CN202246897U CN2011203156352U CN201120315635U CN202246897U CN 202246897 U CN202246897 U CN 202246897U CN 2011203156352 U CN2011203156352 U CN 2011203156352U CN 201120315635 U CN201120315635 U CN 201120315635U CN 202246897 U CN202246897 U CN 202246897U
Authority
CN
China
Prior art keywords
cathode
plate
cathode titanium
metal
negative electrode
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011203156352U
Other languages
English (en)
Inventor
李建林
王红光
李树海
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HENAN FAMOUS DIAMOND INDUSTRIAL Co Ltd
Original Assignee
HENAN FAMOUS DIAMOND INDUSTRIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HENAN FAMOUS DIAMOND INDUSTRIAL Co Ltd filed Critical HENAN FAMOUS DIAMOND INDUSTRIAL Co Ltd
Priority to CN2011203156352U priority Critical patent/CN202246897U/zh
Application granted granted Critical
Publication of CN202246897U publication Critical patent/CN202246897U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Electrolytic Production Of Metals (AREA)

Abstract

一种易剥离阴极析出镍的装置,包括矩形阴极钛板,在阴极钛板上端固定有阴极导电铜板,在阴极钛板左右两层均设置有绝缘套管。本实用新型的使用,在电解过程中,因绝缘套管的作用,电解析出的金属镍无法沉积在有绝缘套管的位置,这样在剥离阴极板金属时,就会很轻松将其剥离掉,而且能够保证金属板的完整性,保证了金属板的质量,工作效率也大大提高,每小时剥离数量达到60个左右,同时节省了人力物力。

Description

一种易剥离阴极析出镍的装置
技术领域
本实用新型属于电解技术领域,尤其涉及一种对多晶金刚石进行电解提取金属镍的装置。
背景技术
    在对多晶金刚石进行电解提取金属镍的生产过程中,阴极钛板上会沉积大量的金属镍,阴极板完全被电解析出的金属覆盖,当阴极板沉积的金属超出一定的厚度时,就需要将阴极板上形成的金属分离回收,因析出的金属将阴极板覆盖完全,所以在剥离金属时产生了很大的困难,需要先将阴极板两侧的金属用锤子敲碎,然后再将阴极板两面的镍板敲落,如此操作无法保证阴极板的完整性,剥离时间较长,有时剥离一个就需要1-2个小时,工人的工作劳动强度大,工作效率低,影响公司的长远发展。
实用新型内容
针对在剥离阴极板上金属镍困难的技术问题,本实用新型提供一种易剥离阴极析出镍的装置。
为了解决上述技术问题采用以下技术方案:一种易剥离阴极析出镍的装置,包括矩形阴极钛板,在阴极钛板上端固定有阴极导电铜板,在阴极钛板左右两层均设置有绝缘套管。
所述的绝缘套管为聚乙烯制成的。
所述的绝缘套管的侧面设置轴向的开口,绝缘套管通过开口夹设在阴极钛板的左右两侧。
本实用新型的使用,在电解过程中,因绝缘套管的作用,电解析出的金属镍无法沉积在有绝缘套管的位置,这样在剥离阴极板金属时,就会很轻松将其剥离掉,而且能够保证金属板的完整性,保证了金属板的质量,工作效率也大大提高,每小时剥离数量达到 60个左右,同时节省了人力物力。
附图说明
图1为本实用新型的结构示意图。
具体实施方式
如图1所示,一种易剥离阴极析出镍的装置,包括矩形阴极钛板2,在阴极钛板2上端固定有阴极导电铜板1,在阴极钛板2左右两层均设置有绝缘套管3,绝缘套管为聚乙烯制成的,绝缘套管3的侧面设置轴向的开口,绝缘套管通过开口夹设在阴极钛板的左右两侧。

Claims (3)

1.一种易剥离阴极析出镍的装置,包括矩形阴极钛板,在阴极钛板上端固定有阴极导电铜板,其特征是:在阴极钛板左右两层均设置有绝缘套管。
2.根据权利要求1所述的易剥离阴极析出镍的装置,其特征是:所述的绝缘套管为聚乙烯制成的。
3.根据权利要求1所述的易剥离阴极析出镍的装置,其特征是:所述的绝缘套管的侧面设置轴向的开口,绝缘套管通过开口夹设在阴极钛板的左右两侧。
CN2011203156352U 2011-08-26 2011-08-26 一种易剥离阴极析出镍的装置 Expired - Fee Related CN202246897U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2011203156352U CN202246897U (zh) 2011-08-26 2011-08-26 一种易剥离阴极析出镍的装置

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2011203156352U CN202246897U (zh) 2011-08-26 2011-08-26 一种易剥离阴极析出镍的装置

Publications (1)

Publication Number Publication Date
CN202246897U true CN202246897U (zh) 2012-05-30

Family

ID=46108167

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2011203156352U Expired - Fee Related CN202246897U (zh) 2011-08-26 2011-08-26 一种易剥离阴极析出镍的装置

Country Status (1)

Country Link
CN (1) CN202246897U (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2024098482A1 (zh) * 2022-11-12 2024-05-16 邯郸市创力机械有限公司 一种剥离永久阴极板上析出物的方法

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2024098482A1 (zh) * 2022-11-12 2024-05-16 邯郸市创力机械有限公司 一种剥离永久阴极板上析出物的方法

Similar Documents

Publication Publication Date Title
CN101217206A (zh) 废旧锂电池回收中集流体的高效剥离方法
CN104674299B (zh) 铜电解精炼中不锈钢板附着少量纯铜的回收方法
CN102277495B (zh) 从废旧锂离子二次电池回收金属锂的方法
CN101974765A (zh) 从含锑锡铅物料中分离锑的综合方法
CN103668322B (zh) 一种铜镍基合金废料回收铜、镍的方法
CN201793781U (zh) 防止沉积金属产生不规则剥离端面的阴极板
CN202246897U (zh) 一种易剥离阴极析出镍的装置
WO2016086811A1 (zh) 一种直接电解金属碎料的方法
CN203683689U (zh) 一种清除残余阳极电解质结壳的装置
CN204752875U (zh) 一种锌电积铝阴极板
KR101455326B1 (ko) 음극판의 전착금속 박리장치
CN100499252C (zh) 生物浸出法回收废旧锂离子电池中有价金属的方法
CN207483873U (zh) 一种用于电解精炼阴极种板的包边装置
CN106025421A (zh) 一种锂电池电极的电镀剥离回收方法
CN204111885U (zh) 一种新型无夹边条永久阴极板
CN205382214U (zh) 一种阴极板锌片预开口装置
CN202730270U (zh) 一种处理残极的装置
CN102296325A (zh) 旋转阴极连续固相电解处理废铅蓄电池工艺
CN202201994U (zh) 一种镍电解钛种板装置
CN208158025U (zh) 一种剥线机
CN203956398U (zh) 一种铝转镍极耳的焊接工装
CN203858974U (zh) 一种全自动变压器脱胶皮及沾锡机
CN203320157U (zh) 带卸板架的电解锰自动剥离装置
CN202265614U (zh) 一种电积、电解镍的阴极板
CN207159384U (zh) 一种夹边条及应用其的阴极板

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
CF01 Termination of patent right due to non-payment of annual fee
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20120530

Termination date: 20160826