CN201981244U - 一种用于提高酸法处理铝矿石溶出效率的装置 - Google Patents
一种用于提高酸法处理铝矿石溶出效率的装置 Download PDFInfo
- Publication number
- CN201981244U CN201981244U CN2010206746516U CN201020674651U CN201981244U CN 201981244 U CN201981244 U CN 201981244U CN 2010206746516 U CN2010206746516 U CN 2010206746516U CN 201020674651 U CN201020674651 U CN 201020674651U CN 201981244 U CN201981244 U CN 201981244U
- Authority
- CN
- China
- Prior art keywords
- outer tube
- dissolution efficiency
- pipe
- carrier pipe
- acid treatment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种用于提高酸法处理铝矿石溶出效率的装置,包括用于输送含高浓度酸的原矿浆的输料管(1),其输料管(1)为锆金属材料结构的输料管,在输料管(1)的一段上包裹有外管(2),在外管(2)上设有蒸汽热源连接管(4)和出汽管(5)。本实用新型不仅具有结构简单、操作方便、溶出效率高、能提高现有生产线的生产能力的优点,而且还具有投资小、效果显著、使用寿命长等优点。
Description
技术领域
本实用新型涉及一种用于提高酸法处理铝矿石溶出效率的装置,属于酸法处理铝矿石溶出技术领域。
背景技术
目前,在用酸法处理铝矿石时,一般都是采用高浓度的无机酸与原矿浆在溶出池中进行溶出,在进行一段时间溶出后,再将含高浓度酸的原矿浆输送到下一工序进行处理。现有的这种溶出方式存在着溶出时间较长、溶出效率较低的问题。因此还是不能满足生产的需要。
且溶出温度也较高,这时需要一种新型的溶出装置,该装置必需能耐腐蚀耐高温,溶出效率高,可以提高生产能力(流动速度快,效率高)。
发明内容
本实用新型的目的在于:提供一种结构简单、操作方便、溶出效率较高、能提高生产能力的用于提高酸法处理铝矿石溶出效率的装置,以克服现有技术的不足。
本实用新型是这样实现的:本实用新型的一种用于提高酸法处理铝矿石溶出效率的装置为:该装置包括用于输送含高浓度酸的原矿浆的输料管,该输料管为锆金属材料结构的输料管,在输料管的一段上包裹有外管,在外管上设有蒸汽热源连接管和出汽管。
上述外管通过异径接头连接在输料管上,并且在外管内与输料管之间连接有支持板。
上述外管的长度不小于12米。
在上述的外管上安装有用于补偿外管与输料管之间热胀差的填料函。
由于采用了上述技术方案,本实用新型利用输送含高浓度酸的原矿浆的过程中,对含高浓度酸原矿浆进行加热,使含高浓度酸的原矿浆在输送过程中、并在高温条件下使其溶出速度加快,从而大大降低了原有工艺生产线所需的时间,有效地提高了酸法处理铝矿石的溶出效率。本实用新型的装置结构简单,加工制造容易,耐腐蚀性能良好,使用寿命长;并且介质在管内的流动速度高,传热效果好,单位时间流量大,运转效率高,节约了能源,大大提高了生产能力。因此,本实用新型与现有技术相比,本实用新型不仅具有结构简单、操作方便、溶出效率高、能提高现有生产线的生产能力的优点,而且还具有投资小、效果显著、使用寿命长等优点。
附图说明
图1为本实用新型装置的结构示意图;
图2为图1的A-A剖视结构示意图。
附图标记说明:1-输料管,2-外管,3-填料函,4-连接管,5-出汽管,6-异径接头,7-支持板,L-外管长度。
具体实施方式
下面结合附图和实施例对本实用新型作进一步的详细说明。
本实用新型的实施例:本实用新型可用于对现有的酸法处理铝矿石的生产线进行改造,实施时,采用锆金属材料制作的输料管来输送含高浓度酸的原矿浆,并在输料管的一段上套一个外管,然后向外管中输入蒸汽热源,使通过输料管流经包裹有外管段的含高浓度酸的原矿浆被加热,这样即可使含高浓度酸的原矿浆在输送的过程中、并在高温条件下使其溶出速度加快,从而提高酸法处理铝矿石的溶出效率。具体实施时,最好采用本实用新型的一种用于提高酸法处理铝矿石溶出效率的装置进行实施,该装置的结构示意图如图1和图2所示,包括用于输送含高浓度酸的原矿浆的输料管1,输料管1为采用锆金属材料制作的输料管,制作时,在输料管1的一段上套一节外管2,外管2可采用普通钢管制作,将外管2的长度L制作成不小于12米,并将外管2通过异径接头6焊接或紧密地套接在输料管1上,在外管2的一端制作出能与蒸汽热源管道连接的连接管4,在外管2的另一端制作一个出汽管5(如图1所示),为了更加稳固地支撑输料管1,可在外管2内与输料管1之间固定上支持板7(如图2所示),支持板7的材料可选用钛合金材料制作;为了在工作时能较好地补偿输料管1与外管2之间的热胀差,可在外管2上安装上用于补偿外管2与输料管1之间热胀差的填料函3;填料函3可直接采用现有技术中的填料函成品来安装即可。
Claims (4)
1.一种用于提高酸法处理铝矿石溶出效率的装置,包括用于输送含高浓度酸的原矿浆的输料管(1),其特征在于:输料管(1)为锆金属材料结构的输料管,在输料管(1)的一段上包裹有外管(2),在外管(2)上设有蒸汽热源连接管(4)和出汽管(5)。
2.根据权利要求1所述的用于提高酸法处理铝矿石溶出效率的装置,其特征在于:外管(2)通过异径接头(6)连接在输料管(1)上,并且在外管(2)内与输料管(1)之间连接有支持板(7)。
3.根据权利要求1或2所述的用于提高酸法处理铝矿石溶出效率的装置,其特征在于:外管(2)的长度(L)不小于12米。
4.根据权利要求1或2所述的用于提高酸法处理铝矿石溶出效率的装置,其特征在于:在外管(2)上安装有用于补偿外管(2)与输料管(1)之间热胀差的填料函(3)。