CN202791109U - 玻璃钢加筋管直接头 - Google Patents
玻璃钢加筋管直接头 Download PDFInfo
- Publication number
- CN202791109U CN202791109U CN 201220364384 CN201220364384U CN202791109U CN 202791109 U CN202791109 U CN 202791109U CN 201220364384 CN201220364384 CN 201220364384 CN 201220364384 U CN201220364384 U CN 201220364384U CN 202791109 U CN202791109 U CN 202791109U
- Authority
- CN
- China
- Prior art keywords
- straight joint
- fiber reinforced
- reinforced plastic
- joint
- glass fiber
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn - After Issue
Abstract
本实用新型创造涉及一种玻璃钢加筋管直接头,其特征在于该直接头的形状为圆柱体,由上下两个圆柱体用螺栓连接在一起,接头的内壁为内螺纹;接头的外壁为光滑面,接头的上下圆柱体的左右两边分别设有法兰连接,法兰之间设有垫片,上下法兰和垫片用螺栓连接,接头左右两端的内腔分别嵌入连接玻璃钢加筋管道的内螺纹;所述的加筋管直接头的管子内径50~1000毫米,由纤维增强热固性树脂模压料SMC或BMC热压成型。本实用新型创造与现有技术相比,接头的内侧带有与加筋管外侧相配的螺纹槽,可以将管紧紧地连接在一起,强度高、使用方便、且耐腐蚀、使用寿命长、是一种简洁、牢固且快速的接头。
Description
[技术领域]
本实用新型创造涉及排水、排污、光纤、电缆、公路和铁路地下施工、水利灌溉、化工、矿山流体的输送管道接头,具体地说是一种玻璃钢加筋管直接头。
[背景技术]
随着我国经济的发展对市政工程、电力系统、化工行业、通信、水利灌溉安全的要求也日益提高,因此选择较好的输送管道更为重要,长期以来,输送管道采用金属材料制成,如钢管、铁管等,传统金属材料管道由于其生产过程能耗大、工序多以及实际使用中在潮湿、污积物、沿海盐雾等恶劣环境中的金属导电性、易锈蚀、寿命短、设施维护费用高等缺点而渐渐被淘汰,取而代之的是各种新型材质管道。现在市场上常见有玻璃钢复合材料缠绕成型的管道、挤出成型的PVC等各种单一的塑料管道以及各种中空塑料上设有加筋的塑料波纹管道。
一种新型玻璃钢加筋管的出现,其接头使用传统的接头已无法满足使用的要求,玻璃钢加筋管的连接无法像塑料波纹管那样进行焊接,,如果像塑料平管那样用胶粘直插,由于有波纹的存在,其密封不是很可靠,所以要寻找一种新的连接方法,来保证新管道的使用。
[发明内容]
本实用新型的目的就是为了解决上述矛盾,满足市场需求,提供一种结构新颖、安全可靠的根据玻璃钢模压制造技术原理,采用短纤维增强的模塑料SMC 或BMC模压成型来生产这种玻璃钢加筋管的直接头。
为实现上述目的,设计一种玻璃钢加筋管直接头,其特征在于该直接头的形状为圆柱体,由上下两个半圆柱体用螺栓连接在一起,直接头的内壁为内螺纹;直接头的外壁为光滑面,直接头的上下圆柱体的左右两边分别设有法兰连接,上下法兰之间设有垫片,上下法兰用螺栓连接,直接头左右两端的内腔分别嵌入连接玻璃钢加筋管道的内螺纹;所述的加筋管直接头的管子内径50~1000毫米,由短纤维增强热固性树脂模压料SMC或BMC热压成型。 所述的纤维采用玻璃纤维,碳纤维或玄武岩纤维或芳伦纤维。所述的树脂是环氧树脂或聚酯树脂或酚醛树脂或改性的高性能热固性树脂。高性能热固性树脂:脲醛树脂、三聚氰胺-甲醛树脂、不饱和树脂、聚氨酯、聚酰亚胺等增强树脂,包括替代玻璃的热固性树脂。所述的直接头内壁内螺纹与玻璃钢加筋管道的外螺纹相啮合。
本实用新型与现有技术相比,其直接头的内侧带有与加筋管外侧相配的螺纹槽,可以将管紧紧地连接在一起,直接头材料采用短纤维增强热固性树脂模压料SMC或BMC热压而成,强度高、使用方便,且耐腐蚀、使用寿命长、是一种简洁、牢固且快速的接头。
[附图说明]
图1为本实用新型创造的产品构造的示意图;
图2为本实用新型创造图1的纵向示意图;
图3为本实用新型创造图1的横向示意图;
参见图1,其中:1为左端的玻璃钢加筋管,2为加筋管直接头;
参见图2,其中:3为耐腐蚀螺栓,4为胶垫;
参见图3,其中:5为直接头的内螺纹槽;
指定图1为本实用新型的摘要附图。
[具体实施方式]
下面结合附图,对本实用新型创造做进一步详细说明,这种装置的方法和原理对本专业的人来说是非常清楚的。应当理解,此处所描述的具体实施例仅用于解释本实用新型,并不用于限定本实用新型。
图1给出了本接头的构造示意图。
参见图1,将要连接的加筋管(1)拼在一起,接头圆柱体上下分开,将上下圆柱体上的螺纹槽(5)对准加筋管(1)表面的外螺纹,合拢上下圆柱体的直接头,加上胶垫,锁紧螺栓即可完成本实用新型。直接头所用材料为短纤维增强模压料SMC或BMC,树脂材料为环氧、聚酯或酚醛树脂。
Claims (4)
1.一种玻璃钢加筋管直接头,其特征在于该直接头的形状为圆柱体,由上下两个半圆柱体用螺栓连接在一起,直接头的内壁为内螺纹;直接头的外壁为光滑面,直接头的上下半圆柱体的左右两边分别设有法兰连接,上下法兰之间设有垫片,上下法兰由螺栓连接,直接头左右两端的内腔分别嵌入连接玻璃钢加筋管道的内螺纹;所述的加筋管直接头的管子内径50~1000毫米。
2.根据权利要求1所述的玻璃钢加筋管直接头,其特征在于直接头的材料采用短纤维增强热固性树脂模压料SMC或BMC热压成型。
3.根据权利要求1所述的玻璃钢加筋管直接头,其特征在于所述的树脂是环氧树脂或聚酯树脂或酚醛树脂或改性的高性能热固性树脂。
4.根据权利要求1所述的玻璃钢加筋管直接头,其特征在于所述的直接头内壁的螺纹与玻璃钢加筋管道的外螺纹相啮合。