CN201296772Y - 电极钢坯防氧化装置 - Google Patents
电极钢坯防氧化装置 Download PDFInfo
- Publication number
- CN201296772Y CN201296772Y CNU2008201065906U CN200820106590U CN201296772Y CN 201296772 Y CN201296772 Y CN 201296772Y CN U2008201065906 U CNU2008201065906 U CN U2008201065906U CN 200820106590 U CN200820106590 U CN 200820106590U CN 201296772 Y CN201296772 Y CN 201296772Y
- Authority
- CN
- China
- Prior art keywords
- argon
- cover
- hood
- argon gas
- steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
电极钢坯防氧化装置,它包括氩气罩,氩气罩为有顶盖和底盖的圆形筒,顶盖与底盖之间为空心的,氩气罩的内壁上固定设置输送氩气的管道,管道上等分设置8个通气孔,通气孔的直径是4毫米,通气孔的轴线与底盖盖面成30~50度角,氩气罩的底盖上设置通气孔,通气孔的轴线与底盖的盖面成30~50度角,氩气罩的顶盖上覆盖有石棉盖。将本实用新型罩在电渣炉的结晶器的上部,在冶炼过程中输入氩气,氩气通过氩气罩进入结晶器,氩气有效地隔绝电极坯与空气、熔渣与空气的接触,防止电极钢坯氧化,使钢中的氧含量明显降低,降低钢中的非金属夹杂物含量,从而提高了钢的纯净度,提高了产品质量。
Description
技术领域:
本实用新型属于冶金企业特种炉炼钢作业过程的辅助设施,具体涉及电极钢坯防氧化装置。
背景技术:
冶金企业炼钢作业过程中,当采用电炉钢作坯料或感应炉冶炼出的钢作坯料,经普通电渣炉电渣重熔,生产出的钢产品的纯净度较低,氧含量较高,且分布不均匀,产品质量难以保证。究其原因是电极钢坯在冶炼过程中,由于氧、氮含量较高,钢坯氧化造成产品质量下降。
发明内容:
本实用新型旨在提供能够降低电极钢坯氧、氮含量的电极钢坯防氧化装置。
实现本实用新型的技术方案是:包括氩气罩,氩气罩为有顶盖和底盖的圆形筒,顶盖与底盖之间为空心的,氩气罩的内壁上固定设置输送氩气的管道,管道上等分设置8个通气孔,通气孔的直径是4毫米,通气孔的轴线与底盖盖面成30~50度角,一般为45度角,氩气罩的底盖上设置通气孔,通气孔的轴线与底盖的盖面成30~50度角,一般为45度角,氩气罩的顶盖上覆盖有石棉盖。
将本实用新型罩在电渣炉的结晶器的上部,在冶炼过程中输入氩气,氩气通过氩气罩进入结晶器,氩气有效地隔绝电极坯与空气、熔渣与空气的接触,防止电极钢坯氧化,使钢中的氧含量明显降低,降低钢中的非金属夹杂物含量,从而提高了钢的纯净度,提高了产品质量。
附图说明:
图1是本实用新型实施例的主视图(轴向剖视)。
图2是图1的仰视图。
图中:1.氩气罩 2.石棉盖 3.管道 4.通气孔
5.通气孔 6.底盖 7.氩气管
具体实施方式:
实施例:图1、图2所示,本实施例包括氩气罩1,氩气罩1为有顶盖和底盖6的圆形筒,顶盖与底盖6之间为空心的,沿氩气罩1内壁的一周固定设置输送氩气的管道3,管道3上等分设置8个通气孔4,通气孔4的直径是4毫米,通气孔4的轴线与底盖6的盖面成45度角,底盖6上设置通气孔5,通气孔5的轴线与底盖6的盖面成45度角,氩气罩1的顶盖上覆盖有石棉盖2,石棉盖2为直径大于氩气罩1的直径的圆形石棉垫。
Claims (2)
1、电极钢坯防氧化装置,包括氩气罩,其特征是氩气罩为有顶盖和底盖的圆形筒,顶盖与底盖之间为空心的,氩气罩的内壁上固定设置输送氩气的管道,管道上等分设置8个通气孔,通气孔的直径是4毫米,通气孔的轴线与底盖盖面成30~50度角,氩气罩的底盖上设置通气孔,通气孔的轴线与底盖的盖面成30~50度角,氩气罩的顶盖上覆盖有石棉盖。
2、根据权利要求1所述的电极钢坯防氧化装置,其特征是所述的通气孔的轴线与底盖盖面成45度角。