CN202730277U - 一种阳极氧化用阴极系统 - Google Patents
一种阳极氧化用阴极系统 Download PDFInfo
- Publication number
- CN202730277U CN202730277U CN 201220285758 CN201220285758U CN202730277U CN 202730277 U CN202730277 U CN 202730277U CN 201220285758 CN201220285758 CN 201220285758 CN 201220285758 U CN201220285758 U CN 201220285758U CN 202730277 U CN202730277 U CN 202730277U
- Authority
- CN
- China
- Prior art keywords
- cylinder
- cathode
- oxidation
- negative electrode
- cathode compartment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种阳极氧化用阴极系统,包括:放置所述阴极的底座,所述底座上有精确的导轨,在所述导轨上固定有气缸,在所述气缸上固定有阴极室,在所述阴极室内插有所述阴极;在所述气缸的驱动下所述阴极室带动所述阴极在所述导轨上移动。所述底座由四根螺栓固定在工作台上。所述气缸上具有将所述阴极室定位在所述气缸上的定位销。采用本实用新型的阴极系统可以实现对阀体活塞孔的局部氧化,配合自动控制技术,可以通过气缸的快速移动实现对产品的氧化,提高氧化的效率;电解液能保持高速流动,带走氧化时产生的热量。
Description
技术领域
本实用新型涉及一种阴极系统,特别是涉及一种ABS阀体的活塞孔氧化用的阴极系统。
背景技术
在现代汽车产业中,越来越多的汽车使用Anti-locked Braking System系统,即防抱死刹车系统(以下缩写为ABS)。而ABS阀体的活塞孔为了达到耐磨性要求,通常都需要进行阳极氧化处理。传统的阳极氧化方法是把整个ABS阀体置于氧化槽液中进行整体氧化,其不足之处有:第一:不能对活塞孔有针对性地进行氧化;第二:对整个阀体进行氧化,导致电流分散;第三,造成能源浪费。
发明内容
鉴于以上问题,本实用新型的目的在于,提供一种ABS阀体活塞孔氧化用的阴极系统,将此阴极安装在工作台上,通过工作台上的气缸带动阴极移动可以实现对活塞孔的局部氧化。
本实用新型的技术解决方案如下:
一种阳极氧化用阴极系统,包括:放置所述阴极的底座,所述底座上有精确的导轨,在所述导轨上固定有气缸,在所述气缸上固定有阴极室,在所述阴极室内插有所述阴极;在所述气缸的驱动下所述阴极室带动所述阴极在所述导轨上移动。并且,氧化生产时通过气缸的移动带动阴极进入阀体的活塞孔,氧化完成时气缸带动阴极退出活塞孔。
所述底座由四根螺栓固定在工作台上,所述底座与导轨的材料为不锈钢。
所述气缸上有两个定位销,通过定位销把阴极室准确的定位在气缸体上。
所述阴极室通过螺栓固定在气缸上,阴极室的有中心孔以供阴极通过,在阴极
室的侧面开有供氧化液流进的通道,阴极室的末端有密封圈、阴极衬套和紧固螺栓。所述阴极室的材料为不导电的硬质塑料。
所述阴极有阴极头和阴极体两部分,在这两部分之间通过0形圈进行减震;阴
极体通过螺栓固定在阴极室上;在阴极体上通过螺栓固定有阴极接线柱,氧化时接电源的阴极。所述的阴极头材质为耐腐蚀的钛铂合金,阴极体的材质为不锈钢。
与现有技术相比,本实用新型的技术效果如下:
第一:采用本实用新型的阴极系统可以实现对阀体活塞孔的局部氧化;
第二:采用本实用新型的阴极系统,配合自动控制技术,可以通过气缸的快速移动实现对产品的氧化,提高氧化的效率;
第三:采用的阴极系统在氧化过程中,电解液能保持高速流动,带走氧化时产生的热量。
附图说明
图1是本实用新型阴极系统的结构示意图。
具体实施方式
下面结合实施例和附图对本实用新型作进一步说明,但不应以此限制本实用新型的保护范围。
实施例1
请先参阅图1,图1是本实用新型阴极系统的结构示意图。由图1可知,一种阀体活塞孔氧化用阴极系统,构成为:阴极底座1作为阴极系统的基体,在底座1上分别固定精确导轨2,在导轨2上配有可沿导轨移动的气缸3,在气缸3上设有两个定位销4,底座1通过四根螺栓5固定在工作台上。阴极室6 通过螺栓15经定位销固定在气缸3上,氧化时电解液经导管14导入阴极室接口13进入壁内管道,经过滤网7,从阴极衬套8与阴极头16之间的间隙流进待氧化的活塞孔,紧固螺栓10配合密封垫9及密封圈12将阴极衬套8固定在阴极室6上。阴极体19通过螺栓22配合密封圈18将阴极体19固定在阴极室6上,在阴极体19和阴极头16之间有一减震垫17,通过螺栓21将接线柱20紧固在阴极体19上,在氧化时,气缸带动阴极系统向前运动,阴极头16进入阀体活塞孔,密封衬套11与阀体孔壁紧密接触,电解液经阴极头16与阴极衬套8之间的空隙进入活塞孔,当氧化完成时,气缸带动阴极系统回到原位,阴极头16从而退出阀体活塞孔。
实验表明,要对ABS阀体的活塞孔进行局部氧化,采用本实用新型的氧化阴极系统,通过在活塞孔两边对称地放置两个这样的阴极系统,配合一定的自动控制技术,氧化时电解液从一边进入,经过阀体活塞孔后从另一个阴极流出,在此过程中通过一定的电流就可以对活塞孔进行局部氧化。由于只对活塞孔进行了氧化处理,因此氧化效率高,氧化时间短。
Claims (7)
1.一种阳极氧化用阴极系统,其特征在于,包括:放置所述阴极的底座,所述底座上有精确的导轨,在所述导轨上固定有气缸,在所述气缸上固定有阴极室,在所述阴极室内插有所述阴极;在所述气缸的驱动下所述阴极室带动所述阴极在所述导轨上移动。
2.根据权利要求1所述的阴极系统,其特征在于,所述底座由四根螺栓固定在工作台上。
3.根据权利要求1所述的阴极系统,其特征在于,所述气缸上具有将所述阴极室定位在所述气缸上的定位销。
4.根据权利要求1所述的阴极系统,其特征在于,所述阴极室通过螺栓固定在所述气缸上。
5.根据权利要求1所述的阴极系统,其特征在于,所述阴极室的侧面开有供氧化液流进的通道,所述阴极室的末端有密封圈、阴极衬套和紧固螺栓。
6.根据权利要求1所述的阴极系统,其特征在于,所述阴极包括阴极头和阴极体两部分,在这两部分之间设置有减震0形圈。
7.根据权利要求6所述的阴极系统,其特征在于,所述阴极本体通过螺栓固定在所述阴极室上,且在所述阴极体上通过螺栓固定有阴极接线柱。