CN201246534Y - Pc-pe耐高温防腐耐磨复合油管 - Google Patents
Pc-pe耐高温防腐耐磨复合油管 Download PDFInfo
- Publication number
- CN201246534Y CN201246534Y CNU2008201346596U CN200820134659U CN201246534Y CN 201246534 Y CN201246534 Y CN 201246534Y CN U2008201346596 U CNU2008201346596 U CN U2008201346596U CN 200820134659 U CN200820134659 U CN 200820134659U CN 201246534 Y CN201246534 Y CN 201246534Y
- Authority
- CN
- China
- Prior art keywords
- oil pipe
- pipe
- resistant
- wear
- oil
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种PC-PE耐高温防腐耐磨复合油管,适用于油田采油井、偏磨井、注水井和化工管道等。它是在钢制的油管内嵌有PC与PE共混材料制造的内衬管,内衬管采用过盈装配工艺嵌入油管内。内衬管具有记忆效应,可自动调适产生于油井温度变化和应力变化导致的油管伸缩变形,能始终保持内衬管涨紧抵靠在钢制油管的内表面,使内管不脱落、不剥离。本实用新型由于在钢制油管内嵌有PC-PE共混材料制造的内管,提高了使用温度,可在2500米以内、井温110℃以内的采油井使用,抗偏、耐磨、防腐蚀,不结垢、不结蜡,提高了油管的使用寿命,节约了石油开采成本。
Description
技术领域
本实用新型涉及一种在油田、化工、输送热水等领域使用的耐高温防腐耐磨复合油管,可以广泛地应用于采油井、偏磨采油井等。
背景技术
目前油田采用的防腐耐磨复合油管的内衬管,是用热塑性高密度聚乙烯材料制造的,仅使用在1200米以内、井温在80℃以内的浅油井使用。而内管的装配工艺采用过渡配合,内管与油管易脱离、剥离,导致井下事故的发生,造成修井作业。现有的防腐耐磨复合油管已经不适应高温、深井杆管偏磨的需求。
发明内容
本实用新型的目的,在于提供一种具有良好性能的PC—PE耐高温防腐耐磨复合油管。
本实用新型的目的是通过以下技术方案实现的。
一种PC—PE耐高温防腐耐磨复合油管,是在钢制油管内嵌有具耐高温、防腐蚀、防结蜡、耐磨性能的内衬管,该内衬管在油管的两端向外凸出,即在油管的两端采用内管凸出的结构。
内衬管的外径大于钢制油管的内径,内衬管过盈装配在钢制油管内。所述的过盈装配,是采用异径滚轮塑料管材轧压缩径装置嵌入到钢制油管内的。内衬管由PC—PE共混材料制造。内衬管具有记忆效应,可以自动适应由于油井温度变化和应力变化而导致的油管伸缩变形,并能始终保证内管紧紧地涨紧在钢制油管的内表面,使内管不脱落、不剥离。
本实用新型的优点在于:PC—PE共混材料制造的内管具有较好的耐高温、防腐、防结蜡、耐磨性能,可以在2500米以内、井温在110℃以内的采油井使用。衬管的内表面光滑、柔韧,降低了抽油杆的磨损,对油管和抽油杆都起到了良好的保护作用,提高了油管的使用寿命。旧油管嵌入内管也可以重新利用,降低了石油的开采成本,提高了工作效率。
附图说明
附图是本实用新型PC—PE耐高温防腐耐磨复合油管的结构示意图。
图中:1、钢制油管,2、PC—PE耐高温防腐耐磨内管。
具体实施方式
参见附图,在钢制油管1内,嵌有具耐高温、防腐蚀、防结蜡、耐磨性能的内衬管2;内衬管2的外径大于钢制油管1的内径。采用过盈装配工艺,用异径滚轮塑料管材轧压缩径装置,将内衬管2嵌入到钢制油管1内。内衬管2具有记忆效应,可自动适应由于油井温度变化而导致的油管的伸缩变形,并能始终保证内管紧贴、涨紧在钢制油管1的内表面,而使内管不脱落、不剥离。
具体制作时,首先用塑料挤出设备制造出PC—PE共混材料制成的内衬管2,内衬管2的外径大于钢制油管1的内径1.5—2mm;然后用异径滚轮塑料管材轧压缩径装置,将内衬管2过盈装配嵌入钢制油管1内;在油管1的两端做出凸出的结构。
Claims (4)
1.一种PC—PE耐高温防腐耐磨复合油管,其特征在于:是在钢制油管内嵌有具耐高温、防腐蚀、防结蜡、耐磨性能的内衬管,该内衬管在油管的两端向外凸出。
2.根据权利要求1所述的PC—PE耐高温防腐耐磨复合油管,其特征在于:所述内衬管的外径大于钢制油管的内径,内衬管过盈装配在钢制油管内。
3.根据权利要求1所述的PC—PE耐高温防腐耐磨复合油管,其特征在于:所述的内衬管由PC—PE共混材料制造。
4.根据权利要求2所述的PC—PE耐高温防腐耐磨复合油管,其特征在于:所述的过盈装配,是采用异径滚轮塑料管材轧压缩径装置嵌入到钢制油管内的。