CN202359782U - Overlapping combined decorative plane material - Google Patents
Overlapping combined decorative plane material Download PDFInfo
- Publication number
- CN202359782U CN202359782U CN2011203867087U CN201120386708U CN202359782U CN 202359782 U CN202359782 U CN 202359782U CN 2011203867087 U CN2011203867087 U CN 2011203867087U CN 201120386708 U CN201120386708 U CN 201120386708U CN 202359782 U CN202359782 U CN 202359782U
- Authority
- CN
- China
- Prior art keywords
- thin slice
- paper
- substrate layer
- overlapping combined
- plane materiel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model relates to an overlapping combined decorative plane material. The overlapping combined decorative plane material is characterized by comprising a substrate layer and a decorative plane layer coated on the substrate layer. The decorative plane layer is composed of densely distributed plant slices having geometric patterns. Adjacent plant slices have their edges mutually overlapped. Compared with the prior art, the overlapping combined decorative plane material provided in the utility model has the advantages of simple structure, reasonable design, working hour reduction and manufacturing efficiency increase due to the fact that edges are no longer required to abut on corresponding ones before being connected during a sticking process. Furthermore, the overlapping combined decorative plane material has a structure which overcomes defects that plant slices are arched or cracked under the influence of the environment.
Description
Technical field:
The utility model relates to a kind of overlapping combined decoration plane materiel.
Background technology:
Decorative material for wall surface is that people beautify the necessary material in the indoor environment, but present decorative material for wall surface majority is a plane decoration, lacks third dimension, builds on metope with parting material three-dimensional moulding, the cost height, construct numerous and diverse.
Existing a kind of stereo decoration plane materiel; Comprise substrate layer and paste the architectural surface on substrate layer; Architectural surface is processed by the plant thin slice that is geometrical pattern that gathers; Limit between the adjacent two plant thin slices abuts against together (shown in Fig. 1 a, being example to grow limit shape), and the advantage of this stereo decoration plane materiel is to have three-dimensional aesthetic feeling; Its shortcoming is because the plant thin slice receives the influence of varying environment different temperatures, different humidity easily; Produce the elongation or the contraction of plant thin slice; Making its plant thin slice of adjacency when manufacturing is seamlessly to abut against together; And in the market or the field of employment plant thin slice splicing limit occurs and arch upward or crack phenomenon (shown in a, b among Fig. 1 b, the 1c) occurs, had a strong impact on product quality and application life.
Summary of the invention:
One of them purpose of the utility model promptly is to provide a kind of overlapping combined decoration plane materiel, and this overlapping combined decoration plane materiel is not only simple in structure, reasonable in design, and helps preventing that arching upward or going out crack phenomenon from appearring in the decoration plane material material.
The utility model purpose realizes through following technical scheme:
The overlapping combined decoration plane materiel of the utility model is characterized in that: comprise substrate layer and paste the architectural surface on substrate layer, said architectural surface is gathered by the plant thin slice that is geometrical pattern and constitutes, and splices each other in the edge of adjacent plant thin slice.
The geometrical pattern of above-mentioned plant thin slice is one or more in polygon, circle or the ellipse.
Above-mentioned plant thin slice is one or more in the synthetic thin slice skin of bamboo skin, wooden skin, rattan peel or plant.
Above-mentioned substrate layer is anti-cracking layer (play a kind of medium layer of good bond between the thin slice, abbreviate anti-cracking layer as), and the material of anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper.
Above-mentioned substrate layer comprises anti-cracking layer and substrate layer.
The material of the bonding mediator of above-mentioned anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper.
Above-mentioned substrate layer material is a kind of in nonwoven, wool paper, PLASTIC LAMINATED, clamping plate, density board, foaming plate, ecological plate etc. or the PU film.
The preparation method of the overlapping combined decoration plane materiel of the utility model; This overlapping combined decoration plane materiel preparation method is simple; Not only help improving and make work efficiency, and help preventing that crack phenomenon from appearring arching upward or going out in the decoration plane material material, and have strong third dimension; Utilize the various reflecting effect decoration panels after the concavo-convex fluctuating of plant thin slice, more show beautiful colorful.
The utility model is made the method for overlapping combined decoration plane materiel, it is characterized in that: on substrate layer, paste the plant thin slice that is geometrical pattern one by one, spliced each other in the edge of adjacent plant thin slice.
When above-mentioned substrate layer is anti-cracking layer; The material of anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper, when making, is at first pasting the anti-cracking material plant thin slice back side with cloth glue machine roller coating cloth glue; Naturally dried under the normal temperature 3-10 hour; After drying it is washed into required geometrical pattern shape with stamping cutting die, surperficial with cloth glue machine roller coating glue at substrate layer then, normal temperature dried 1-3 hour naturally; The geometrical pattern shape that punching press is good is attached to the substrate layer surface; Splice each other in the edge of guaranteeing the plant thin slice with geometrical pattern shape that punching press is good during stickup, stickup back precompressed 1-3 minute, errorless back, assembly pendulum position completion in hot pressing 1-5 minute under the 80-110 temperature of check geometrical pattern shape.
When above-mentioned substrate layer comprises anti-cracking layer and substrate layer; The material of anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper, and the substrate layer material is a kind of in nonwoven, wool paper, PLASTIC LAMINATED, clamping plate, density board, foaming plate or the PU film; When making, at first at anti-cracking layer upper surface with cloth glue machine roller coating glue, stick the plant thin slice, after colding pressing 20 minutes to 60 minutes under the cold press normal temperature, under the 80-110 temperature hot pressing 1-5 minute; Then, with cloth glue machine roller coating glue, dried naturally under the normal temperature 3-10 hour, after drying it is washed into required geometrical pattern shape with stamping cutting die at anti-cracking layer soffit; Surperficial at substrate layer then with cloth glue machine roller coating glue; Normal temperature dried 1-3 hour naturally; The geometrical pattern shape that punching press is good is attached to the substrate layer surface; Splice each other in the edge of guaranteeing the plant thin slice with geometrical pattern shape that punching press is good during stickup, stickup back precompressed 1-3 minute, errorless back, assembly pendulum position completion in hot pressing 1-5 minute under the 80-110 temperature of check geometrical pattern shape.
The utility model appliable plant thin slice edge dexterously splices each other; Make the elongation or the shrinkage phenomenon of the plant thin slice that receives environment temperature and humidity effect easily occur in two independent aspects, thereby avoided existing plant thin slice to occur in arching upward of jointing positions or crack phenomenon.Compared with prior art, having simple in structurely, reasonable in design, need not each limit during stickup and carry out correspondence and be abutted against, shorten man-hour, improve make efficiency, mainly is to have overcome the plant thin slice arching upward or crack phenomenon because of what ambient influnence produced.
Description of drawings:
Fig. 1 a is the organigram of existing a kind of stereo decoration plane materiel;
Fig. 1 b is the organigram (profile of Fig. 1 a) that existing stereo decoration plane materiel plant thin slice produces the phenomenon that arches upward;
Fig. 1 c is the organigram (profile of Fig. 1 a) that existing stereo decoration plane materiel plant thin slice produces crack phenomenon;
Fig. 2 a is the utility model organigram;
Fig. 2 b is the utility model cross-section structure sketch map;
Fig. 3 is the another kind of organigram of implementing of the utility model;
Fig. 4 is the another kind of organigram of implementing of the utility model;
Fig. 5 is the organigram of PU film.
The specific embodiment:
The overlapping combined decoration plane materiel of the utility model; Comprise substrate layer 1 and paste the architectural surface 2 on substrate layer 1; Architectural surface 2 is gathered by the plant thin slice that is geometrical pattern 3 and constitutes; Splicing (shown in Fig. 2 a, 2b) each other in the edge 4 of adjacent plant thin slice, has formed lap at the place's two plant thin slices that splice each other, and the utility model appliable plant thin slice edge 4 dexterously splices each other; Make the elongation or the shrinkage phenomenon of the plant thin slice that receives environment temperature and humidity effect easily occur in two independent aspects (shown in Fig. 2 b), thereby avoided existing plant thin slice to occur in arching upward of jointing positions or crack phenomenon.
The geometrical pattern of above-mentioned plant thin slice 3 can be in polygon, circle or the ellipse one or more, and wherein polygon can be triangle (equilateral triangle or non-equilateral triangle), quadrangle (square, rectangle, isosceles trapezoid etc.), hexagon (regular hexagon or non-regular hexagon) etc.
Fig. 2 a, 2b are example with the rectangle, all splice each other in the 4 whole limits, edge of wherein adjacent plant thin slice; The edge 4 whole limit segment sections of certainly adjacent plant thin slice splice also each other can (as shown in Figure 3, it be example that this figure only extracts three plant thin slices, and remaining shape continues with identical unit with width in length).
Fig. 4 is to be example with the hexagon, and it is example that this figure only extracts several plant thin slices, and remaining shape continues with identical unit with width in length.
Above-mentioned what enumerate only is in the overlapping combined decoration plane materiel a kind of geometrical pattern only to be arranged with a slice, certainly, with the geometrical pattern of plant thin slice in the overlapping combined decoration plane materiel of a slice two or more can be arranged, and this is unrestricted.
Above-mentioned plant thin slice is one or more in the synthetic thin slice skin of bamboo skin, wooden skin, rattan peel or plant.
When above-mentioned substrate layer when one deck is only arranged is anti-cracking layer, the material of anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper.
When above-mentioned substrate layer comprises anti-cracking layer and substrate layer; The material of anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper, and the substrate layer material is a kind of in nonwoven, wool paper, PLASTIC LAMINATED, clamping plate, density board, foaming plate or the PU film.
The PU film is a kind of material of handling through special process (concrete structure is seen Fig. 5, and wherein 6 is Polyurethane, and 7 is the TPU PUR, and 8 is PET hot pressing cloth, and 9 is polypropylene amine), and its nontoxic, environmental protection can not have side effects to human body.Plant thin slice, scientific and technological skin, bamboo skin are equal to the PU film and combine the back advantage to be: it has changed wood materials self; Because of contraction, expansion unstability and the wrinkling that environmental change produced; Product combines with the PU film, and product can directly be used on metope, and is more perfect during applying.Solved natural wallpaper and caused the phenomenon that mouldy flavescence comes off because of aqueous vapor, humidity.
The utility model is with after the PU film combines, during construction, can be mutually harmonious with bonding adhesive more than employed 80 ℅ on the existing market, and have easy construction, superiority such as clean and tidy, clean, time saving and energy saving, be the high-quality wallpaper material that is difficult to seek on the existing market.
The substrate layer of the overlapping combined decoration plane materiel of the utility model can only have the anti-cracking layer of one deck, also can comprise anti-cracking layer and substrate layer, and having additional substrate layer certainly will more help improving the quality of products and application life.
The utility model is made the method for overlapping combined decoration plane materiel, on substrate layer, pastes the plant thin slice that is geometrical pattern one by one, is spliced each other in the edge of adjacent plant thin slice.
When above-mentioned substrate layer is anti-cracking layer, the material of anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper, when making; At first, dried naturally under the normal temperature 3-10 hour, after drying it is washed into required geometrical pattern shape with stamping cutting die pasting the anti-cracking material plant thin slice back side with cloth glue machine roller coating cloth glue; Then on substrate layer surface with cloth glue machine roller coating glue, normal temperature dried 1-3 hour naturally, the geometrical pattern shape that punching press is good is attached to the substrate layer surface; Splicing each other in the edge of guaranteeing the plant thin slice with geometrical pattern shape that punching press is good during stickup, (being employed in the edge and splicing and also shortened the overlapping time of staff and the uniformity of finished product pattern, is owing to when punching press plant thin slice, all be many usually and carry out simultaneously; So only can guarantee the uniformity of its shape basically, and each other size certain error is arranged is unavoidable, so if according to existing connecting method; Promptly two adjacent plant thin slice limits and limit be to being abutted against, and be seamless to what lean in order to guarantee so, will be behind several plant thin slices of splicing; One row's plant thin slice generation is tilted, and a possible other row often occurs in actual production toward other lopsidedness like this; And the way that solves is done over again exactly, so just causes work efficiency extremely low, and requirement is that the staff who knows a thing or two could accomplish; Splice and to avoid doing over again phenomenon and the utility model is employed in the edge; Also need not the staff of specialty, also reduced cost of labor thereby not only improved work efficiency), paste back precompressed 1-3 minute; Errorless back, assembly pendulum position completion in hot pressing 1-5 minute under the 80-110 temperature of check geometrical pattern shape; The above-mentioned precompressed or the pressure of hot pressing are the pressure of every square centimeter of 5-8 kilogram, and normal temperature is room temperature, and employed glue is white glue with vinyl.
When above-mentioned substrate layer comprises anti-cracking layer and substrate layer; The material of anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper, and the substrate layer material is a kind of in nonwoven, wool paper, PLASTIC LAMINATED, clamping plate, density board, foaming plate or the PU film; When making, at first at anti-cracking layer upper surface with cloth glue machine roller coating glue, stick the plant thin slice, after colding pressing 20 minutes to 60 minutes under the cold press normal temperature, under the 80-110 temperature hot pressing 1-5 minute; Then, with cloth glue machine roller coating glue, dried naturally under the normal temperature 3-10 hour, after drying it is washed into required geometrical pattern shape with stamping cutting die at anti-cracking layer soffit; Then on substrate layer surface with cloth glue machine roller coating glue, normal temperature dried 1-3 hour naturally, the geometrical pattern shape that punching press is good is attached to the substrate layer surface; Splicing each other in the edge of guaranteeing the plant thin slice with geometrical pattern shape that punching press is good during stickup, (being employed in the edge and splicing and also shortened the overlapping time of staff and the uniformity of finished product pattern, is owing to when punching press plant thin slice, all be many usually and carry out simultaneously; So only can guarantee the uniformity of its shape basically, and each other size certain error is arranged is unavoidable, so if according to existing connecting method; Promptly two adjacent plant thin slice limits and limit be to being abutted against, and be seamless to what lean in order to guarantee so, will be behind several plant thin slices of splicing; One row's plant thin slice generation is tilted, and a possible other row often occurs in actual production toward other lopsidedness like this; And the way that solves is done over again exactly, so just causes work efficiency extremely low, and requirement is that the staff who knows a thing or two could accomplish; Splice and to avoid doing over again phenomenon and the utility model is employed in the edge; Also need not the staff of specialty, also reduced cost of labor thereby not only improved work efficiency), paste back precompressed 1-3 minute; Errorless back, assembly pendulum position completion in hot pressing 1-5 minute under the 80-110 temperature of check geometrical pattern shape; The above-mentioned precompressed or the pressure of hot pressing are the pressure of every square centimeter of 5-8 kilogram, and normal temperature is room temperature, and employed glue is white glue with vinyl.
The utility model appliable plant thin slice edge dexterously splices each other; Make the elongation or the shrinkage phenomenon of the plant thin slice that receives environment temperature and humidity effect easily occur in two independent aspects, thereby avoided existing plant thin slice to occur in arching upward of jointing positions or crack phenomenon.Compared with prior art, having simple in structurely, reasonable in design, need not each limit during stickup and carry out correspondence and be abutted against, shorten man-hour, improve make efficiency, mainly is to have overcome the plant thin slice arching upward or crack phenomenon because of what ambient influnence produced.
Though the existing preferred embodiment of the utility model discloses as above, be not that any decoration plane material splices each other in the edge of adjacent plant thin slice and all falls into the protection domain of the utility model in order to qualification the utility model.
Claims (7)
1. overlapping combined decoration plane materiel is characterized in that: comprise substrate layer and paste the architectural surface on substrate layer, said architectural surface is gathered by the plant thin slice that is geometrical pattern and constitutes, and splices each other in the edge of adjacent plant thin slice.
2. overlapping combined decoration plane materiel according to claim 1 is characterized in that: the geometrical pattern of said plant thin slice is one or more in polygon, circle or the ellipse.
3. overlapping combined decoration plane materiel according to claim 1 and 2 is characterized in that: said plant thin slice is one or more in the synthetic thin slice skin of bamboo skin, wooden skin, rattan peel or plant.
4. overlapping combined decoration plane materiel according to claim 3 is characterized in that: said substrate layer is anti-cracking layer, and the material of anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper.
5. overlapping combined decoration plane materiel according to claim 3 is characterized in that: said substrate layer comprises anti-cracking layer and substrate layer.
6. overlapping combined decoration plane materiel according to claim 5 is characterized in that: the material of said anti-cracking layer is a kind of in paper, nonwoven, cloth, explosion-proof paper, paper gasket or the wool paper.
7. overlapping combined decoration plane materiel according to claim 5 is characterized in that: said substrate layer material is a kind of in nonwoven, wool paper, PLASTIC LAMINATED, clamping plate, density board, foaming plate, ecological plate or the PU film.