CN201901709U - 一种新型过硫酸铵的生产装置 - Google Patents
一种新型过硫酸铵的生产装置 Download PDFInfo
- Publication number
- CN201901709U CN201901709U CN2010206405899U CN201020640589U CN201901709U CN 201901709 U CN201901709 U CN 201901709U CN 2010206405899 U CN2010206405899 U CN 2010206405899U CN 201020640589 U CN201020640589 U CN 201020640589U CN 201901709 U CN201901709 U CN 201901709U
- Authority
- CN
- China
- Prior art keywords
- copper bar
- bar
- negative pole
- production equipment
- electrolyzer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Abstract
本实用新型提供了一种新型过硫酸铵的生产装置,包括电解槽、正极铜排、负极铜排、阳极和阴极,所述电解槽是用塑料板制造,所述正极铜排和所述负极铜排位于所述电解槽的上方,所述阳极与正极铜排连接,所述阴极与负极铜排连接,其特征在于:所述阴极为若干个石墨阴极板;所述阳极是钛杆外螺旋绕钋丝并点焊而成。本实用新型提供的一种新型过硫酸铵的生产装置,具有环保高效节能的特点。
Description
技术领域
本实用新型涉及了一种新型过硫酸铵的生产装置,特别是一种高效节能环保并且能连续生产的过硫酸铵生产装置。
背景技术
目前国内生产过硫酸铵的装置是以钛板点焊钋丝作阳极,上端用钛板引出连接于加电铜排,以铅板作负极,上端用铅板排引出并连接于加电铜排,置于塑料槽中,注入一定浓度的硫酸铵溶液,接通电源后,电解硫酸铵产生过硫酸铵,这两种溶液混在一起,在不断加入硫酸铵溶液后,就不断有硫酸铵和过硫酸铵的混合溶液溢流排出,对该种混合溶液冷冻后,过硫酸铵结晶析出,剩下的硫酸铵溶液再加热反固,配置硫酸铵溶液再加入电解槽。以铅板作阴极,制作过程中会被硫酸溶液腐蚀,生成包色的硫酸铅,常称作铅泥,大部分沉淀在电解槽的底部,少量的铅泥会含在过硫酸铵的成品中,并影响了产品品质,铅板的使用寿命一般在一年半左右。目前对铅泥的处理非常困难,铅泥是有毒的重金属,严重污染环境,这种生产装置每隔一年半左右就要全面停产捞出铅泥清理电解槽,更换新铅板,铅板在电解过程中被腐蚀的铅泥会覆盖在铅板表面,从而影响电解,降低生产效率。
发明内容
为了克服现有技术中的缺点,本实用新型提供了一种新型过硫酸铵的生产装置,包括电解槽、正极铜排、负极铜排、阳极和阴极,所述电解槽是用塑料板制造,所述正极铜排和所述负极铜排位于所述电解槽的上方,所述阳极与正极铜排连接,所述阴极与负极铜排连接,其特征在于:所述阴极为若干个石墨阴极板;所述阳极是钛杆外螺旋绕钋丝并点焊而成。
所述石墨阴极板螺纹固定在石墨导电杆上,并置于所述电解槽中。
所述石墨导电杆上端与所述负极铜排连接。
所述钛杆置于隔膜管中,并钛杆的上端与正极铜排连接。
所述隔膜管为陶瓷隔膜管,该隔膜管下端封闭,上端开口,并插在一塑料盒的底板上。
该装置至少有6个所述塑料盒,该塑料盒上端开口,以便引出所述钛杆与正极铜排连接;所述塑料盒用一出口管连接并引出所述电解槽外。
本实用新型的优点:
1、环保,寿命长,石墨的耐腐蚀性能非常好,在硫酸铵溶液里不会被腐蚀,也无任何杂质分解出,也就保证了产品的纯度,对环境部产生任何影响,解决了原生产装置的铅泥的污染问题,实现了清洁生产。
2、高效节能
由于石墨阴极板表面不被腐蚀并直接与电解液接触,两只之间不存在电阻,因此生产效率会很高;本实用新型采用了隔膜管分离技术,电焊产生的产品进入隔膜管,并由塑料盒收集,再通过与塑料盒连接的出口管引出,进入收集总管,流进冷冻分离工序,这样就实现了产品直接与原料溶液的分开,节省了能量。
附图说明
图1是本实用新型的结构示意图;
图2是图1的右视图。
附图说明:1、电解槽2、负极铜排3、石墨阴极板4、石墨导电杆5、出口管6、塑料盒7、正极铜排8、隔膜管9、钛杆
具体实施方式
以下是通过附图详细说明本实用新型的技术方案。
如图1和2所示,本实用新型所述的一种新型过硫酸铵的生产装置,用塑料板制造电解槽1,采用石墨阴极板3作为阴极,并置于电解槽1中,石墨阴极板3采用高强度的高纯石墨螺丝固定在石墨导电杆4上,石墨导电杆4上端与负极铜排2连接。阳极是以钛杆9外螺旋绕钋丝并电焊制作而成,并置于陶瓷隔膜管8中,隔膜管8下端封闭,上端开口并插在塑料盒6的底板上,所述塑料盒6上面开口,以便引出钛杆9与正极铜排7连接,该生产装置至少有6个所述的塑料盒6,所述塑料金6用一出口管5连接并引出电解槽1外。
在电解槽1中加入一定浓度的硫酸铵溶液,再将正极铜排7和负极铜排2加上直流电,那么阳极钋与阴极石墨就对硫酸铵进行电解,产生的过硫酸铵进入陶瓷隔膜管8中,汇集到其上端的塑料盒6里,并从出口管5流出,再进行冷冻结晶和离心分离,生成颗粒状的过硫酸铵,电解槽1中不断加入硫酸铵溶液,在电解作用下,就不断产生过硫酸铵,实现了连续生产。
Claims (6)
1.一种新型过硫酸铵的生产装置,包括电解槽、正极铜排、负极铜排、阳极和阴极,所述电解槽是用塑料板制造,所述正极铜排和所述负极铜排位于所述电解槽的上方,所述阳极与正极铜排连接,所述阴极与负极铜排连接,其特征在于:所述阴极为若干个石墨阴极板;所述阳极是钛杆外螺旋绕钋丝并点焊而成。
2.根据权利要求1所述的生产装置,其特征在于:所述石墨阴极板螺纹固定在石墨导电杆上,并置于所述电解槽中。
3.根据权利要求1或2所述的生产装置,其特征在于:所述石墨导电杆上端与所述负极铜排连接。
4.根据权利要求1所述的生产装置,其特征在于:所述钛杆置于隔膜管中,并钛杆的上端与正极铜排连接。
5.根据权利要求4所述的生产装置,其特征在于:所述隔膜管为陶瓷隔膜管,该隔膜管下端封闭,上端开口,并插在一塑料盒的底板上。
6.根据权利要求1或5所述的生产装置,其特征在于:该装置至少有6个所述塑料盒,该塑料盒上端开口,以便引出所述钛杆与正极铜排连接;所述塑料盒用一出口管连接并引出所述电解槽外。