CN202124490U - 还原炉石墨电极 - Google Patents
还原炉石墨电极 Download PDFInfo
- Publication number
- CN202124490U CN202124490U CN2011202724565U CN201120272456U CN202124490U CN 202124490 U CN202124490 U CN 202124490U CN 2011202724565 U CN2011202724565 U CN 2011202724565U CN 201120272456 U CN201120272456 U CN 201120272456U CN 202124490 U CN202124490 U CN 202124490U
- Authority
- CN
- China
- Prior art keywords
- graphite
- silicon core
- clamping
- folder
- lobe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种还原炉石墨电极,它属于多晶硅生产领域。它由石墨底座、石墨夹盖、石墨夹瓣、硅芯构成,石墨底座的顶部带螺纹,石墨夹盖的内部带有螺纹,石墨底座和石墨夹盖匹配夹持石墨夹瓣,石墨夹瓣整体为圆锥形,石墨夹瓣的中孔为夹持硅芯孔,硅芯置于中孔中,石墨夹瓣再夹紧硅芯。本实用新型其具有优点:一、降低硅芯和石墨电极的接触电阻,缩短预热时间,降低功耗;二、增加石墨电极对夹持硅芯的竖直度,保证硅棒直径最大化,提高稳定性;三、新的石墨结构设计提高石墨件重复利用率,降低成本。
Description
一、技术领域
本实用新型涉及一种还原炉石墨电极,它属于多晶硅生产领域。
二、背景技术
传统的还原炉石墨电极(硅棒支撑件)为直接和电极相连接,其结构是石墨电极夹住硅芯,硅芯通电发热后沉积多晶硅。硅芯通电击穿方式主要有两种:预热击穿和高电压击穿。对于预热击穿工艺目前国内普遍面临以下问题:
1、硅芯和石墨电极接触电阻大难以击穿,预热时间长,功耗大。
2、石墨电极夹持的硅芯的竖直度不理想,影响后期硅棒沉积直径大小和稳定性
3、石墨电极使用中损坏现象严重,重复利用性较差,成本较高
三、实用新型的内容
本实用新型的目的是提供一种新型的还原炉石墨电极,其具有优点:一、降低硅芯和石墨电极的接触电阻,缩短预热时间,降低功耗;二、增加石墨电极对夹持硅芯的竖直度,保证硅棒直径最大化,提高稳定性;三、新的石墨结构设计提高石墨件重复利用率,降低成本。
本实用新型的目的是这样来实现的:它由石墨底座、石墨夹盖、石墨夹瓣、硅芯构成,石墨底座的顶部带螺纹,石墨夹盖的内部带有螺纹,石墨底座和石墨夹盖匹配夹持石墨夹瓣,石墨夹瓣整体为圆锥形,石墨夹瓣的中孔为夹持硅芯孔,硅芯置于中孔中,石墨夹瓣再夹紧硅芯。所述的石墨底座底部为圆槽设计,其分别设计有内圆斜锥面、外圆斜锥面和中心小孔,内圆斜锥面为导电接触面,外圆斜锥面不作为导电接触面,中心小孔为石墨底座是受热膨胀缓冲孔。所述的石墨夹瓣的夹瓣整体为圆锥形,中孔为夹持硅芯孔,石墨夹瓣的夹瓣三等分切削为三瓣,对硅芯的三个方向夹紧固定硅芯。
本实用新型还原炉石墨电极,其具有以下优点:
其一:石墨夹瓣实行三瓣制,三瓣夹持硅芯,保证硅芯稳定和竖直,安装硅芯的竖直角度达到89-90度,几乎做到完全竖直。保证硅芯之间的距离,使硅棒生长直径最大可达180mm。
其二:同时石墨夹瓣夹持的硅芯有保证充分传热,保证预热时预热的热量可以传递至和夹瓣接触的硅芯,提高了该处硅芯温度,降低了该处硅芯电阻,有利于击穿。经过实践证明,石墨夹瓣三瓣式切削的结构设计在使用上预热时间普遍在15min.,比传统的纯粹实体锥夹瓣要缩短10-15min。预热电功耗减少50%。
其三:石墨夹瓣保证夹瓣和硅芯的有效接触面和稳定性,硅芯稳定性好,硅芯/硅棒倒炉率低于1%。
其四:石墨底座结构设计保证底槽内圆斜锥面作为导电面接触良好,底槽外圆斜锥面的设计,保证石墨底座在还原炉运行中受热膨胀被缓冲间距缓冲,保证石墨底座不受应力挤压损坏。
其五:石墨底座和石墨夹盖理想结合,保证硅棒沉积长粗后能和石墨夹盖接触,石墨夹盖又能为硅棒提供支撑,保证硅棒稳定。
其六:石墨底座重复利用率高,由于三件套设计,硅棒最终生长后仅和石墨夹盖接触,在拆卸硅棒后,石墨损坏部分只有夹瓣和夹盖,而石墨底座丝毫未受损。在移除夹盖和夹瓣后,石墨底座仍可重复使用,重复使用率达到80%。比传统的石墨结构大大降低了成本。
四、附图说明
附图1为本实用新型还原炉石墨电极的工作状态装配图。
附图2为本实用新型还原炉石墨电极的剖视图。
附图3为为本实用新型还原炉石墨电极的俯视图。
附图4为为本实用新型还原炉石墨电极的仰视图。
附图5为为本实用新型还原炉石墨电极的石墨底座的立体图。
附图6为为本实用新型还原炉石墨电极的石墨底座的剖视图。
附图7为为本实用新型还原炉石墨电极的石墨夹盖立体图。
附图8为为本实用新型还原炉石墨电极的石墨夹盖剖视图。
附图9为为本实用新型还原炉石墨电极的石墨夹瓣的立体图。
附图10为为本实用新型还原炉石墨电极的石墨夹瓣的单瓣结构图。
五、具体实施方式
下面结合附图来对本实用新型具体实施方式作进一步的说细描述:
参照附图,本实用新型还原炉石墨电极,它由石墨底座5、石墨夹盖3、石墨夹瓣2、硅芯1构成,石墨底座5的顶部带螺纹,石墨夹盖3的内部带有螺纹,石墨底座5和石墨夹盖3匹配夹持石墨夹瓣2,石墨夹瓣2整体为圆锥形,石墨夹瓣2的中孔8为夹持硅芯1孔,硅芯1置于中孔8中,石墨夹瓣2再夹紧硅芯1。所述石墨底座5底部为圆槽设计,其分别设计有外圆斜锥面6、内圆斜锥面7和中心小孔4,内圆斜锥面7为导电接触面,外圆斜锥面6不作为导电接触面,中心小孔4为石墨底座5是受热膨胀缓冲孔。所述石墨夹瓣2的夹瓣整体为圆锥形,中孔8为夹持硅芯1孔,石墨夹瓣2的夹瓣三等分切削为三瓣,对硅芯1的三个方向夹紧固定硅芯。
Claims (3)
1.一种多晶硅生产中的还原炉石墨电极,它由石墨底座(5)、石墨夹盖(3)、石墨夹瓣(2)、硅芯(1)构成,其特征在于:石墨底座(5)的顶部带螺纹,石墨夹盖(3)的内部带有螺纹,石墨底座(5)和石墨夹盖(3)匹配夹持石墨夹瓣(2),石墨夹瓣(2)整体为圆锥形,石墨夹瓣(2)的中孔(8)为夹持硅芯(1)孔,硅芯(1)置于中孔(8)中,石墨夹瓣(2)再夹紧硅芯(1)。
2.如权利要求所述的还原炉石墨电极,其特征在于:石墨底座(5)底部为圆槽设计,其分别设计有外圆斜锥面(6)、内圆斜锥面(7)和中心小孔(4),内圆斜锥面(7)为导电接触面,外圆斜锥面(6)不作为导电接触面,中心小孔(4)为石墨底座(5)是受热膨胀缓冲孔。
3.如权利要求所述的还原炉石墨电极,其特征在于:石墨夹瓣(2)的夹瓣整体为圆锥形,中孔(8)为夹持硅芯(1)孔,石墨夹瓣(2)的夹瓣三等分切削为三瓣,对硅芯(1)的三个方向夹紧固定硅芯。