CN201514800U - 高压电机用单层聚酰亚胺薄膜双层云母带绕包铜扁线 - Google Patents
高压电机用单层聚酰亚胺薄膜双层云母带绕包铜扁线 Download PDFInfo
- Publication number
- CN201514800U CN201514800U CN2009200443150U CN200920044315U CN201514800U CN 201514800 U CN201514800 U CN 201514800U CN 2009200443150 U CN2009200443150 U CN 2009200443150U CN 200920044315 U CN200920044315 U CN 200920044315U CN 201514800 U CN201514800 U CN 201514800U
- Authority
- CN
- China
- Prior art keywords
- polyimide film
- layer
- mica tape
- double
- conductor
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型提供一种高压电机用单层聚酰亚胺薄膜双层云母带绕包铜扁线,包括导体(1),所述导体(1)外间隙地绕包有聚酰亚胺薄膜(2)和环氧聚酯薄膜粉云母带(3)。本实用新型使用聚酰亚胺薄膜、环氧聚酯薄膜粉云母带,可以提高绕包线的耐电压、耐电晕、抗拉强度等性能指标。
Description
技术领域
本实用新型涉及一种绕包铜扁线。
背景技术
漆包线是绕组线的一个主要品种,由导体和绝缘层两部组成,裸线经退火软化后,再经过多次涂漆,烘焙而成。但要生产出即符合标准要求,又满足客户要求的产品并不容易,它受原材料质量,工艺参数,生产设备,环境等因素影响,因此,各种漆包线的质量特性各不相同,但都具备机械性能,化学性能,电性能,热性能四大性能。
由于国内外电机制造水平发展的迅速,特别是国外高输出功率、尽量小巧的电机结构和生产过程的环保化,对于电机定子部件的绕包线提出了苛刻的技术要求:如要求绕包线具有耐电压、耐电晕、高强度和柔韧性好的性能。目前,还没有能够完全达到如上要求的绕包线。
发明内容
本实用新型的目的在于提供一种能够同时满足耐电压、耐电晕的绕包铜扁线。
本实用新型的目的是这样实现的:一种高压电机用单层聚酰亚胺薄膜双层云母带绕包铜扁线,包括导体,其特征在于:所述导体外间隙地绕包有聚酰亚胺薄膜和环氧聚酯薄膜粉云母带。
所述聚酰亚胺薄膜和环氧聚酯薄膜粉云母带绕包间隙范围为0.3~0.4mm。
所述导体为铜导体。
本实用新型的有益效果为:
1、本实用新型使用聚酰亚胺薄膜、环氧聚酯薄膜粉云母带,可以提高绕包线的耐电压、耐电晕、抗拉强度等性能指标;
2、本实用新型是一种耐电压、耐电晕、高强度和柔韧性好的绕包线,且结构简单、制造方便、性能可靠,可以广泛适用于高压电机;
3、本实用新型高压电机单层聚酰亚胺薄膜双层云母带绕包铜扁线能够耐电压击穿在14000~17000V,行业中同等厚度的绕包线的击穿电压值在6000~9000V,并具有极好的耐电晕性能,从而大大提升电机的使用寿命;
4、本实用新型的高压电机用单层聚酰亚胺薄膜双层云母带绕包铜扁线,通过对绕包线中间的导体使用挤-拉法进行拉制,使导体的尺寸达到高精度,由数字驱动编制的启动、停止程序、生产过程控制整个绕包过程,实现本实用新型的目的。
附图说明
图1为本实用新型产品的结构示意图。
具体实施方式
下面结合附图,对本实用新型技术方案进行详细说明,但是本实用新型的保护范围不局限于所述实施例。
实施例1
一种高压电机用单层聚酰亚胺薄膜双层云母带绕包铜扁线,包括导体1,所述导体1外间隙地绕包有聚酰亚胺薄膜2和环氧聚酯薄膜粉云母带3;所述聚酰亚胺薄膜2和环氧聚酯薄膜粉云母带3绕包间隙范围为0.3~0.4mm;所述导体1为铜导体。
在本实用新型中,所述导体1通过挤-拉法进行加工;导体1由Φ12.5mm的圆铜杆由挤压机经过挤压模具在500℃下一次挤压而成所要求尺寸的铜扁线;由于Φ12.5mm的圆铜杆进入挤压模具时呈现软态抗拉力很小,而挤压模具由高硬度的材质制成,不会由于模具磨损产生导体1尺寸精度波动的问题;这样可以保证经挤压模具压制导体尺寸的精度,保持导体1尺寸的波动控制在0.003~0.008mm的范围内,实现在导体1的尺寸高精度。
本实用新型中,对于绝缘材料的选择,为了使绕包线达到耐高电压,耐电晕和高的抗拉强度,本实用新型中的绝缘材料采用聚酰亚胺薄膜、环氧聚酯薄膜粉云母带。所述聚酰亚胺薄膜的成分苯四酸成分和40%摩尔-99%摩尔的对苯二胺成分与3%摩尔-78%摩尔的的构成单元成分形成的,具有良好的耐电压性能。
在所述环氧聚酯薄膜粉云母带3上通过粘合胶粘合覆有2层聚酯薄膜,可以提高绕包线的耐电压、耐电晕、抗拉强度等性能指标。
所述环氧聚酯薄膜粉云母带3的成分为粉云母,占云母带含量≥56%wt,所述粘合胶为环氧类粘合胶,占云母带含量的8~13%wt,所述聚酯薄膜为电工用PET薄膜,其厚度为0.017~0.023mm。
由于环氧聚酯薄膜粉云母带3的厚度和单位重量是标准规定的,而在规定标准范围变动云母带中的云母成分份,粘合胶成份和聚酯薄膜成份可以改变抗电压、抗电晕、抗拉强度等指标,可以满足不同用户的技术要求。
聚酰亚胺薄膜2、环氧聚酯薄膜粉云母带3的绕包铜扁线制造中的关键,为达到薄绝缘层和保持绕包线在电机线圈制造过程中弯曲后不损坏聚酰亚胺薄膜和环氧聚酯薄膜粉云母带,必须间隙绕包而为达到耐高电压,又不能浸渍绝缘漆,故绕包的间隙、层与层之间的搭叠都要做到25~33%。
本实用新型中,由高精度的数字驱动编制的启动和停止程序控制绕包头转速精度非常高,通过控制聚酰亚胺薄膜2、环氧聚酯薄膜粉云母带3盘在生产过程中控制绕包的张力精度,从而使聚酰亚胺薄膜2、环氧聚酯薄膜粉云母带3绕包的间隙31严格的控制在0.3~0.4mm之间;通过在设备中安装频闪显示仪,实时显示绕包过程中的层与层之间的搭叠力的实时情况,严格控制搭叠精度。
Claims (3)
1.一种高压电机用单层聚酰亚胺薄膜双层云母带绕包铜扁线,包括导体(1),其特征在于:所述导体(1)外间隙地绕包有聚酰亚胺薄膜(2)和环氧聚酯薄膜粉云母带(3)。
2.根据权利要求1所述的高压电机用单层聚酰亚胺薄膜双层云母带绕包铜扁线,其特征在于:所述聚酰亚胺薄膜(2)和环氧聚酯薄膜粉云母带(3)绕包间隙范围为0.3~0.4mm。
3.根据权利要求1或2所述的高压电机用单层聚酰亚胺薄膜双层云母带绕包铜扁线,其特征在于:所述导体(1)为铜导体。