Prior art keywords
sleeve
spiral grooves
coiling sleeve
straight
rubber sleeve
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201220292112
Other languages
English (en)
Inventor
于顺兵
宋伟
刘丹
张民
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shougang Group Co Ltd
Original Assignee
Shougang Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shougang Corp filed Critical Shougang Corp
Priority to CN 201220292112 priority Critical patent/CN202715656U/zh
Application granted granted Critical
Publication of CN202715656U publication Critical patent/CN202715656U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Landscapes

  • Winding, Rewinding, Material Storage Devices (AREA)

Abstract

本实用新型提供了一种冷轧薄带钢卷取套筒,包括一橡胶套筒,所述橡胶套筒的外表面设置有螺旋沟槽、内表面设置有直线沟槽,所述螺旋沟槽共72条,双向平均分布在所述橡胶套筒外表面交织成网格状,所述直线沟槽共24条,在平行于所述橡胶套筒的轴线方向上、平均分布在所述橡胶套筒的内表面。本实用新型提供的薄带钢卷取套筒对改善钢卷最内圈芯轴压痕和带头压痕缺陷具有明显的改善作用,能够极大的提高带钢整卷的表面质量。

Description

一种冷轧薄带钢卷取套筒
技术领域
本实用新型涉及冷轧板带轧制技术领域,特别涉及一种冷轧薄带钢卷取套筒。
背景技术
随着冷轧薄板生产工艺技术水平、制作精度等的日益提高,钢板的质量水平已经达到了空前的高度,与此同时,冷轧薄板的最终用户对钢板的质量要求也更加严格和苛刻,如一些国际汽车制造厂商要求汽车面板整卷无任何缺陷交货,这对各钢铁企业来说都是非常具有挑战性的工作。
冷轧薄板大多数产品均以钢卷状态交货,一般来说钢卷整卷的表面质量是有区别的,主要是由于钢卷最内圈在卷取开始和卸卷时和卷取机芯轴要产生相对运动,卷取过程中钢卷最内圈和卷取机芯轴时刻保持紧密接触,因此一般钢卷最内圈容易产生一些缺陷,主要是卷取机芯轴压痕和内圈带头压痕缺陷。一般冷轧薄板生产企业卷取机芯轴上都会安装卷取套筒,用套筒来减少钢卷最内圈压痕缺陷和卷取擦伤缺陷,但是由于卷取套筒设计不合理,一般在外表面不开沟槽,内表面开螺旋槽,导致绝大多数钢卷最内圈都存在100米左右的芯轴压痕和带头压痕缺陷,因此,如何通过工艺或者设备改进来提高钢卷最内圈的带钢表面质量是各大钢厂都面临的问题。
实用新型内容
本实用新型所要解决的技术问题是提供一种冷轧薄带钢卷取套筒,用于解决目前存在的钢卷最内圈芯轴压痕和带头压痕缺陷,提高整个钢卷的质量水平。
为解决上述技术问题,本实用新型提供了一种冷轧薄带钢卷取套筒,包括一橡胶套筒,所述橡胶套筒的外表面设置有螺旋沟槽、内表面设置有直线沟槽。
进一步地,所述螺旋沟槽是多条,双向平均分布在所述橡胶套筒外表面交织成网格状。
进一步地,所述螺旋沟槽是72条。
进一步地,所述螺旋沟槽的深度3mm、宽度3mm、底倒圆角R1.5mm。
进一步地,所述螺旋沟槽的导程长1000mm。
进一步地,所述直线沟槽共24条,在平行于所述橡胶套筒的轴线方向上、平均分布在所述橡胶套筒的内表面。
进一步地,所述直线沟槽的深度3mm、宽度3mm、底倒圆角R1.5mm。
本实用新型提供的冷轧薄带钢卷取套筒通过卷取套筒外表面的网格螺旋沟槽可以防止钢卷最内圈带钢头部进入槽内产生翘起造成带头压痕,通过卷取套筒内表面的直线沟槽可以排除空气,保证卷取套筒与芯轴紧密抱紧,避免出现钢卷卷取过程中打滑而产生擦伤缺陷;经过实际使用能够消除钢卷卷取擦伤缺陷,并且带头压痕和芯轴压痕缺陷能够控制在15米以内,与一般卷取套筒外表面不开槽、内表面开螺旋槽的设计相比,提高了带钢整卷的表面质量,为用户能够百分之百的使用整个钢卷创造了条件。
附图说明
图1为本实用新型实施例提供的卷取套筒结构示意图。
图2为本实用新型实施例提供的卷取套筒外表面展开的部分示意图。
图3为本实用新型实施例提供的卷取套筒内表面展开的部分示意图。
具体实施方式
参见图1、图2和图3,本实用新型实施例提供的一种冷轧薄带钢卷取套筒,包括一橡胶套筒1,橡胶套筒1的外表面设置有螺旋沟槽2、内表面设置有直线沟槽3。
其中,螺旋沟槽2共72条,双向平均分布在橡胶套筒1外表面交织成网格状。
其中,螺旋沟槽2的深度3mm、宽度3mm、底倒圆角R1.5mm。
其中,螺旋沟槽2的导程长1000mm。
其中,直线沟槽3共24条,在平行于橡胶套筒1的轴线方向上、平均分布在橡胶套筒1的内表面。
其中,直线沟槽3的深度3mm、宽度3mm、底倒圆角R1.5mm。
实际工作时,将卷取套筒1安装到卷取机芯轴上,卷取机芯轴进行一次膨胀,由于卷取套筒内表面加工有直线型沟槽,能够保证卷取套筒内表面与芯轴逐步接触的过程中,卷取套筒内表面与芯轴之间的空气被完全排出,从而保证实现卷取套筒内壁与芯轴的压紧,避免出现卷取过程中套筒与芯轴打滑而产生钢卷擦划伤缺陷和芯轴扇形块造成的芯轴压痕缺陷;然后,助卷器缩回并抱住卷取机芯轴和卷取套筒;之后,带钢进行穿带,穿带时带钢头部首先与卷取机芯轴上的卷取套筒外表面接触,由于卷取套筒外表面有网格状沟槽,与一般卷取套筒外表面带直线状沟槽的结构相比,能够防止带钢头部进入卷取套筒外表面的沟槽内,避免造成带头翘起,从而减少带头压痕缺陷,然后正常进行卷取,卷取完成后正常卸卷操作。
本实用新型提供的薄带钢卷取套筒对改善钢卷最内圈芯轴压痕和带头压痕缺陷具有非常明显的改善作用,能够极大的提高带钢整卷的表面质量。
最后所应说明的是,以上具体实施方式仅用以说明本实用新型的技术方案而非限制,尽管参照实例对本实用新型进行了详细说明,本领域的普通技术人员应当理解,可以对本实用新型的技术方案进行修改或者等同替换,而不脱离本实用新型技术方案的精神和范围,其均应涵盖在本实用新型的权利要求范围当中。

Claims (7)

1.一种冷轧薄带钢卷取套筒,包括一橡胶套筒,其特征在于:所述橡胶套筒的外表面设置有螺旋沟槽、内表面设置有直线沟槽。
2.根据权利要求1所述的卷取套筒,其特征在于:所述螺旋沟槽是多条,双向平均分布在所述橡胶套筒外表面交织成网格状。
3.根据权利要求2所述的卷取套筒,其特征在于:所述螺旋沟槽是72条。
4.根据权利要求2所述的卷取套筒,其特征在于:所述螺旋沟槽的深度3mm、宽度3mm、底倒圆角R1.5mm。
5.根据权利要求2所述的卷取套筒,其特征在于:所述螺旋沟槽的导程长1000mm。
6.根据权利要求1所述的卷取套筒,其特征在于:所述直线沟槽共24条,在平行于所述橡胶套筒的轴线方向上、平均分布在所述橡胶套筒的内表面。
7.根据权利要求6所述的卷取套筒,其特征在于:所述直线沟槽的深度3mm、宽度3mm、底倒圆角R1.5mm。
CN 201220292112 2012-06-18 2012-06-18 一种冷轧薄带钢卷取套筒 Expired - Fee Related CN202715656U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201220292112 CN202715656U (zh) 2012-06-18 2012-06-18 一种冷轧薄带钢卷取套筒

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201220292112 CN202715656U (zh) 2012-06-18 2012-06-18 一种冷轧薄带钢卷取套筒

Publications (1)

Publication Number Publication Date
CN202715656U true CN202715656U (zh) 2013-02-06

Family

ID=47617495

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201220292112 Expired - Fee Related CN202715656U (zh) 2012-06-18 2012-06-18 一种冷轧薄带钢卷取套筒

Country Status (1)

Country Link
CN (1) CN202715656U (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108031727A (zh) * 2018-01-11 2018-05-15 北京市城南橡塑技术研究所 冷轧卷取机芯轴用橡胶套筒

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108031727A (zh) * 2018-01-11 2018-05-15 北京市城南橡塑技术研究所 冷轧卷取机芯轴用橡胶套筒
CN108031727B (zh) * 2018-01-11 2024-04-12 北京市城南橡塑技术研究所 冷轧卷取机芯轴用橡胶套筒

Similar Documents

Publication Publication Date Title
CN102974684A (zh) 一种碳钢板型材导轨冷弯成型的方法
CN202715656U (zh) 一种冷轧薄带钢卷取套筒
CN111774455A (zh) 一种集装箱底侧梁板材的连续反向冷弯成型方法
CN201220252Y (zh) 一种复杂形状工件的压延成型模具
CN104438949B (zh) 一种列车减震支架加工工艺
CN203209466U (zh) 一种矩形截面钢丝辊拉组合成形工艺的生产设备
CN104475543B (zh) 超薄钢带连续滚冲装置
CN202180135U (zh) 铁道车辆塞拉门铰链卷圆成型模具
CN104985037B (zh) 冷弯波纹板成形方法
CN103240372A (zh) 无内胎轮辋板材轧制模具及轧制方法
CN101435476B (zh) 增加负荷检测次数的弹簧生产工艺流程
CN102513427A (zh) 一种基于闸压床的长薄钣金零件边卷圆成形方法及模具
CN201455047U (zh) 助卷辊在线抛光器
CN202180109U (zh) 一种防止划伤钢卷内圈的卷取机卷筒
CN204194516U (zh) 一种分切铝带在线修边装置
CN203781453U (zh) 自动化丝网卷制设备中的纠偏装置
CN103252384B (zh) 一种分卷平整机组卷取机卷筒
CN204866839U (zh) 镍带中冷轧辊
CN204657844U (zh) 可移动式除毛刺机
CN206229911U (zh) 一种冲压模具冲头
CN206122435U (zh) 小尺寸波纹薄板折边装置
CN204234461U (zh) 一种能消除带钢表面点线状缺陷的立辊
CN203221169U (zh) 无内胎轮辋板材轧制模具
CN204096707U (zh) 一种铜箔收卷装置
CN102962310B (zh) 不等长弧形钣金件坯料制造方法

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
EE01 Entry into force of recordation of patent licensing contract

Assignee: BEIJING SHOUGANG COLD ROLLING THIN PLATE CO., LTD.

Assignor: Capital Iron & Steel General Company

Contract record no.: 2015990001019

Denomination of utility model: Cold rolling thin strip steel reel-up sleeve

Granted publication date: 20130206

License type: Common License

Record date: 20151209

LICC Enforcement, change and cancellation of record of contracts on the licence for exploitation of a patent or utility model
CP01 Change in the name or title of a patent holder
CP01 Change in the name or title of a patent holder

Address after: 100041 Shijingshan Road, Beijing, No. 68, No.

Patentee after: Shougang Group Co. Ltd.

Address before: 100041 Shijingshan Road, Beijing, No. 68, No.

Patentee before: Capital Iron & Steel General Company

CF01 Termination of patent right due to non-payment of annual fee
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20130206

Termination date: 20210618