CN201738484U - 薄壁空心砖 - Google Patents

薄壁空心砖 Download PDF

Info

Publication number
CN201738484U
CN201738484U CN2010202586626U CN201020258662U CN201738484U CN 201738484 U CN201738484 U CN 201738484U CN 2010202586626 U CN2010202586626 U CN 2010202586626U CN 201020258662 U CN201020258662 U CN 201020258662U CN 201738484 U CN201738484 U CN 201738484U
Authority
CN
China
Prior art keywords
thin
brick
walled hollow
hollow brick
moulded
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010202586626U
Other languages
English (en)
Inventor
周忠平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZAOYANG BEIJIXING BUILDING MATERIAL CO Ltd
Original Assignee
ZAOYANG BEIJIXING BUILDING MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZAOYANG BEIJIXING BUILDING MATERIAL CO Ltd filed Critical ZAOYANG BEIJIXING BUILDING MATERIAL CO Ltd
Priority to CN2010202586626U priority Critical patent/CN201738484U/zh
Application granted granted Critical
Publication of CN201738484U publication Critical patent/CN201738484U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种薄壁空心砖,用于建筑领域。砖体内有通孔,砖体内的孔为错缝“三二三二三”排列。经多次搅拌及沉化、发酵的泥料在真空挤泥机旋转的螺旋铰刀叶片推动下经过机口内的芯具,挤压成型为薄壁空心砖,湿坯砖经烘干室自动烘干后进入遂道窑焙烧、成型。本实用新型可增加成型砖体的强度,减轻砖体成型时泥条的阻力;薄壁空心窖重在650-700公斤/立方,大大提高了烧结空心砖的孔洞率,减轻了容重、形体的变化,使之更符合建筑模块,以适应变化万千的建筑艺术造型;真正做到了轻质、高强、环保、隔热、保暧、隔音,解决了外墙开裂、渗水等影响建筑结构的根本问题。

Description

薄壁空心砖
技术领域
本实用新型涉及制砖技术领域,特别是一种薄壁空心砖。
背景技术
目前国内高层框架结构填充墙应用得最多的是加气混凝土切块。这种砖的最大缺点就是吸水率高、遇到高温和低温时膨胀系数大,容易开裂、渗水,始终无法解决,严重超出了高层建筑的设计要求,以致无法在高层建筑房屋上使用。
发明内容
为克服现有技术的不足,本实用新型的发明目的在于提供一种薄壁空心砖,通过采用十三孔错缝“三二三二三”排列的空心结构,以提高烧结空心砖的孔洞率,减轻砖的容重的目的。
为实现上述目的,本实用新型的技术方案在于:砖体内有通孔,孔为错缝排列,第一列设3个孔,第二列设2个孔,第三列设3个孔,第四列设2个孔,第五列设3个孔,砖体外部有凹槽。
本实用新型与现有技术相比,可增加成型砖体的强度,减轻砖体成型时泥条的阻力;薄壁空心窖重在650-700公斤/立方,大大提高了烧结空心砖的孔洞率,减轻了容重、形体的变化,使之更符合建筑模块,以适应变化万千的建筑艺术造型;真正做到了轻质、高强、环保、隔热、保暧、隔音,解决了外墙开裂、渗水等影响建筑结构的根本问题。
附图说明
附图是本实用新型的立体简图。
具体实施方式
如附图所示,砖体1内有十三个孔,孔为错缝“三二三二三”排列。硬塑双级真空挤泥机将搅拌与抽真空密闭地串联在一起,在高压下,使经搅拌并切碎的泥料进入真空室,并在真空室中被抽取泥料中的空气后再次被挤出而成为表面光滑且密实的泥条,经多次搅拌及沉化、发酵的泥料在旋转的螺旋铰刀叶片推动下经过机口内的芯具,挤压成型为薄壁空心砖,湿坯砖经烘干室自动烘干后进入遂道窑焙烧、成型。成型的薄壁空心砖窖重在650-700公斤/立方,大大提高了烧结空心砖的孔洞率,减轻了容重、形体的变化;砖体1内孔错缝“三二三二三”排列,可有效提高砖体1的热工性能、湿传导性能,当烧结薄壁空心砖的导热系数λ=0.18w/(m·k)、墙厚为30cm,外墙的传热系数k值为0.65w(m2k),高强、环保、隔热、保暧、隔音,外墙无开裂、渗水等现象。

Claims (3)

1.一种薄壁空心砖,包括砖体(1),其特征在于:砖体(1)内有通孔,孔为错缝排列。
2.根据权利要求1所述的薄壁空心砖,其特征在于:砖体(1)内第一列设3个孔,第二列设2个孔,第三列设3个孔,第四列设2个孔,第五列设3个孔。
3.根据权利要求1所述的薄壁空心砖,其特征在于:砖体(1)外部有凹槽。
CN2010202586626U 2010-07-10 2010-07-10 薄壁空心砖 Expired - Fee Related CN201738484U (zh)