CN201463500U - 珍珠岩玻化电炉生产装置 - Google Patents
珍珠岩玻化电炉生产装置 Download PDFInfo
- Publication number
- CN201463500U CN201463500U CN2009200859128U CN200920085912U CN201463500U CN 201463500 U CN201463500 U CN 201463500U CN 2009200859128 U CN2009200859128 U CN 2009200859128U CN 200920085912 U CN200920085912 U CN 200920085912U CN 201463500 U CN201463500 U CN 201463500U
- Authority
- CN
- China
- Prior art keywords
- perlite
- electric furnace
- vitreous
- cone
- vitrified
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种珍珠岩玻化电炉生产装置,它包括珍珠岩玻化电炉,用于支撑珍珠岩玻化电炉的立式支架,立式支架旁设置预热料提升机,提升机旁设预热炉,预热炉输出设预热料输送槽,珍珠岩玻化电炉顶部与提升机上端之间设上料斗,上料斗与珍珠岩玻化电炉顶部之间设有锥形均匀布料器,珍珠岩玻化电炉内的电热元件由螺旋杆紧固器固定在炉壁上。该电炉生产装置由于具有锥形均匀布料器能将黑曜岩、松脂岩、珍珠岩等火山石矿砂烧制成表面玻化内部空心不吸水球团,使全球储量最大的火山矿砂玻化成新型不进水保温材料,提高了保温效果,使珍珠岩矿产品保温材料应用领域更广泛。同时将电热元件如波带发热元件通过螺旋杆紧固器固定在炉壁上,有效解决了波带发热元件脱漏的问题。
Description
技术领域
本实用新型属于珍珠岩玻化珠加工设备,具体涉及一种珍珠岩玻化电炉生产装置。
背景技术
珍珠岩矿在我国和世界上是储量最大的火山石山脉,以前只能用来生产普通珍珠岩保温材料,由于吸水率高,保温效果差,应用范围有一定局限性。现有珍珠岩玻化电炉生产线中由于没有均料装置,加工的珍珠岩的膨胀不均,很难将矿砂烧制成表面玻化内部空心不吸水球团。而电炉中的电热元件如波带发热元件在使用一段时间后会脱落。
发明内容
本实用新型的目的在于提供一种珍珠岩玻化电炉生产装置,以解决上述问题。
本实用新型的技术方案为:珍珠岩玻化电炉生产装置,它包括珍珠岩玻化电炉,用于支撑珍珠岩玻化电炉的立式支架,立式支架旁设置预热料提升机,提升机旁设预热炉,预热炉输出设预热料输送槽,珍珠岩玻化电炉顶部与提升机上端之间设上料斗,上料斗与珍珠岩玻化电炉顶部之间设有锥形均匀布料器,珍珠岩玻化电炉内的电热元件由螺旋杆紧固器固定在炉壁上。
所述锥形均匀布料器包括支撑座,支撑坐上连接落料缸,落料缸上连接进料管,落料缸内设有均料板,均料板面上开设有均料落料孔,均料板下设有导料落料筒,导料落料筒下设有锥形布料体。
所述螺旋杆紧固器包括导杆一端设限位凸台,导杆一端是圆弧端头或锥形端头;导杆上设螺旋头,螺旋头的端面与导杆轴向具有80~90°的夹角。
该电炉生产装置由于具有锥形均匀布料器能将黑曜岩、松脂岩、珍珠岩等火山石矿砂烧制成表面玻化内部空心不吸水球团,使全球储量最大的火山矿砂玻化成新型不进水保温材料,提高了保温效果,使珍珠岩矿产品保温材料应用领域更广泛。同时将电热元件如波带发热元件通过螺旋杆紧固器固定在炉壁上,有效解决了波带发热元件脱漏的问题。
附图说明
图1珍珠岩玻化电炉生产装置示意图。
图2锥形均匀布料器结构示意图。
图3螺旋杆紧固器示意图。
具体实施方式
本实施例用于对本实用新型权利要求的解释,本实用新型的保护范围不限于下述结构的描述。
如图1所示,预热炉1输出设预热料输送槽2,预热料输送槽2的末端对着提升机3上的运料车14.提升机3设在立式支架4旁,可以与之连接.珍珠岩玻化电炉5设在立式支架4内,由立式支架4支撑固定,立式支架4下部设有工作平台6.珍珠岩玻化电炉包括炉体外壳,外壳内陶瓷纤维波浪叠压模块,组合炉膛,炉胆,波带发热元件,高铝螺旋杆紧固器,微电脑程序玻化工艺过程控温柜.其的炉膛尺寸为Φ650mm,炉胆为Φ480mm,炉体高度为Φ9000mm的典型结构.珍珠岩玻化电炉的结构不在此累述.珍珠岩玻化电炉5顶部与提升机3上端之间设上料斗7,上料斗7固定在立式支架4上部,上料斗7与珍珠岩玻化电炉5顶部之间设有锥形均匀布料器8.珍珠岩玻化电炉5的出料端15(落料斗的出口)与送料管9连接,送料管9一端与风机10连接,送料管9的另一端与料仓12连接.送料管10与料仓12之间的夹角为45~80°,本实施例中夹角为60°.风机10与送料管9之间形成风机套管负压吸料正压送料系统.它送料时间短,仅8-10秒,冷却快,玻化后空芯球团产品在输送料仓过程中不易破损.料仓12上设成品打包口11.
采用预热炉将矿砂游离水蒸发并预热到玻化前最佳结晶水进炉温度,使玻化工艺完整。
波带发热元件通过高铝螺旋杆紧固器固定在炉壁上;高铝的螺旋杆紧固器13如图3所示,包括导杆13.1一端设限位凸台13.2,导杆13.1一端是圆弧端头或锥形端头,本实施例为圆弧端头;导杆13.1上设螺旋头13.3,螺旋头13.3的端面与导杆轴向具有80~90°的夹角,本实施例中螺旋头13.3的端面与导杆轴向夹角为90°。高铝螺旋杆紧固器直径Φ20mm,长度210mm,材质高铝耐火材料或陶瓷,氧化铝材料,1400℃高温烧结成型。它能压紧发热元件穿过炉膛螺旋进入陶瓷纤维波浪叠块,使玻带电热元件不易松动脱出与炉胆短路。
如图2所示,锥形均匀布料器8包括支撑座8.1呈下端开口的桶形。支撑座8.1上连接落料缸8.2,落料缸8.2上连接进料管8.3,落料缸8.2内设有均料板8.4(本实施例中均料板8.4是支撑座8.1上顶板的一部分),均料板8.4面上开设有均料落料孔8.5(形成均布的多孔板),均料板8.5下设有导料落料筒8.6,导料落料筒8.6下设有锥形布料体8.7。锥形布料体8.7包括布料锥顶8.8,布料锥顶8.8下缘设置竖向导料筒8.9。锥形布料体8.7与调节吊杆8.10连接,调节吊杆8.10穿过落料缸8.1与落料缸连接,具体的调节吊杆8.10上设螺纹杆8.11,螺纹杆8.11连接调节螺母8.12。导料落料筒8.6的内壁呈倒锥形,落料筒下端口与锥形布料体的布料锥顶之间有间隙8.13,间隙8.13可通过调节吊杆8.10进行调节,调节吊杆8.10在落料缸内的部分上设有导向锥体8.14。锥形均匀布料器8使矿砂能通过多孔板分配,沿锥体均匀落料并沿炉胆内最佳加热间距均匀玻化一致。
Claims (10)
1.一种珍珠岩玻化电炉生产装置,它包括珍珠岩玻化电炉,用于支撑珍珠岩玻化电炉的立式支架,立式支架旁设置预热料提升机,提升机旁设预热炉,预热炉输出设预热料输送槽,珍珠岩玻化电炉顶部与提升机上端之间设上料斗,其特征在于上料斗与珍珠岩玻化电炉顶部之间设有锥形均匀布料器,珍珠岩玻化电炉内的电热元件由螺旋杆紧固器固定在炉壁上。
2.如权利要求1所述珍珠岩玻化电炉生产装置,其特征在于锥形均匀布料器包括支撑座,支撑坐上连接落料缸,落料缸上连接进料管,落料缸内设有均料板,均料板面上开设有均料落料孔,均料板下设有导料落料筒,导料落料筒下设有锥形布料体。
3.如权利要求2所述珍珠岩玻化电炉生产装置,其特征在于锥形布料体包括布料锥顶,布料锥顶下缘设置竖向导料筒。
4.如权利要求2或3所述珍珠岩玻化电炉生产装置,其特征在于锥形布料体与调节吊杆连接,调节吊杆穿过落料缸与落料缸连接。
5.如权利要求4所述珍珠岩玻化电炉生产装置,其特征在于调节吊杆上设螺纹杆,螺纹杆连接调节螺母。
6.如权利要求4所述珍珠岩玻化电炉生产装置,其特征在于调节吊杆在落料缸内的部分上设有导向锥体。
7.如权利要求2或3所述珍珠岩玻化电炉生产装置,其特征在于导料落料筒的内壁呈倒锥形,落料筒下端口与锥形布料体的布料锥顶之间有间隙。
8.如权利要求1所述珍珠岩玻化电炉生产装置,其特征在于螺旋杆紧固器包括导杆一端设限位凸台,导杆一端是圆弧端头或锥形端头;导杆上设螺旋头,螺旋头的端面与导杆轴向具有80~90°的夹角。
9.如权利要求1所述珍珠岩玻化电炉生产装置,其特征在于珍珠岩玻化电炉的出料端与送料管连接,送料管一端与风机连接,送料管的另一端与料仓连接。
10.如权利要求9所述珍珠岩玻化电炉生产装置,其特征在于送料管与料仓之间的夹角为45~80°。