CN201756572U - 一种防止连续退火炉内带钢划伤的装置 - Google Patents

一种防止连续退火炉内带钢划伤的装置 Download PDF

Info

Publication number
CN201756572U
CN201756572U CN2010202371075U CN201020237107U CN201756572U CN 201756572 U CN201756572 U CN 201756572U CN 2010202371075 U CN2010202371075 U CN 2010202371075U CN 201020237107 U CN201020237107 U CN 201020237107U CN 201756572 U CN201756572 U CN 201756572U
Authority
CN
China
Prior art keywords
continuous annealing
steel strip
annealing furnace
polyurethane rubber
drying box
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010202371075U
Other languages
English (en)
Inventor
王静
谢志彪
郭洪宇
张大韬
郑庆福
唐伟
蔡恒君
赵德华
崔恒
柳军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Angang Steel Co Ltd
Original Assignee
Angang Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Angang Steel Co Ltd filed Critical Angang Steel Co Ltd
Priority to CN2010202371075U priority Critical patent/CN201756572U/zh
Application granted granted Critical
Publication of CN201756572U publication Critical patent/CN201756572U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种防止连续退火炉内带钢划伤的装置,在连续退火炉烘干箱出口和转向辊之间上下交错设置两根聚氨酯胶辊,聚氨酯胶辊两端通过轴承座连接在烘干箱风机风箱上。由于从连续退火炉烘干箱出来的带钢行进在两根聚氨酯胶辊之间,从而缓解了带钢的抖动幅度,避免带钢与烘干箱出口接触,减少带钢表面划伤及其他缺陷的生成,提高带钢的表面质量,保证机组生产的稳定性,提高连续退火线的生产速度,增加了企业收益。其结构简单,便于操作和维护,可适应不同规格冷轧板的调整需要。

Description

一种防止连续退火炉内带钢划伤的装置
技术领域
本实用新型属于退火设备领域,尤其涉及一种避免大型立式连续退火炉生产时烘干箱划伤带钢表面的装置。
背景技术
近年来,随着汽车、家电等行业逐步向节能降耗方向迈进,市场上对于0.6mm以下的冷轧板的需求量也越来越大。由于在罩式炉退火工艺流程生产较薄的冷轧板会出现粘结这一固有缺陷,因此薄料生产的合格率较低。同时由于连续退火生产的冷轧板具有表面清洁度高,板型好等优点,国内外连续退火生产线薄料的生产比例亦就越来越大。
对于以薄料生产为主的连续退火机组,要想达产就必须使生产薄料时的速度达到280m/min以上,但在机组速度提高的同时带钢抖动幅度也在增大,极易使带钢接触连续退火炉的烘干箱风口,造成钢板表面划伤。为了保证钢板表面质量,则必须降速,但是频繁的降速会带来温度不合、炉内辊印等一系列缺陷,从而给机组的达产造成很大的困难,所以必须突破连续退火生产线的这一痼疾,以便高速生产出高质量的冷轧薄板,满足日益增长的市场需求。
发明内容
本实用新型的目的旨在提供一种结构简单,便于操作,能有效防止大型立式连续退火炉烘干箱风口划伤卷板的缺陷,从而实现迅速达产的装置。
为此,本实用新型采取的解决方案是:
一种防止连续退火炉内带钢划伤的装置,是在连续退火炉烘干箱出口和转向辊之间设置两根聚氨酯胶辊,聚氨酯胶辊两端通过轴承座连接在烘干箱风机风箱上。
所述的聚氨酯胶辊直径为¢75~¢90mm;两根聚氨酯胶辊采用上下交错布置,两根聚氨酯胶辊上下间距为80~90mm,水平距离为87~92mm。
由于在连续退火炉烘干箱出口设置两根聚氨酯胶辊,从而有效缓解和控制了带钢的抖动幅度,避免带钢与烘干箱出口接触,减少了带钢表面划伤及其他缺陷的生成,提高了带钢的表面质量,满足了用户的质量要求。同时,保证了机组生产的稳定性,相对提高了连续退火线的生产速度,增加了企业收益。其结构简单,便于操作和维护,投资少、见效快,且可适应不同规格冷轧板的调整需要。
附图说明
附图为本实用新型安装状态示意图。
图中:转向辊1、带钢2、聚氨酯胶辊3、烘干箱4。
具体实施方式
附图为防止连续退火炉内带钢划伤的装置安装状态示意图,居于上部的是两个转向辊1,转向辊1的下方为烘干箱4,从烘干箱4上端出口出来的带钢2绕在转向辊1上,并通过转向辊1改变前进方向。本实用新型是在烘干箱4出口和转向辊1之间设置两根直径为¢80mm的聚氨酯胶辊3,聚氨酯胶辊3的两端通过轴承座连接在烘干箱4的风机风箱上面。聚氨酯胶辊3的长度根据退火带钢的最大宽度确定,即聚氨酯胶辊3的长度应大于带钢的最大宽度,本实用新型选取的长度为1800mm。两根聚氨酯胶辊3之间上下交错布置,两根聚氨酯胶辊上下间距为85mm;水平距离为90mm,小于烘干机风口间距100mm。同时,两根聚氨酯胶辊3之间水平距离可以调整,以适应不同规格料的调整需要。

Claims (3)

1.一种防止连续退火炉内带钢划伤的装置,其特征是,在连续退火炉烘干箱出口和转向辊之间设有两根聚氨酯胶辊,聚氨酯胶辊两端通过轴承座连接在烘干箱风机风箱上。
2.根据权利要求1所述的防止连续退火炉内带钢划伤的装置,其特征是,所述的两根聚氨酯胶辊采用上下交错布置,两根聚氨酯胶辊上下间距为80~90mm,水平距离为87~92mm。
3.根据权利要求1所述的防止连续退火炉内带钢划伤的装置,其特征是,所述的聚氨酯胶辊直径为¢75~¢90mm。
CN2010202371075U 2010-06-25 2010-06-25 一种防止连续退火炉内带钢划伤的装置 Expired - Fee Related CN201756572U (zh)