CN202419038U - Internal anticorrosion alloy joint coating for pipeline - Google Patents

Internal anticorrosion alloy joint coating for pipeline Download PDF

Info

Publication number
CN202419038U
CN202419038U CN2011202508763U CN201120250876U CN202419038U CN 202419038 U CN202419038 U CN 202419038U CN 2011202508763 U CN2011202508763 U CN 2011202508763U CN 201120250876 U CN201120250876 U CN 201120250876U CN 202419038 U CN202419038 U CN 202419038U
Authority
CN
China
Prior art keywords
pipeline
resistant alloy
corrosion resistant
corrosion
anticorrosion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011202508763U
Other languages
Chinese (zh)
Inventor
不公告发明人
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2011202508763U priority Critical patent/CN202419038U/en
Application granted granted Critical
Publication of CN202419038U publication Critical patent/CN202419038U/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model discloses an internal anticorrosion alloy joint coating for a pipeline. The internal anticorrosion alloy joint coating is an internal anticorrosion coating joint coating method for water supply and discharge pipelines in petrochemical cities. Anticorrosion alloy short pipes are lined in the pipeline. Coatings cover a part of the inner surfaces of anticorrosion steel pipes. During the welding of the pipeline, the anticorrosion alloy short pipes are jointed and welded by adopting anticorrosion welding rods or anticorrosion welding wires, and the steel pipes are welded after the welding of the lining pipes are finished. Therefore, the aim of isolating the corrosion of a medium to parent metal is fulfilled.

Description

Corrosion-resistanting interpolating port in the pipeline corrosion resistant alloy
Technical field
The utility model relates to oil, chemical pipeline, urban water supply and sewerage antirust coating in pipeline repaired mouth, does not especially need the scene that steel pipe is handled again, the repaired mouth that only needs welding junction to accomplish.
Background technique
At present, known oil, chemical pipeline undercoating patch technology have: electrostatic powder coating, the spraying of liquid coating motor-driven carrier, memory alloy repaired mouth, internal lining pipe connect repaired mouth.Deficiency is that electrostatic powder coating needs pipeline in welding process, will weld a mouth and mends a mouth, and construction speed is slow; The spraying of liquid coating motor-driven carrier all has requirement to caliber and coating, can not satisfy the repaired mouth of less caliber and pipeline bend; The higher application of memory alloy price is few; Internal lining pipe connects the outer shape that will change steel pipe makes the caliber of internal lining pipe identical with main line, and there are certain difficulty in site operation and anti-corrosion pipeline when prefabricated, and influence the attractive in appearance of abovegrade piping.
Summary of the invention
In order to overcome the deficiency of existing pipeline internal corrosion repaired mouth; The utility model provides a kind of joint coating on pipeline structure, and it is accomplished when the pipeline internal corrosion layer is prefabricated, has saved on-the-spot repaired mouth operation; Do not change the external structure of pipeline, the pipeline internal joint patch technology that direct welding can be accomplished.Corrosion-resistanting interpolating port in the pipeline corrosion resistant alloy; Be in pipeline, form, it is characterized in that: do liner with the corrosion resistant alloy pipe in the anti-corrosion pipeline interface section by carbon steel pipes, corrosion-inhibiting coating, corrosion resistant alloy pipe; One end of corrosion resistant alloy pipe connects another root corrosion resistant alloy pipe, and the other end is connected with anticorrosive coat; Corrosion resistant alloy pipe outer wall is connected with the inner-walls of duct contact; Corrosion resistant alloy Guan Yiduan is connected with pipeline anticorrosion coating is tight, and the other end is connected with corrosion resistant alloy pipe full weld.
The utility model solves the technological scheme that its technical problem adopted: before pipeline internal corrosion is prefabricated, the corrosion resistant alloy pipe is closely served as a contrast into anti-corrosion pipe two ends (gap of corrosion resistant alloy steel pipe and steel pipe should less than 0.5mm).The length of corrosion resistant alloy pipe is generally that (120~150mm), thickness is generally (between 0.5~3mm), and confirms thickness according to the size of caliber.The corrosion resistant alloy pipe reserves the length of welding, and is suitable not influence being welded as of steel pipe.When interior anticorrosive coat applies, should cover more than the corrosion resistant alloy pipe 40mm burned anticorrosive coat when corrosion resistant alloy pipe reservation 80mm welds fully.What this kind joint coating on pipeline structure was the most suitable is powder coating; End in the corrosion resistant alloy pipeline need not carry out preservative treatment, and powder coating melts the natural shutoff in back, and for example: the polyethylene powders coating thickness can reach more than the 3mm; After joint coating on pipeline was accomplished, the variation of its caliber was very little.When powder coating applied, corrosion resistant alloy pipe outer wall can not done locating point.
If the employing liquid coating need be after lining be gone into the corrosion resistant alloy pipe; Earlier reconciling into putty contacts an end in the corrosion resistant alloy pipeline with pipeline slit with the film forming matter resin of liquid coating (generally need to add a certain proportion of resin curing agent and filler) accordingly carries out shutoff and makes it and the transition of pipeline smooth interior surfaces; Corrosion-resistant construction in treating just can carry out after putty is done solid work, perhaps the spraying of pipeline internal corrosion layer is together last, when treating the corrosion-inhibiting coating surface drying; With the corrosion resistant alloy pipe serve as a contrast into; And adopt coating that the corrosion resistant alloy pipe is covered the coating more than the 40mm, until the purpose that reaches design and seal for pipe joints, but when liquid coating is anticorrosion; Corrosion resistant alloy pipe outer wall need be done locating point, prevents that the stressed collision of corrosion resistant alloy pipe from moving to destroy coating and have influence on the repaired mouth effect.
Pipeline when butt joint during site operation, adopt earlier in the part welding that corrosion resistant alloy wire solder (welding wire) reserves the corrosion resistant alloy pipe, carry out the welding of steel pipe again, joint coating on pipeline was accomplished simultaneously after welding was accomplished.
Corrosivity difference according to pipeline medium is selected the corrosion resistant alloy short tube: as: 304,316L, 904L, two phase stainless steel, monel metal, Hastelloy or the like corrosion resistant material.
Corrosion resistant alloy pipe: can adopt the intercepting of corrosion resistant alloy pipe, also can be corrosion resistant alloy sheet material and be welded through machining.
Description of drawings
Below in conjunction with accompanying drawing and embodiment the utility model is further specified.
Fig. 1 is the joint coating on pipeline longitudinal section tectonic maps of the utility model.
Fig. 2 is a corrosion resistant alloy pipe longitudinal section tectonic maps.
1. carbon steel tube weld bonds among the figure, 2. corrosion resistant alloy pipe weld bond, 3. corrosion resistant alloy pipe, 4. Corrosion Resisting Steel tack weld.
Embodiment
Steel pipe need carry out the non-corrosive metal (NCM) surface before prefabricated and handles anticorrosion in Fig. 1; Derusting by sandblasting reaches the regulation of GB8923Sa2.5 level; After rust cleaning is accomplished; Corrosion resistant alloy pipe (3) lining is gone into the steel duct two ends, and this operation should be adopted plank to knock corrosion resistant alloy pipe (3) to make concordant with the port at steel pipe two ends.The coating of the internal surface of corrosion resistant alloy pipe (3) part also need be carried out sandblast makes it have certain depth of abrasion pattern, with increase its with steel pipe in the combination force of barrier coating, the coating of carrying out the interior barrier coating of steel pipe at last reaches the thickness that requires in the design.After the barrier coating construction is accomplished in the steel pipe, the port of steel pipe and corrosion resistant alloy pipe (3) is beaten the groove of 45, the groove of steel pipe and corrosion resistant alloy pipe (3) remains on same the oblique line.When on-the-spot pipeline welds, adopt Corrosion Resisting Steel welding rod (or welding wire) earlier corrosion resistant alloy pipe weld bond (2) to be welded, adopt carbon steel that carbon steel tube weld bond (1) is welded again, accomplish the repaired mouth work of pipeline simultaneously.
In Fig. 2, weld on the outer wall circumferencial direction of corrosion resistant alloy pipe (3) 2~4 independently solder joint become the position that Corrosion Resisting Steel tack weld (4) is used for fixing corrosion resistant alloy pipe (3); The attention steel pipe is beaten groove and tack weld (4) is not all destroyed, and keeps the fastening effect of corrosion resistant alloy pipe tack weld (4) in the steel pipe.

Claims (3)

1. corrosion-resistanting interpolating port in the pipeline corrosion resistant alloy; In pipeline, form by carbon steel pipes, corrosion-inhibiting coating, corrosion resistant alloy pipe, it is characterized in that: do liner with the corrosion resistant alloy pipe in the anti-corrosion pipeline interface section; One end of corrosion resistant alloy pipe connects another root corrosion resistant alloy pipe, and the other end is connected with anticorrosive coat.
2. corrosion-resistanting interpolating port in the pipeline corrosion resistant alloy according to claim 1 is characterized in that: corrosion resistant alloy pipe outer wall is connected with the inner-walls of duct contact.
3. corrosion-resistanting interpolating port in the pipeline corrosion resistant alloy according to claim 1, it is characterized in that: corrosion resistant alloy Guan Yiduan is connected with pipeline anticorrosion coating is tight, and the other end is connected with the corrosion resistant alloy full weld.
CN2011202508763U 2011-07-16 2011-07-16 Internal anticorrosion alloy joint coating for pipeline Expired - Fee Related CN202419038U (en)