CN201706133U - 一种测温连接点带压堵漏工具 - Google Patents
一种测温连接点带压堵漏工具 Download PDFInfo
- Publication number
- CN201706133U CN201706133U CN2010201336318U CN201020133631U CN201706133U CN 201706133 U CN201706133 U CN 201706133U CN 2010201336318 U CN2010201336318 U CN 2010201336318U CN 201020133631 U CN201020133631 U CN 201020133631U CN 201706133 U CN201706133 U CN 201706133U
- Authority
- CN
- China
- Prior art keywords
- seamless steel
- temperature measurement
- leakage
- welded
- blind plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
一种测温连接点的堵漏工具,其特征是:在测温连接点用无缝钢管1,其中一端厚度小于另一端厚度的圆形盲板2闷死,在盲板中间开一圆孔,将截止阀3在开孔处焊接,无缝钢管1的长度视测温点的长度确定,无缝钢管1的壁厚视系统压力确定,一般为3.5mm-6mm,盲板2与无缝钢管1采用焊接的方式,盲板2的连缘打成坡口,增加焊接强度,截止阀3的接头插入盲板中间的开孔内并焊接牢固,截止阀接头内加垫片密封,直形连接头4焊接在设备管道5上,测温点6插入直形连接头4内并通过螺纹连接,中间用垫片密封,本实用新型提供的堵漏工具,其优点是,能在系统带压的情况下,消除测温连接点的泄漏,以避免物料的损失和减少环境污染。
Description
技术领域:
本实用新型属于化工、医药领域管道泄漏的一种堵漏工具,尤其涉及一种能在系统带压的情况下,消除测温连接点的泄漏,以避免物料的损失和减少环境污染的堵漏工具。
技术背景:
目前,在化工、医药生产工艺过程中,都是以管道连接,使一些汽体、液体、粉体等由一个工艺设备进入另一个工艺设备,在管道与管道连接过程中,都是采用螺丝连接,在测量管道温度时,采用在连接点上插入测温点,因此,天长日久,管道连接螺丝由于腐蚀等因素产生缝隙或滑丝,产生泄漏汽体、液体、粉体等现象,汽体、液体、粉体的泄漏是通过测温点进行测试,对于泄漏在紧固无效的情况下大多采用引流的方式,要么待停车处理,造成物料的损失和污染环境,但泄漏会逐渐加强,严重时被迫停车处理,给生产造成严重的经济损失。
发明内容:
为了实现在不停车的情况下消除测温连接点的泄漏,本实用新型提供一种堵漏工具,能在系统带压的情况下,消除测温连接点的泄漏,以避免物料的损失和减少环境污染。
本实用新型是通过以下技术方案实现本发明目的的。
一种测温连接点的堵漏工具,其特征是:在测温连接点用无缝钢管1和一端厚度小于另一端厚度的圆形盲板2闷死,在盲板中间开一圆孔,将截止阀3在开孔处焊接,无缝钢管1的长度视测温点的长度确定,无缝钢管1的壁厚视系统压力确定,一般为3.5mm-6mm,盲板2与无缝钢管1采用焊接的方式,盲板2的连缘打成坡口,增加焊接强度,截止阀3的接头插入盲板中间的开孔内并焊接牢固,截止阀接头内加垫片密封,直形连接头4焊接在设备管道5上,测温点6插入直形连接头4内并通过螺纹连接,中间用垫片密封。
本实用新型提供的堵漏工具,其优点是,能在系统带压的情况下,消除测温连接点的泄漏,以避免物料的损失和减少环境污染。
附图说明:
附图是本实用新型的结构示意图
在附图中,1是无缝钢管,2是盲板,3是截止阀,4是直形连接头 ,5是设备管道,6是测温点。
具体实施方式:
下面结合附图对实用新型作进一步的说明。
一种测温连接点的堵漏工具,它是用一内径为50mm的无缝钢管1,其中一端用厚度为10mm的圆形盲板2闷死,在盲板中间开一直径为16mm的孔,将截止阀3在开孔处焊接。无缝钢管1的长度视测温点的长度确定,无缝钢管1的壁厚视系统压力确定,一般为3.5mm-6mm。盲板2与无缝钢管1采用焊接的方式,盲板2的边缘要打坡口,以增加焊接强度。截止阀3的接头插入盲板中间的开孔内并焊接牢固,截止阀3接头内应加垫片密封。
堵漏时,将堵漏工具套在直形连接头4的外部,堵漏工具顶端的截止阀3打开,将直形连接头3与堵漏工具连接处焊接,如果泄漏量较大时,可在直形连接头4周围涂一些密封胶以减少直形连接头与堵漏工具连接处的泄漏量,方便焊接,待焊接牢固后关闭堵漏工具顶端的截止阀。
Claims (1)
1.一种测温连接点的堵漏工具,其特征是:在测温连接点用无缝钢管(1)和一端厚度小于另一端厚度的圆形盲板(2)闷死,在盲板中间开一圆孔,将截止阀(3)在开孔处焊接,无缝钢管(1)的长度视测温点的长度确定,无缝钢管(1)的壁厚视系统压力确定,一般为3.5mm-6mm,盲板(2)与无缝钢管(1)采用焊接的方式,盲板(2)的连缘打成坡口,增加焊接强度,截止阀(3)的接头插入盲板中间的开孔内并焊接牢固,截止阀接头内加垫片密封,直形连接头(4)焊接在设备管道(5)上,测温点(6)插入直形连接头(4)内并通过螺纹连接,中间用垫片密封。