CN202746797U - 一种带有双胶圈钢插口接头的钢筋混凝土管 - Google Patents
一种带有双胶圈钢插口接头的钢筋混凝土管 Download PDFInfo
- Publication number
- CN202746797U CN202746797U CN 201220431723 CN201220431723U CN202746797U CN 202746797 U CN202746797 U CN 202746797U CN 201220431723 CN201220431723 CN 201220431723 CN 201220431723 U CN201220431723 U CN 201220431723U CN 202746797 U CN202746797 U CN 202746797U
- Authority
- CN
- China
- Prior art keywords
- reinforced concrete
- concrete pipe
- rubber ring
- pipe
- steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种钢筋混凝土管,特别涉及一种污水排放用的钢筋混凝土管,本实用新型由钢承口(1)、胶圈槽一(2)、胶圈槽二(3)、试压孔(4)、钢插口(5)、钢筋笼骨架(6)、混凝土(7)组成。本实用新型可较好地解决了钢筋混凝土管接口要整条管段安装完成后才能加压检验的弊端,既节约了检验用水,又解决了因修理不合格接口而二次开挖管坑的繁琐,应用双胶圈的柔性接口连接对提高钢筋混凝土管道连接质量有着重要的意义。
Description
技术领域
本实用新型涉及一种钢筋混凝土管,特别涉及一种污水排放用的钢筋混凝土管。
背景技术
钢筋混凝土管广泛应用于雨水、污水、引水及农田排灌等工程中,管子的连接方式也多种多样,通常分为柔性接头管和刚性接头管。在排污管道工程中,因管节短,接口多,管道接口成为工程中重要的组成部分,其质量好坏直接影响工程质量,也影响整个排污系统的正常运行。目前,在管道安装施工过程中不能对单个连接接口进行加压试验,其接口的连接是否漏水要等整段管安装后,将整段管道灌满水才能检验接口的连接质量,工程质量隐患大,对不合格接口进行修补,费时费力并给实际施工带来不少困难。
发明内容
本实用新型的目的在于设计一种带有双胶圈钢插口接头的钢筋混凝土管,使得通过在两个胶圈之间的空隙进行水压检验,来解决钢筋混凝土管接口要整条管段安装完成后才能加压检验的弊端。
一种带有双胶圈钢插口接头的钢筋混凝土管的基本原理是在钢插口设置两处胶圈槽,并在两槽之间预设注水试压孔,槽内放置密封胶圈,通过与钢承口的对接挤压胶圈进行闭水,可通过在两个胶圈槽之间的打压孔进行接口水压检验,进而可以对单个连接接口进行质量检验。
一种带有双胶圈钢插口接头的钢筋混凝土管基本结构由钢承口(1)、胶圈槽一(2)、胶圈槽二(3)、试压孔(4)、钢插口(5)、钢筋笼骨架(6)、混凝土(7)组成,钢承口(1)与钢插口(4)分别焊接在钢筋笼骨架(5)的两端,用混凝土(7)将其包裹,在钢插口(4)上设有胶圈槽一(2)和胶圈槽二(3),在两胶圈槽之间开有试压孔(4),试压孔(4)内带有螺纹,可用螺栓封堵。
本实用新型可较好地解决了钢筋混凝土管接口要整条管段安装完成后才能加压检验的弊端,既节约了检验用水,又解决了因修理不合格接口而二次开挖管坑的繁琐,应用双胶圈的柔性接口连接对提高钢筋混凝土管道连接质量有着重要的意义。
附图说明
附图1为本实用新型的结构示意图。由钢承口(1)、胶圈槽一(2)、胶圈槽二(3)、试压孔(4)、钢插口(5)、钢筋笼骨架(6)、混凝土(7)组成。
具体实施方式
在实际使用过程中,钢承口(1)与钢插口(5)分别焊接在钢筋笼骨架(6)的两端,用混凝土(7)将其包裹。两管道对接后,通过对胶圈槽一(2)和胶圈槽二(3)之间预设的试压孔(4)加压,进行水压试验,来检验单个连接接口是否漏水,打压合格后用螺栓将试压孔(4)堵死。
Claims (2)
1.一种带有双胶圈钢插口接头的钢筋混凝土管,其特征在于:由钢承口(1)、胶圈槽一(2)、胶圈槽二(3)、试压孔(4)、钢插口(5)、钢筋笼骨架(6)、混凝土(7)组成,钢承口(1)与钢插口(4)分别焊接在钢筋笼骨架(5)的两端,用混凝土(7)将其包裹。
2.如权利要求1所述的一种带有双胶圈钢插口接头的钢筋混凝土管,其特征在于:所述在钢插口(4)上设有胶圈槽一(2)和胶圈槽二(3),在两胶圈槽之间开有试压孔(4),试压孔(4)内带有螺纹,可用螺栓封堵。