CN202398642U - 拉丝模水冷模套 - Google Patents

拉丝模水冷模套 Download PDF

Info

Publication number
CN202398642U
CN202398642U CN2011205098205U CN201120509820U CN202398642U CN 202398642 U CN202398642 U CN 202398642U CN 2011205098205 U CN2011205098205 U CN 2011205098205U CN 201120509820 U CN201120509820 U CN 201120509820U CN 202398642 U CN202398642 U CN 202398642U
Authority
CN
China
Prior art keywords
die sleeve
die
water
core rod
sleeve body
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011205098205U
Other languages
English (en)
Inventor
翟海平
翟素萍
董吉林
徐华
翟华平
翟世先
顾晓友
任崇清
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU XIHU SPECIAL STEEL CO Ltd
Original Assignee
JIANGSU XIHU SPECIAL STEEL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU XIHU SPECIAL STEEL CO Ltd filed Critical JIANGSU XIHU SPECIAL STEEL CO Ltd
Priority to CN2011205098205U priority Critical patent/CN202398642U/zh
Application granted granted Critical
Publication of CN202398642U publication Critical patent/CN202398642U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种拉丝模水冷模套,包括模套本体、与模套本体相配合的模芯,所述的模套本体上设置有至少一个水槽,其具有结构简单、增大模套的散热面积,改善模芯的冷却条件、模芯使用寿命长的优点。

Description

拉丝模水冷模套
技术领域
本实用新型涉及拉丝模设备领域,尤其涉及一种拉丝模水冷模套。
背景技术
现有技术中,拉丝模模芯的材质是硬质合金或聚晶材料,模套材料是45#钢,根据模芯的外型尺寸,在车床上将45#圆棒加工成相应的使用尺寸,采用热镶套方法(将模套加热到800℃,用钳子放在平面铁镦上,孔向上,将模芯出口端对正模套孔,用铁锤轻轻打压)静配合将模芯压入模套中。其影响模具质量的因素有:模套外壁厚度尺寸小,传热快,冷却条件好,模芯寿命长,缺点是模套受力差,容易变形,使模芯与模套松动,模芯的应力就不能充分地传到模套上,使模芯爆裂。如增加模套外壁厚度,使模芯应力充分地传到模套不会爆裂,缺点是传热差,模芯温度高,使模芯硬度下降,耐磨性降低,造成模孔扩张快,使用寿命短,带来钢丝表面尺寸变化大,产品尺寸精度降低。
发明内容
为解决现有技术不足,本实用新型提供一种结构简单、增大模套的散热面积,改善模芯的冷却条件、模芯使用寿命长的拉丝模水冷模套。  
本实用新型采用如下技术方案:拉丝模水冷模套,包括模套本体、与模套本体相配合的模芯,其特征在于:所述的模套本体上设置有至少一个水槽。
所述的模套本体上设置有4个均匀分布的水槽。
所述的水槽的截面形状为V形。
本实用新型拉丝模水冷模套在模套本体上设置有水槽,增加了模套的散热面积,延长模芯的使用寿命。
进一步的模套本体上设置有4个均匀分布的水槽,可以增大模套的散热面积。
更进一步的所述的水槽的截面形状为V形,同样能够增大模套的散热面积。
本实用新型拉丝模水冷模套具有结构简单、增大模套的散热面积,改善模芯的冷却条件、模芯使用寿命长的优点。
附图说明
图1是本实用新型的结构示意图。 
图中序号:1、模套本体;2、模芯;3、水槽。
具体实施方式
下面结合附图和具体实施方式对本实用新型作进一步说明。
如图1所示,一种拉丝模水冷模套,包括模套本体1、与模套本体1相配合的模芯2,所述的模套本体1上设置有4个均匀分布的水槽3;所述的水槽3的截面形状为V形。
本实用新型采用在模套上进行水槽设计,增大模套的散热面积,改善模芯的冷却条件。就是在模套的外圆对称四点(90°)钻出圆孔8-10mm而贯穿模壁,再以孔径两边向纵5-15mm(根据外径尺寸选取)开一个斜面槽,以斜面长度达到最大为最佳。
以上详细说明了本实用新型的实施方式,但这只是为了便于理解而举的实例,不应被视为是对本实用新型范围的限制。同样,任何所属技术领域的技术人员均可根据本实用新型的技术方案及其较佳实施例的描述,做出各种可能的等同改变或替换,但所有这些改变或替换都应属于本实用新型权利要求的保护范围。

Claims (3)

1.拉丝模水冷模套,包括模套本体(1)、与模套本体(1)相配合的模芯(2),其特征在于:所述的模套本体(1)上设置有至少一个水槽⑶。
2.根据权利要求1所述的拉丝模水冷模套,其特征在于:所述的模套本体(1)上设置有4个均匀分布的水槽⑶。
3.根据权利要求1或2所述的拉丝模水冷模套,其特征在于:所述的水槽⑶的截面形状为V形。
CN2011205098205U 2011-12-09 2011-12-09 拉丝模水冷模套 Expired - Fee Related CN202398642U (zh)