CN103743893B - 一种水泥混凝土路面板内湿度梯度测试方法 - Google Patents

一种水泥混凝土路面板内湿度梯度测试方法 Download PDF

Info

Publication number
CN103743893B
CN103743893B CN201310752709.2A CN201310752709A CN103743893B CN 103743893 B CN103743893 B CN 103743893B CN 201310752709 A CN201310752709 A CN 201310752709A CN 103743893 B CN103743893 B CN 103743893B
Authority
CN
China
Prior art keywords
pvc
humidity
test point
cement concrete
road deck
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310752709.2A
Other languages
English (en)
Other versions
CN103743893A (zh
Inventor
魏亚
高翔
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tsinghua University
Original Assignee
Tsinghua University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tsinghua University filed Critical Tsinghua University
Priority to CN201310752709.2A priority Critical patent/CN103743893B/zh
Publication of CN103743893A publication Critical patent/CN103743893A/zh
Application granted granted Critical
Publication of CN103743893B publication Critical patent/CN103743893B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种水泥混凝土路面板内湿度梯度测试方法,根据上下密、中间疏的原则确定路面板沿深度方向的测试点数目和位置;在水泥混凝土路面铺筑完成后,在测试点插入一个底端密封侧边开口的PVC套管,并在PVC套管中插入PVC插管;待混凝土初凝结束后,将PVC插管取出,插入湿度传感器,并在封口处涂抹密封胶;将湿度传感器的接线头连接到采集仪上,接通电路进行路面板湿度的测量,本发明可确保路面的测量数据较为准确、全面,同时测试工作所需的安装装置较少、简单易行,且测试工作的重复性较强。

Description

一种水泥混凝土路面板内湿度梯度测试方法
技术领域
本发明属于道路施工检测技术领域,特别涉及一种水泥混凝土路面板内湿度梯度测试方法。
背景技术
湿度的不均匀分布导致路面板发生体积变化,这种变化受到约束时路面将产生巨大的翘曲应力,是路面板产生破坏的主要因素之一。路面板内的湿度梯度是研究路面板由湿度引起的翘曲应力的重要参数之一。目前一般采用湿度传感器来测试混凝土结构物中内部的湿度,但是湿度传感器的布置方案以及确保传感器准确采集预设位置湿度数据的方法没有统一的要求,这样可能会使测试工作费时费力,不能高效、准确地搜集敏感区域的湿度数据,进而影响到后续翘曲应力的计算。
发明内容
为了克服上述现有技术的缺点,本发明的目的在于提供一种水泥混凝土路面板内湿度梯度测试方法,能实现水泥混凝土路面板沿深度方向湿度分布的连续测量。
为了实现上述目的,本发明采用的技术方案是:
一种水泥混凝土路面板内湿度梯度测试方法,包括如下步骤:
(1)根据上下密、中间疏的原则确定路面板沿深度方向的测试点数目和位置;
(2)在水泥混凝土路面铺筑完成后,在测试点插入一个底端密封侧边开口的PVC套管,并在PVC套管中插入PVC插管;
(3)待混凝土初凝结束后,将PVC插管取出,插入湿度传感器,并在封口处涂抹密封胶;
(4)将湿度传感器的接线头连接到采集仪上,接通电路进行路面板湿度的测量。
所述步骤(1)中上下密、中间疏是指距离路面板板顶8cm的区域和距离路面板板底8cm的区域为密集布置区,两个密集布置区中间为稀疏布置区。
所述密集布置区中,测试点布置于距离路面板板顶1cm、2cm、4cm和8cm的位置,以及距离路面板板底1cm、2cm、4cm和8cm的位置;所述稀疏布置区中,相邻测试点的竖直间距为10cm。
所述PVC套管底端以塑料片封住,距底端1.5±0.2cm的区域开一条周向的细缝作为开口,从该开口开始向顶端用直尺量测设定长度,并用记号笔做好标记。
与现有技术相比,本发明可确保路面的测量数据较为准确、全面,同时测试工作所需的安装装置较少、简单易行,且测试工作的重复性较强。
附图说明
图1为本发明测试方法所用的湿度传感器。
图2为本发明测试方法的传感器安装过程示意图。图2-1为底端密封并开口的PVC套管的插入深度,图2-2为将PVC套管插入现浇混凝土中,图2-3为将口径较小的PVC插管插入上述套管中,图2-4为待混凝土初凝结束后取出PVC插管,并插入湿度传感器,图2-5为在PVC套管顶端开口处和湿度传感器的间隙之间涂抹高分子胶以避免外部空气湿度的影响。
图3为板内沿深度测试点的选取示意图。
图4为本发明测试方法所用的PVC套管。
图5为本发明测试方法所用的PVC插管。
具体实施方式
下面结合附图和实施例详细说明本发明的实施方式。
本发明所用仪器设备包括:
湿度采集仪:显示分辨率为0.1%,记录间隔为0.1s~60s,采用220VAC交流电源供电,工作环境温度为0~50℃,所处环境湿度小于90%R.H。
湿度传感器:电流输出型,两线4mA~20mA,测试范围为0~100%R.H,插入端直径为1.4cm,长度可随要求定制,如图1所示,其数据采集区域1在底端0.3~2.8cm的范围内,外径为Ф1.4。
如图2所示,本发明一种水泥混凝土路面板湿度测试方法,包括以下步骤:
(1)根据上下密、中间疏的原则确定路面板沿深度方向的测试点数目和位置,如图3所示,测试点5、测试点6、测试点7、测试点8、测试点9、测试点10、测试点11、测试点12是选定的不同深度的测试点,测试点5距离板顶1cm,测试点6距离板顶2cm,测试点7距离板顶4cm,测试点7距离板顶8cm;测试点9距离板底1cm,测试点10距离板底2cm,测试点11距离板底4cm,测试点12距离板底8cm。以上为密集布置区的测试点分布,在稀疏布置区可有选择地布置间距为10cm左右的点。
(2)如图2-1所示,在PVC套管距底端1.5cm左右的区域锯一条细缝作为开口3,并将底端用封口装置2如塑料片封住,从该缝开始向顶端用直尺量测设定长度,用记号笔13做好预设深度标记4,设计完成的PVC套管如图4所示,采用Ф2管径的PVC管;
(3)如图2-2所示,一般在水泥混凝土路面铺筑完成后将PVC套管插入至标记好的深度,如图2-3所示,在套管中插入PVC插管,PVC插管如图5所示,采用Ф1.6管径的PVC管;
(4)如图2-4所示,待混凝土初凝结束后,将PVC插管取出,插入湿度传感器,如图2-5所示,在封口处涂抹高分子密封胶14。
(5)将湿度传感器的接线头连接到采集仪上,接通电路,设置好记录间隔等参数即可进行路面板湿度的测量。

Claims (1)

1.一种水泥混凝土路面板内湿度梯度测试方法,其特征在于,包括如下步骤:
(1)根据上下密、中间疏的原则确定路面板沿深度方向的测试点数目和位置,其中上下密、中间疏是指距离路面板板顶8cm的区域和距离路面板板底8cm的区域为密集布置区,两个密集布置区中间为稀疏布置区;
(2)在水泥混凝土路面铺筑完成后,在测试点插入一个底端密封侧边开口的PVC套管,并在PVC套管中插入PVC插管,所述PVC套管底端以塑料片封住,距底端1.5±0.2cm的区域开一条周向的细缝作为开口,从该开口开始向顶端用直尺量测设定长度,并用记号笔做好标记;
(3)待混凝土初凝结束后,将PVC插管取出,插入湿度传感器,并在封口处涂抹密封胶;
(4)将湿度传感器的接线头连接到采集仪上,接通电路进行路面板湿度的测量。
CN201310752709.2A 2013-12-31 2013-12-31 一种水泥混凝土路面板内湿度梯度测试方法 Active CN103743893B (zh)