CN202055558U - 混凝土裂缝骑缝孔灌浆装置 - Google Patents
混凝土裂缝骑缝孔灌浆装置 Download PDFInfo
- Publication number
- CN202055558U CN202055558U CN2011201204883U CN201120120488U CN202055558U CN 202055558 U CN202055558 U CN 202055558U CN 2011201204883 U CN2011201204883 U CN 2011201204883U CN 201120120488 U CN201120120488 U CN 201120120488U CN 202055558 U CN202055558 U CN 202055558U
- Authority
- CN
- China
- Prior art keywords
- roulette
- grouting
- grout
- nozzle
- concrete crack
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种混凝土裂缝骑缝孔灌浆装置,包括注浆嘴,混凝土裂缝上开设有骑缝孔,注浆嘴底端与骑缝孔上端连接;注浆嘴由嘴底板和安装在嘴底板上的注浆管组成,嘴底板底端与骑缝孔上端连接;注浆嘴底端通过胶凝材料层与骑缝孔上端连接。本实用新型提供的混凝土裂缝骑缝孔灌浆装置,骑缝孔起到了灌浆盒的作用,克服了现有注浆嘴的平面式嘴底板以“点式”出浆格式出浆,造成浆液难以排出的不足,浆液易排出,不易造成漏浆事故;加大了裂缝受灌长度,变“点受浆”为“线受浆”模式,利于浆液的注入,确保了灌浆效果;本实用新型改变了出、受浆格式,保证了“钻孔+贴嘴法”化学灌浆施工工艺的顺利实施,结构简单,施工便捷,成本低。
Description
技术领域
本实用新型涉及一种混凝土裂缝内部化学灌浆修补施工用装置,尤其是一种混凝土裂缝骑缝孔灌浆装置。
背景技术
目前,在混凝土裂缝内部化学灌浆修补技术中使用的注浆嘴通常由平面式的嘴底板和注浆管组成。
当混凝土裂缝修补采用 “钻孔+贴嘴法”化学灌浆施工工艺时,其浆液在缝内行径的路线为:从缝底向缝口逐渐扩散,最后由注浆嘴排出,此时表明裂缝面充填饱满、密实。若采用现有注浆嘴,在该工艺条件下,其使用功能上存在两个不足:1、该注浆嘴由于采用平面式的嘴底板,为“点式”出浆格式,不利于浆液的排出,容易使封缝和注浆嘴被顶开造成漏浆事故;2、当灌浆需要再由注浆嘴向缝内反灌时,注浆嘴嘴底无一个储浆装置,裂缝受浆长度偏小,为“点”受浆格式,不利于浆液的注入。
发明内容
本实用新型所要解决的技术问题是提供一种混凝土裂缝骑缝孔灌浆装置,能克服现有注浆嘴的不足,改变了出、受浆格式,保证了“钻孔+贴嘴法” 化学灌浆施工工艺的顺利实施。
为解决上述技术问题,本实用新型所采用的技术方案是:一种混凝土裂缝骑缝孔灌浆装置,包括注浆嘴,混凝土裂缝上开设有骑缝孔,注浆嘴底端与骑缝孔上端连接。
注浆嘴由嘴底板和安装在嘴底板上的注浆管组成,嘴底板底端与骑缝孔上端连接。
注浆嘴底端通过胶凝材料层与骑缝孔上端连接。
本实用新型提供的混凝土裂缝骑缝孔灌浆装置,由于在混凝土裂缝上开设有骑缝孔,将现有的注浆嘴底端与骑缝孔上端连接,骑缝孔起到了灌浆盒的作用,克服了现有注浆嘴的平面式嘴底板以“点式”出浆格式出浆,造成浆液难以排出的不足,浆液易排出,不易造成漏浆事故;加大了裂缝受灌长度,变“点受浆”为“线受浆”模式,利于浆液的注入,确保了灌浆效果;本实用新型改变了出、受浆格式,保证了“钻孔+贴嘴法”化学灌浆施工工艺的顺利实施,结构简单,施工便捷,成本低。
附图说明
下面结合附图和实施例对本实用新型作进一步说明:
图1为本实用新型的结构示意图。
具体实施方式
如图1所示,本实用新型包注浆嘴1,混凝土裂缝5上开设有骑缝孔2, 注浆嘴1底端与骑缝孔2上端连接。
注浆嘴1由嘴底板3和安装在嘴底板3上的注浆管4组成,嘴底板3底端与骑缝孔2上端连接,嘴底板3为平板式。
注浆嘴1底端通过胶凝材料层6与骑缝孔2上端连接。
骑缝孔以裂缝5为中心线,采用取芯钻钻取,孔深根据需要适宜即可。
本实用新型的安装及使用步骤如下:
1、采用取芯钻钻取孔深适宜的骑缝孔2,起到了灌浆盒的作用。
2、将骑缝孔2清洗干净。
3、粘贴注浆嘴1:先在嘴底板3四周涂胶凝材料,形成胶凝材料层6,用定位
针穿过注浆管4,对准裂缝5的缝口插入并将注浆嘴1压向混凝土面,拔出定位针时,以不粘附胶凝材料为合格;待所有注浆嘴1粘贴完毕且胶凝材料凝固即可。
4、在注浆嘴1背面,连同裂缝5的封缝胶凝材料一起进行覆盖,起到加固、稳
定作用。
5、连接灌浆管进行试气(压风)、灌浆等,完成注浆全部工序。
灌浆结束待浆液固化后,应对贴嘴及封缝材料进行拆除清理。
Claims (3)
1.一种混凝土裂缝骑缝孔灌浆装置,包括注浆嘴(1),其特征在于:混凝土裂缝(5)上开设有骑缝孔(2), 注浆嘴(1)底端与骑缝孔(2)上端连接。
2.根据权利要求1所述的混凝土裂缝骑缝孔灌浆装置,其特征在于:注浆嘴(1)由嘴底板(3)和安装在嘴底板(3)上的注浆管(4)组成,嘴底板(3)底端与骑缝孔(2)上端连接。
3.根据权利要求1所述的混凝土裂缝骑缝孔灌浆装置,其特征在于:注浆嘴(1)底端通过胶凝材料层(6)与骑缝孔(2)上端连接。