output shaft of the rotary motor, and a plurality of suspension beams are uniformly distributed on the hanging rack main body; a clamp which can move horizontally along the suspension beams is arranged on each suspension beam; and the working end of the clamp clamps a metal workpiece and is inserted into the anode oxidation pond. According to the anode oxidation device, the hanging rack main body with the plurality of clamps is arranged on the rotary output shaft of the rotary motor, and the clamps capable of moving horizontally along the suspension beams can be used for adjusting the working distance between the metal workpiece and a cathode bar, so that the working distance between the metal workpiece surface and the cathode bar is always consistent, and an oxide layer with uniform thickness can be formed on the surface of the cylindrical metal workpiece; and a plurality of metal workpieces can be treated in once anode oxidation treatment, so that the efficiency of metal workpiece surface treatment can be greatly improved. The anode oxidation device can be applied to metal surface treatment.

Description

A kind of anodic oxidation device
Technical field
The utility model relates to field of metal surface treatment, particularly relates to a kind of anodic oxidation device for cylindric workpiece such as tooth implant, nails.
Background technology
Some metal or alloy, such as titanium or titanium alloy, the anode oxide film that its surface forms has higher hardness, wear resistance, anticorrosion, biological activity, is widely used in the mini-medical instrument field such as tooth implant, nail.Usually in the surface treatment for the metal works of tabular, sheet, cathode and anode be relatively and the position regularly, metal works is installed to carries out anodized surface behind the treating pond and process.And for the small workpiece of the cylindric irregularities such as tooth implant, nail, in anode oxidation process, the inconsistent oxidated layer thickness heterogeneity that will cause the surface to form of the operating distance between workpiece surface and negative electrode.
In anode oxidation process, if only process a metal works at every turn, whole process will be comparatively loaded down with trivial details, time-consuming, and efficient is extremely low, and the treatment effect that also is difficult to simultaneously the metal works that assurance handles at every turn is consistent.
So, need now a kind ofly can make zone of oxidation that surface of workpiece forms consistency of thickness and the anodic oxidation device of high treatment efficiency.
The utility model content
The purpose of this utility model is to provide a kind of anodic oxidation device, and it can make surface of workpiece form the zone of oxidation of consistency of thickness.
The solution that the utility model solves its technical problem is: a kind of anodic oxidation device, it comprises anodic oxidation pond and turning motor, the suspension bracket main body is installed on the front end of the rotating output shaft of described turning motor, a plurality of overarms have been evenly arranged on the described suspension bracket main body, the anchor clamps that an energy moves horizontally along overarm all are installed in the described overarm, behind the working end clamping metal works of described anchor clamps, insert in the anodic oxidation pond.
As further improvement in the technical proposal, be furnished with slide rail in the described overarm, be furnished with the slide block that is complementary with slide rail on the described anchor clamps.
As further improvement in the technical proposal, the bottom in described anodic oxidation pond is equipped with columned cathode bar, and the central shaft of described cathode bar and suspension bracket main center axle are on same vertical line.
As further improvement in the technical proposal, also comprise the direct supply that is arranged on outside the anodic oxidation pond, the positive pole of described direct supply is connected with rotating output shaft, and the negative pole of direct supply is connected with cathode bar.
As further improvement in the technical proposal, the quantity of described overarm is 4.
The beneficial effects of the utility model are: the utility model is equipped with the suspension bracket main body of a plurality of anchor clamps at a rotating output shaft around turning motor, can be with pending metal works clamping behind anchor clamps, the suspension bracket main body of rotation can drive each metal works and be rotated, the stirring action of the alternative stirring rod of metal works of rotation improves electrolytical mass transfer effect; And the operating distance that can regulate metal works and cathode bar along the anchor clamps that overarm moves horizontally, make surface of workpiece remain consistent with the operating distance of cathode bar, so can be implemented in the oxide skin that columned surface of workpiece forms the thickness homogeneous; One time anodic oxidation treatment can be processed a plurality of metal works, has improved widely the efficient that surface of workpiece is processed.
Description of drawings
Below in conjunction with accompanying drawing and example the utility model is further described.
Fig. 1 is structural representation of the present utility model.
Embodiment
Below in conjunction with accompanying drawing, describe the application of the utility model in anodic oxidation in detail.
With reference to Fig. 1, a kind of anodic oxidation device, it comprises anodic oxidation pond 4 and turning motor 2, on the front end of the rotating output shaft 22 of described turning motor 2 suspension bracket main body 1 is installed, a plurality of overarms 11 have been evenly arranged on the described suspension bracket main body 1, an energy all is installed along the moving anchor clamps 5 of overarm 11 translations in the described overarm 11, behind the working end clamping metal works 6 of described anchor clamps 5, inserts in the anodic oxidation pond 4.
Be further used as preferred embodiment, be furnished with slide rail 12 in the described overarm 11, be furnished with the slide block that is complementary with slide rail 12 on the described anchor clamps 5.
Be further used as preferred embodiment, the bottom in described anodic oxidation pond 4 is equipped with columned cathode bar 3, and the central shaft of the central shaft of described cathode bar 3 and suspension bracket main body 1 is on same vertical line.
Suspension bracket main body 1 at the front end of the rotating output shaft 22 of turning motor 2 has been symmetrical arranged a plurality of overarms 11, pending columned metal works 6 clampings can be finished rear-mounted in overarm 11, can regulate and control the operating distance of 3 of metal works 6 and cathode bars by slide rail 12 movable clamps 5 on 11 of hanging oneself from a beam.Drive 1 rotation of suspension bracket main body by rotating output shaft 22, the stirring action of the metal works 6 alternative stirring rod of rotation, improve electrolytical mass transfer effect, thereby only need to finish through an anodic oxidation anodic oxidation treatment of a plurality of metal works 6, can effectively improve metal works 6 surface-treated efficient; Metal works 6 surfaces can remain consistent operating distance with cathode bar 3 in rotary course, and then the surface of whole metal works 6 all experiences identical anodic oxidation treatment process, so can form in the metallic surface oxide skin of thickness homogeneous, can effectively improve the quality that surface of workpiece is processed.
Be further used as preferred embodiment, also comprise the direct supply 7 that is arranged on outside the anodic oxidation pond 4, the positive pole of described direct supply 7 is connected with rotating output shaft 22, and the negative pole of direct supply 7 is connected with cathode bar 3.
Turning motor 2 is connected with suspension bracket main body 1 by rotating output shaft 22, pending cylindric metal works clamping is finished rear-mounted in overarm 11, and fix the position of setting, insert in the anodic oxidation pond 4, inject electrolytic solution, then turning motor 2 opens direct supply 7, and can carry out the anodic oxidation treatment of a plurality of metal works.
Be further used as preferred embodiment, the quantity of described overarm 11 is 4.Can according to actual needs, the overarm 11 of different quantities be set.
More than be that preferred embodiments of the present utility model is specified, but the invention is not limited to described embodiment, those of ordinary skill in the art also can make all equivalent modifications or replacement under the prerequisite of the utility model spirit, the modification that these are equal to or replacement all are included in the application's claim limited range.

Claims (5)

1. anodic oxidation device, it is characterized in that: it comprises anodic oxidation pond (4) and turning motor (2), on the front end of the rotating output shaft (22) of described turning motor (2) suspension bracket main body (1) is installed, a plurality of overarms (11) have been evenly arranged on the described suspension bracket main body (1), the anchor clamps (5) that an energy moves horizontally along overarm (11) all are installed in the described overarm (11), behind the working end clamping metal works (6) of described anchor clamps (5), insert in the anodic oxidation pond (4).
2. anodic oxidation device according to claim 1 is characterized in that: be furnished with slide rail (12) in the described overarm (11), be furnished with the slide block that is complementary with slide rail (12) on the described anchor clamps (5).
3. anodic oxidation device according to claim 1, it is characterized in that: the bottom in described anodic oxidation pond (4) is equipped with columned cathode bar (3), and the central shaft of the central shaft of described cathode bar (3) and suspension bracket main body (1) is on same vertical line.
4. anodic oxidation device according to claim 3, it is characterized in that: also comprise being arranged on the outer direct supply (7) in anodic oxidation pond (4), the positive pole of described direct supply (7) is connected with rotating output shaft (22), and the negative pole of direct supply (7) is connected with cathode bar (3).
5. anodic oxidation device according to claim 1, it is characterized in that: the quantity of described overarm (11) is 4.
CN201220492370.8U 2012-09-25 2012-09-25 Anode oxidation device Expired - Lifetime CN202849573U (en)