CN202106622U - 一种太阳能反光复合膜 - Google Patents

一种太阳能反光复合膜 Download PDF

Info

Publication number
CN202106622U
CN202106622U CN2011201937935U CN201120193793U CN202106622U CN 202106622 U CN202106622 U CN 202106622U CN 2011201937935 U CN2011201937935 U CN 2011201937935U CN 201120193793 U CN201120193793 U CN 201120193793U CN 202106622 U CN202106622 U CN 202106622U
Authority
CN
China
Prior art keywords
layer
film
solar energy
coating
utility
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011201937935U
Other languages
English (en)
Inventor
徐诵舜
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xu Songshun
Original Assignee
NANJING NANZHOU NEW ENERGY RESEARCH AND DEVELOPMENT Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NANJING NANZHOU NEW ENERGY RESEARCH AND DEVELOPMENT Co Ltd filed Critical NANJING NANZHOU NEW ENERGY RESEARCH AND DEVELOPMENT Co Ltd
Priority to CN2011201937935U priority Critical patent/CN202106622U/zh
Application granted granted Critical
Publication of CN202106622U publication Critical patent/CN202106622U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开一种太阳能反光复合膜,由上至下顺序依次真空镀铝层、聚酯薄膜层、压敏胶层和保护膜,在所述真空度铝层上还设有聚四氟乙烯透明涂料层或液态玻璃层。本实用新型通过在其镀铝层表面涂上一层耐高温、防老化、防腐蚀、高透光率的透明聚四氟乙烯或液态玻璃涂料,是其反光膜能够耐受260℃的高温,对光线的透过率可达到94%,可延长其使用寿命至25年,并且可以利用雨水可到达自洁效果。

Description

一种太阳能反光复合膜
技术领域
本实用新型涉及一种反光膜,准确的说是一种太阳能反光复合膜。
背景技术
现有的用于太阳能反光膜的复合工艺为在基材(各种聚酯薄膜)正面设有真空镀铝层,利用镀铝层形成反光面,为防止镀铝层氧化,在镀铝层上通过EVA胶覆盖透明玻璃形一层保护膜,背面涂上一层压敏胶,胶上有一层保护膜,用时只要撕下保护膜,贴在物体表面压紧即可。在这种复合工艺下的反光膜使用寿命一般为5--10年,10年后镀铝层会被氧化而变黑,反光效果很差,即便是当今最好的美国3M公司生产的反光膜最多也只能保证使用15年,15年后也会出现同样的问题。然而目前硅光电池的设计使用寿命为25年,反光膜的使用寿命远远低于硅光电池的使用寿命;然而更换反光膜不仅比较麻烦,而且还要浪费大量的财力物力。
实用新型内容
本实用新型所要解决的技术问题是,克服现有技术的缺点,提供一种耐高温、耐老化、防腐蚀、高透光的太阳能反光复合膜。
为了解决以上技术问题,本实用新型提供一种太阳能反光复合膜,由上至下顺序依次真空镀铝层、聚酯薄膜层、压敏胶层和保护膜,在所述真空度铝层上还设有聚四氟乙烯透明涂料层或液态玻璃层。
本实用新型进一步限定的技术方案是:前述的太阳能反光复合膜,在所述真空度铝层与所述聚四氟乙烯透明涂料层或液态玻璃层之间还设有层聚氨酯与丙烯酸的混合料层。
进一步的,前述的太阳能反光复合膜,所述聚四氟乙烯透明涂料层或液态玻璃层的厚度为10~20微米。
本实用新型的有益效果是:本实用新型耐高温、耐老化、防腐蚀、高透光;能够耐受260℃的高温,对光线的透过率可达到94%,可延长其使用寿命至25年,并且可以利用雨水可到达自洁效果。
附图说明
图1为本实用新型结构示意图。
具体实施方式
    实施例1
本实施例提供的一种太阳能反光复合膜,结构如图1所示,由上至下顺序依次真空镀铝层3、聚酯薄膜层4、压敏胶层5和保护膜6,在所述真空度铝层上还设有一层15微米厚的氟碳涂层1,该涂层的主要成分为聚四氟乙烯,为了使聚四氟乙烯透明涂料与真空度铝层结合的更加牢固,在其之间还设有一层15微米聚氨酯与丙烯酸的混合料层2。
聚四氟乙烯透明涂料层,具有耐高温、耐老化、防腐蚀、高透光的性能,能够耐受260℃高温,对光线的透过率可达到94%,耐候性可达25年以上,完全满足了硅光电池的使用寿命,大大的降低了成本。
除上述实施例外,本实用新型还可以有其他实施方式。凡采用等同替换或等效变换形成的技术方案,均落在本实用新型要求的保护范围。

Claims (2)

1.一种太阳能反光复合膜,由上至下顺序依次真空镀铝层、聚酯薄膜层、压敏胶层和保护膜层,其特征在于:在所述真空度铝层上还设有聚四氟乙烯透明涂料层或液态玻璃层。
2.根据权利要求1所述的太阳能反光复合膜,其特征在于:所述聚四氟乙烯透明涂料层或液态玻璃层的厚度为10~20微米。
CN2011201937935U 2011-01-28 2011-06-10 一种太阳能反光复合膜 Expired - Fee Related CN202106622U (zh)