CN202640939U - 硅胶固化深度测量槽 - Google Patents
硅胶固化深度测量槽 Download PDFInfo
- Publication number
- CN202640939U CN202640939U CN 201220248466 CN201220248466U CN202640939U CN 202640939 U CN202640939 U CN 202640939U CN 201220248466 CN201220248466 CN 201220248466 CN 201220248466 U CN201220248466 U CN 201220248466U CN 202640939 U CN202640939 U CN 202640939U
- Authority
- CN
- China
- Prior art keywords
- silica gel
- depth
- groove
- substrate
- accepting groove
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种硅胶固化深度测量槽,包括长方体的基板,所述基板的表面沿长度方向开设有一个容纳硅胶的收容槽,所述收容槽的深度随所述基板的长度方向逐渐变大,所述基板位于所述收容槽的边缘设有一个深度刻度尺,所述收容槽内每一点的深度与该点在所述深度刻度尺上的刻度相对应。上述硅胶固化深度测量槽确保了实验结果的准确性,还可以提高工作效率、减少样品的浪费。该测试槽结构简单,灵活轻便且可反复使用。
Description
技术领域
本实用新型涉及太阳能光伏领域,特别是一种用于测试硅胶固化深度和固化时间的测试槽。
背景技术
光伏组件目前大致可以分为非聚光的平板太阳能电池组件、聚光光伏发电组件和薄膜电池组件等三类。在光伏组件层压工艺中,组件制造商常常使用硅胶来密封所有的零部件,以保证光伏组件的材料层的安全。随着太阳能光伏技术的日新月异的发展以及应对残酷的市场竞争环境需要,急需加强对光伏组件封装原材料的品质控制,以保证原材料测试结果的准确性、减少测试样品的浪费。然而现有的硅胶固化深度测试工具存在结构单一、工作效率低下、浪费样品的缺点,而且测试结果具有较大的误差。
实用新型内容
基于此,有必要提供一种能够较准确测试硅胶样品的固化深度和固化时间的测试槽。
一种硅胶固化深度测量槽,包括长方体的基板,所述基板的表面沿长度方向开设有一个容纳硅胶的收容槽,所述收容槽的深度随所述基板的长度方向逐渐变大,所述基板位于所述收容槽的边缘设有一个深度刻度尺,所述收容槽内每一点的深度与该点在所述深度刻度尺上的刻度相对应。
在其中一个实施例中,所述收容槽的底面与所述基板的表面形成夹角为3°~5°。
上述硅胶固化深度测量槽确保了实验结果的准确性,还可以提高工作效率、减少样品的浪费。该测试槽结构简单,灵活轻便且可反复使用。
附图说明
图1为一实施方式的硅胶固化深度测量槽的结构示意图;
图2为图1所示硅胶固化深度测量槽的剖面示意图。
具体实施方式
请同时参阅图1和图2,一实施方式的硅胶固化深度测量槽100是由聚对苯二甲酸丁二醇酯、聚偏氟乙烯或聚四氟乙烯等材料制成,其包括一个大致为长方形的基板10。基板10的上表面上沿长度方向开设有一个容纳硅胶的收容槽12。收容槽12大致呈方形,其深度是逐渐变化的。例如,从基板10的一端开始只到基板10的另一端,收容槽12的深度是逐渐增大的。收容槽12的底面与基板10的表面形成夹角优选为3°~5°。
基板10的上表面位于所述收容槽的边缘还设有一个深度刻度尺14。深度刻度尺14可以是直接印刻在基板10上的,也可以是预先成型后粘贴在基板10上的。收容槽12内每一点的深度与该点在深度刻度尺14上的刻度相对应,即深度刻度尺14上的刻度刚好反应了这一位置的深度。
该硅胶固化深度测量槽100的使用方法如下:当进行硅胶薄固化深度和固化时间测试时,将适量的硅胶从收容槽12较深的一端沿收容槽12的长度方向挤入,手握刮刀贴紧基板10的表面并匀速向前拉动至收容槽12较浅的一端。将测试槽和样品放置在测试环境中,待一定时间后,硅胶将形成与收容槽12的形状相同的前深后浅的类似三明治的形状。此时,从收容槽12较浅的一端将硅胶样品揭起至已固化位置,并记录深度刻度尺14显示的该位置槽深度和测试时间,便可得到硅胶固化深度与固化时间的关系。连续测试多个时间段的固化深度即可完成测试。
上述硅胶固化深度测量槽确保了实验结果的准确性,还可以提高工作效率、减少样品的浪费。该测试槽结构简单,灵活轻便且可反复使用。
以上所述实施例仅表达了本实用新型的几种实施方式,其描述较为具体和详细,但并不能因此而理解为对本实用新型专利范围的限制。应当指出的是,对于本领域的普通技术人员来说,在不脱离本实用新型构思的前提下,还可以做出若干变形和改进,这些都属于本实用新型的保护范围。因此,本实用新型专利的保护范围应以所附权利要求为准。
Claims (2)
1.一种硅胶固化深度测量槽,其特征在于,包括长方体的基板,所述基板的表面沿长度方向开设有一个容纳硅胶的收容槽,所述收容槽的深度随所述基板的长度方向逐渐变大,所述基板位于所述收容槽的边缘设有一个深度刻度尺,所述收容槽内每一点的深度与该点在所述深度刻度尺上的刻度相对应。
2.根据权利要求1所述的硅胶固化深度测量槽,其特征在于,所述收容槽的底面与所述基板的表面形成夹角为3°~5°。