CN202359164U - 一种离合器盘状零件压淬装置 - Google Patents
一种离合器盘状零件压淬装置 Download PDFInfo
- Publication number
- CN202359164U CN202359164U CN2011204195937U CN201120419593U CN202359164U CN 202359164 U CN202359164 U CN 202359164U CN 2011204195937 U CN2011204195937 U CN 2011204195937U CN 201120419593 U CN201120419593 U CN 201120419593U CN 202359164 U CN202359164 U CN 202359164U
- Authority
- CN
- China
- Prior art keywords
- quenching device
- patrix
- inlet pipe
- counterdie
- quenching
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种离合器盘状零件压淬装置,它包括上模(1)和下模(2),上模(1)的下表面和下模(2)的上表面均设有导流槽(3),上模(1)上还设有多个与导流槽(3)连通的分流孔(4),上模(1)的上方设有一壳体(5),壳体(5)上设有进液管(6),进液管(6)与分流孔(4)相连通,下模(2)外圈设有一环形凸出板(7),壳体(5)底部外表面上设有一与该环形凸出板(7)相配合的凹槽(8)。本实用新型的有益效果是:提高了盘状零件的生产效率,降低了成本和能耗,淬火硬度均匀性好,产品硬度高,提高了产品的质量和使用寿命,减小了空气污染。
Description
技术领域
本实用新型涉及盘状零件淬火技术领域,特别是一种离合器盘状零件压淬装置。
背景技术
离合器是传递汽车或摩托车动力系统的重要部件,它担负着将动力与发动机之间进行切断与连接的工作,在汽车或摩托车行驶过程中操作频繁。为了保证离合器良好的运行状态,对离合器从动盘总成和压板总成的平面度要求较高,而总成平面度主要由离合器盘状零件的平面度决定。
目前国内在进行盘状零件的整体淬火时,基本采用油池淬火,制得的盘状零件变形大,但离合器盘状零件的平面度不能超过0.3mm,按照传统的加工工艺制得的盘状零件不能达到此技术要求,需在淬火后反复校平、加热,这样就导致盘状零件硬度下降,甚至只能做报废处理,给产品质量和生产成本带来很大影响。
现有技术工艺因需要反复的校平、加热,工艺时间长、耗能大、成本高、效率低,且现有技术为多在敞开环境中进行,造成空气污染,生产环境恶劣。
实用新型内容
本实用新型的目的在于克服现有技术的缺点,提供一种加工效率高、耗能小、成本低、质量高的离合器盘状零件压淬装置。
本实用新型的目的通过以下技术方案来实现:
一种离合器盘状零件压淬装置,它包括上模和下模,上模的下表面和下模的上表面均设有导流槽,上模上还设有多个与导流槽连通的分流孔,上模的上方设有一壳体,壳体上设有进液管,进液管与分流孔相连通。
所述的下模外圈设有一环形凸出板,壳体底部外表面上设有一与该环形凸出板相配合的凹槽。
所述的下模位于导流槽的外侧设有导流孔。
所述的上模的上方设有一个分流孔挡板,进液管的出液口设在此挡板上。
所述的下模的外围设有模罩。
本实用新型具有以下优点:
1、本实用新型使得盘状零件在压力状态下完成淬火,没有因淬火产生的变形,经过淬火加工后的零件精度满足产品技术要求,无需再进行校平、加热等后续精加工工艺处理,极大的提高了盘状零件的生产效率,降低了成本和能耗。
2、本实用新型上模的下表面和下模的上表面均设有导流槽,上模上还设有多个与导流槽连通的分流孔,使得工件淬火硬度均匀性好,产品硬度高,提高了产品的质量和使用寿命。
3、本实用新型的下模外圈设有一环形凸出板,壳体底部外表面上设有一与该环形凸出板相配合的凹槽,当上下模配合压紧工件进行淬火时,工件处于一个封闭的环境中,不会被氧化,提高了加工质量,也减小了空气污染。
附图说明
图1 为本实用新型的结构示意图
图中,1-上模,2-下模,3-导流槽,4-分流孔,5 -壳体,6-进液管,7-环形凸出板,8-凹槽,9-导流孔,10-挡板,11-出液口,12-模罩,13-工件。
具体实施方式
下面结合附图对本实用新型做进一步的描述:
如图1所示,一种离合器盘状零件压淬装置,它包括上模1和下模2,上模1的下表面和下模2的上表面均设有导流槽3,上模1上还设有多个与导流槽3连通的分流孔4,上模1的上方设有一壳体5,壳体5上设有进液管6,进液管6与分流孔4相连通。
所述的下模2外圈设有一环形凸出板7,壳体5底部外表面上设有一与该环形凸出板7相配合的凹槽8。
所述的下模2位于导流槽3的外侧设有导流孔9。
所述的上模1的上方设有一个分流孔4挡板10,进液管6的出液口11设在此挡板10上,挡板10与上模1间的空间与分流孔4、导流槽3形成冷却液流动通道。
所述的下模2的外围设有模罩12。
本实用新型的工作过程如下:将加热至淬火温度的工件13放置于下模2上,然后上模1落下,上模1与下模2闭合,环形凸出板7与凹槽8紧密配合,然后,冷却液经进液管6进入,由分流孔4均匀分流至导流槽3,直接喷向工件13上,对其进行淬火处理,淬火过程中,工件13处于压紧状态且不与外界接触,平面度好,不会被氧化,冷却液经下模导流槽3、导流孔9流出装置后,经循环系统流回贮槽循环使用。完成淬火工序后开启模具,经一次加工即可完成成型与淬火两道工序。
Claims (5)
1.一种离合器盘状零件压淬装置,其特征在于:它包括上模(1)和下模(2),上模(1)的下表面和下模(2)的上表面均设有导流槽(3),上模(1)上还设有多个与导流槽(3)连通的分流孔(4),上模(1)的上方设有一壳体(5),壳体(5)上设有进液管(6),进液管(6)与分流孔(4)相连通。
2.根据权利要求1所述的一种离合器盘状零件压淬装置,其特征在于:所述的下模(2)外圈设有一环形凸出板(7),壳体(5)底部外表面上设有一与该环形凸出板(7)相配合的凹槽(8)。
3.根据权利要求1所述的一种离合器盘状零件压淬装置,其特征在于:所述的下模(2)位于导流槽(3)的外侧设有导流孔(9)。
4.根据权利要求1所述的一种离合器盘状零件压淬装置,其特征在于:所述的上模(1)的上方设有一个分流孔(4)挡板(10),进液管(6)的出液口(11)设在此挡板(10)上。
5.根据权利要求1所述的一种离合器盘状零件压淬装置,其特征在于:所述的下模(2)的外围设有模罩(12)。