CN202808675U - 一种无基材无溶剂透明双面胶带 - Google Patents
一种无基材无溶剂透明双面胶带 Download PDFInfo
- Publication number
- CN202808675U CN202808675U CN 201220300551 CN201220300551U CN202808675U CN 202808675 U CN202808675 U CN 202808675U CN 201220300551 CN201220300551 CN 201220300551 CN 201220300551 U CN201220300551 U CN 201220300551U CN 202808675 U CN202808675 U CN 202808675U
- Authority
- CN
- China
- Prior art keywords
- adhesive tape
- sided adhesive
- double
- transparent
- transparent double
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型公开了一种双面胶带,尤其是一种无基材无溶剂透明双面胶带。所述透明双面胶带由离型纸、丙烯酸透明胶水组成,在所述丙烯酸透明胶水层(2)的表面贴附有离型纸(1)。所述丙烯酸透明胶水层(2)直接贴于胶管(3)上,然后依次层叠缠绕,形成具有同心层叠缠绕的双面胶带产品。本实用新型的目的是提供一种无基材无溶剂透明双面胶带,所述双面胶带不含挥发性有机溶剂,具有优良的粘合效果,不残胶、溢胶,化学稳定性和热稳定性好,初粘性和持粘性好,解决了市面上常用无基材胶带含有挥发性溶剂,容易导所粘贴的致牌、标贴、标识、面板上的字体模糊或FPC腐蚀损坏的问题。
Description
技术领域
本发明涉及双面胶带,特别涉及一种无基材无溶剂透明双面胶带。
背景技术
目前,各种胶带已经成为电子、电器、五金等行业中不可缺少的物品。在丝网印刷、广告、航空、航天、医疗及工业设备、汽车、家电、电子市场等行业中,可用于铭牌、标贴、标识的粘贴。在手机、笔记本电脑、平板电脑、数码相机等电子产品中,可用于软性线路板的固定。此外,还可用于薄膜开关、防震泡沫、五金制品、塑胶制品、模切制品的粘贴等方面。目前,中国国内生产的无基材胶带,都是用含有溶剂的丙烯酸透明胶水涂布再附上离型纸压制而成。含有溶剂的无基材胶带会有残胶、溢胶等现象。尤其铭牌、标贴、标识、面板背胶后,微量的残留甲苯和面板上丝印的油墨产生反应,会导致铭牌、标贴、标识、面板上的字体模糊,严重的影响产品外观。FPC是Flexible Printed Circuit的简称,又称软性线路板、柔性印刷电路板、挠性线路板,简称软板或FPC,是以聚酰亚胺或聚酯薄膜为基材制成的一种具有高度可靠性,绝佳的可挠性印刷电路板,具有配线密度高、重量轻、厚度薄的特点,主要使用在手机、笔记本电脑、PDA、数码相机、LCM等很多产品。在FPC产品运用工艺上,需要将FPC板部分或整个固定在机体上—“背胶”。对这层背胶,FPC要求非常严格:1)不能含有溶剂。即便小量或微量的溶剂,都可以腐蚀软性线路板上的配线,造成FPC腐蚀损坏。2)具有很强的持粘力和内聚力。但市面上目前无基材胶带均含有溶剂,无法满足FPC应用的要求。
为了解决上述问题,本实用新型的发明者经过深入研究,发明了一种无基材透明双面胶带,这种胶带不含挥发性溶剂,例如甲苯,并且具有优良的粘合效果与优异的防水性能,模切加工性好、耐温性好,尺寸稳定性、热稳定性、化学稳定性好,初粘性和持粘性好,抗塑化,使用的时候不会残留胶水或胶带,能适用于更宽的温度范围和恶劣环境。
实用新型内容
本实用新型的目的是提供一种无基材透明双面胶带,所述双面胶带不含挥发性有机溶剂,具有优良的粘合效果,不残胶、溢胶,化学稳定性和热稳定性好,初粘性和持粘性好。解决了市面上常用无基材胶带含有挥发性溶剂,容易导所粘贴的致牌、标贴、标识、面板上的字体模糊或FPC腐蚀损坏的问题。
本实用新型提供的是一种无基材透明双面胶带,由离型纸、丙烯酸透明胶水组成,其特征在于,在所述丙烯酸透明胶水层的表面贴附有离型纸。该丙烯酸透明胶水层不含挥发性溶 剂,尤其不含有甲苯。所述无基材胶带,通过特殊工艺涂布再加UV光固化而成,整个生产过程中都不使用溶剂,而且厚度可控,所述透明双面胶带厚度为0.05mm-0.13mm,优选的双面胶带厚度为0.05mm或者0.13mm。所述丙烯酸透明压水层直接贴于固定环上,然后依次层叠缠绕,形成具有同心层叠缠绕的双面胶带产品。所述固定环可为各种材质的环状物体,优选为胶管,其形状可为任何封闭形状,如圆形、正方形、长方形、椭圆形,优选为圆形。
与同类产品比较,由于本实用新型无基材透明双面胶带不含有溶剂,且具有很强的持粘力和内聚力,因此可用于多种行业多种产品的粘贴上,具有广泛的应用价值。
附图说明
图1是本实用新型中无基材透明双面胶带截面图。
图2是本实用新型中无基材透明双面胶带示意图。
关于附图主要部分的说明
编号 | 名称 |
1 | 离型纸 |
2 | 丙烯酸透明胶水层 |
3 | 胶管 |
具体实施方式
下面结合附图及实施例对本实用新型作进一步描述,但这些实施例只是本实用新型的举例,本实用新型并不仅仅限于此。
实施例1
如图1和图2所示,一种无基材透明双面胶带,由丙烯酸透明胶水层2和离型纸1组成,所述丙烯酸透明胶水层2的表面贴附有离型纸1。该丙烯酸透明胶水层不含挥发性有机溶剂,厚度为0.05mm,直接贴于胶管3上,然后依次层叠缠绕,形成具有同心层叠缠绕的双面胶带产品。
实施例2
如图1和图2所示,一种无基材透明双面胶带,由丙烯酸透明胶水层2和离型纸1组成,所述丙烯酸透明胶水层2的表面贴附有离型纸1。该丙烯酸透明胶水层不含挥发性有机溶剂,厚度为0.13mm,直接贴于胶管3上,然后依次层叠缠绕,形成具有同心层叠缠绕的双面胶带产品。
应该注意的是,对于本实用新型的各种细节可以进行任意的修改,但毫无疑问,这些修改都将落入本实用新型的保护范围之内。
Claims (5)
1.一种无基材无溶剂透明双面胶带,由离型纸、丙烯酸透明胶水组成,其特征在于,在所述丙烯酸透明胶水层(2)的表面贴附有离型纸(1)。
2.根据权利要求1所述的无基材无溶剂透明双面胶带,其特征在于,所述透明双面胶带厚度为0.05mm-0.13mm。
3.根据权利要求1中所述的无基材无溶剂透明双面胶带,其特征在于,所述丙烯酸透明胶水层(2)直接贴于胶管(3)上,然后依次层叠缠绕。
4.根据权利要求2所述的无基材无溶剂透明双面胶带,其特征在于,所述透明双面胶带厚度为0.05mm。
5.根据权利要求4所述的无基材无溶剂透明双面胶带,其特征在于,所述透明双面胶带厚度为0.13mm。