CN202040447U - 钢塑瓷复合管 - Google Patents
钢塑瓷复合管 Download PDFInfo
- Publication number
- CN202040447U CN202040447U CN2011201176440U CN201120117644U CN202040447U CN 202040447 U CN202040447 U CN 202040447U CN 2011201176440 U CN2011201176440 U CN 2011201176440U CN 201120117644 U CN201120117644 U CN 201120117644U CN 202040447 U CN202040447 U CN 202040447U
- Authority
- CN
- China
- Prior art keywords
- pipe
- plastic
- steel
- ceramic
- coal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及燃煤火力发电厂管道输送系统,尤其涉及燃煤电厂煤粉除渣排灰输送管道。一种钢塑瓷复合管,包括外层钢管(1)和内衬陶瓷管(2),在外层钢管和内衬陶瓷管之间设置有塑胶层(3),塑胶层紧贴外层钢管,内衬陶瓷管粘贴在塑胶层内壁上。所述陶瓷管的段与段之间的连接为高温粘胶(4)连接。本实用新型将陶瓷的耐磨损及塑料的耐腐蚀性能相结合,从而提高了管道的耐磨损及耐腐蚀性能,大幅度延长了燃煤电厂煤粉除渣排灰输送管道的使用寿命。
Description
技术领域
本实用新型涉及燃煤火力发电厂管道输送系统,尤其涉及燃煤电厂煤粉除渣排灰输送管道。
背景技术
目前国内各燃煤电厂除渣及排灰管道系统上一般采用以下两种管道:一种是离心浇铸复合陶瓷管道,该管道是采用“自蔓燃高温合成-高速离心技术”制造的复合管材,在高温高速下形成均匀、致密且表面光滑的陶瓷层及过渡层;其制作工艺简单,成本较低,并且具有良好的耐热、耐腐蚀能力,但缺点是其耐磨性比耐磨陶瓷管道差,因此在燃煤电厂的除渣排灰输送管道中容易磨损。另一种是耐磨陶瓷管道,该陶瓷管道采用耐高温强力粘胶将氧化铝陶瓷2粘贴在钢管1道内壁,经加温固化后形成牢固防磨层,参见图1;该种产品耐磨性能良好,制作工艺相对简单,制作周期短,应用较广,如以内衬陶瓷管90°弯头为例,由于其特殊性,在其弯头内的内衬陶瓷管分为了五段,才可布满其内部,每段陶瓷管之间均由高温粘胶连接。
现有的两种管道技术存在的主要问题是:由于煤渣会对管道造成强烈的机械冲击和热冲击,离心浇铸复合陶瓷管道在耐磨性能方面弱于耐磨陶瓷管道,以某企业为例,使用0.5-1年后打开观察并测量,复合层均有明显的磨损或脱落,磨损严重的管道会出现磨穿的现象。对于耐磨陶瓷管道来说,因为受到高温耐磨陶瓷生产工艺的局限,使得长度超过500mm的陶瓷直管烧制异常困难,因而造成长度过长的钢管,内贴陶瓷管之间的连接则必须依靠高温粘胶来实现;另一方面,弯头和三通等部件内贴陶瓷各部分的粘胶连接则更是无法避免。尽管耐磨陶瓷管道具有较强的耐磨性,但由于煤渣及煤粉具有较强的腐蚀性,随着管道的使用,钢管内贴陶瓷粘贴缝隙中的高温粘胶经受不了煤渣不断的腐蚀,因而最终透过粘胶层而腐蚀穿外围钢管。
发明内容
本实用新型的目的在于提供一种钢塑瓷复合管,该钢塑瓷复合管将陶瓷的耐磨损及塑料的耐腐蚀性能相结合,从而提高了管道的耐磨损及耐腐蚀性能,大幅度延长了燃煤电厂煤粉除渣排灰输送管道的使用寿命。
为了实现上述目的,本实用新型采用如下技术方案:
一种钢塑瓷复合管,包括外层钢管和内衬陶瓷管,在外层钢管和内衬陶瓷管之间设置有塑胶层,塑胶层紧贴外层钢管,内衬陶瓷管粘贴在塑胶层内壁上。
所述陶瓷管的段与段之间的连接为高温粘胶连接。
本实用新型在外层钢管和内衬陶瓷管之间设置有塑胶层,内衬陶瓷管的段与段之间通过高温粘胶连接,内衬塑胶层具有耐腐蚀的性能,能阻碍煤渣及煤粉穿透外层的钢管,从而将陶瓷的耐磨损性及塑料的耐腐蚀性有机结合,提高了管道的耐磨损及耐腐蚀性能,大幅度延长了燃煤电厂煤粉除渣排灰输送管道的使用寿命,提高管道的使用寿命至2~3年,比现有管道提高了5~10倍;克服了现有离心浇铸复合陶瓷管道容易磨损的缺陷,以及现有耐磨陶瓷管缝隙连接处粘胶层不耐腐蚀的缺陷。
附图说明
图1为现有的内衬陶瓷直管结构示意图;
图2为本实用新型钢塑瓷复合管结构示意图。
图中:1钢管,2陶瓷管,3塑胶层,4高温粘胶。
具体实施方式
下面结合附图和具体实施例对本实用新型作进一步说明。
参见图2,一种钢塑瓷复合管,包括外层钢管1和内衬陶瓷管2,在外层钢管1和内衬陶瓷管2之间设置有塑胶层3,塑胶层3紧贴外层钢管1,陶瓷管2粘贴在塑胶层3内壁上,所述陶瓷管2的段与段之间的连接为高温粘胶4连接。
本实用新型的衬塑钢管是通过对金属管的缩径压迫内层塑料管,使两种材料产生永久性合理过盈,加之金属管内表面的花纹内筋对塑料管外表面的嵌入作用,以及塑料管复合前的物理和化学改性,使得塑钢管具有不分层、不缩管,长期使用有保障的技术特点,其复合质量高。陶瓷管2道采用耐高温强力粘胶将氧化铝陶瓷粘贴在钢管1道内壁,经加温固化后形成牢固防磨层。
本实用新型的钢塑瓷复合管的内衬陶瓷管2的段与段之间通过高温粘胶4连接,内衬塑胶层3具有耐腐蚀的性能,能阻碍煤渣及煤粉穿透外层的钢管,从而将陶瓷的耐磨损性及塑料的耐腐蚀性有机结合,提高了管道的耐磨损及耐腐蚀性能,大幅度延长了燃煤电厂煤粉除渣排灰输送管道的使用寿命。
以上仅为本实用新型的较佳实施例而已,并非用于限定本实用新型的保护范围,因此,凡在本实用新型的精神和原则之内所作的任何修改、等同替换、改进等,均应包含在本实用新型的保护范围之内。
Claims (2)
1.一种钢塑瓷复合管,包括外层钢管(1)和内衬陶瓷管(2),其特征是:在外层钢管(1)和内衬陶瓷管(2)之间设置有塑胶层(3),塑胶层(3)紧贴外层钢管(1),内衬陶瓷管(2)粘贴在塑胶层(3)内壁上。
2.根据权利要求1所述的钢塑瓷复合管,其特征是:所述陶瓷管(2)的段与段之间的连接为高温粘胶(4)连接。