CN201217882Y - 小口径梯形集成材 - Google Patents

小口径梯形集成材 Download PDF

Info

Publication number
CN201217882Y
CN201217882Y CNU200820126412XU CN200820126412U CN201217882Y CN 201217882 Y CN201217882 Y CN 201217882Y CN U200820126412X U CNU200820126412X U CN U200820126412XU CN 200820126412 U CN200820126412 U CN 200820126412U CN 201217882 Y CN201217882 Y CN 201217882Y
Authority
CN
China
Prior art keywords
small
trapezoidal
caliber
wood
timber
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CNU200820126412XU
Other languages
English (en)
Inventor
梶田靖夫
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Wenguo Furniture Industry Co Ltd
Original Assignee
Shanghai Wenguo Furniture Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Wenguo Furniture Industry Co Ltd filed Critical Shanghai Wenguo Furniture Industry Co Ltd
Priority to CNU200820126412XU priority Critical patent/CN201217882Y/zh
Application granted granted Critical
Publication of CN201217882Y publication Critical patent/CN201217882Y/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本实用新型公开了小口径梯形集成材,具有梯形断面的两层以上的小口径梯形板材通过工业胶热压在一起。本实用新型小口径梯形集成材各个小口径梯形板材通过工业胶热压在一起,梯形截面小段小口径锯解,不仅可以节约木材,充分利用小口径木材,而且集合热压在一起的集成材强度还比以前有所改善。采用锯切面为梯形的小口径锯解方法,出材率大大提高,一般可以达到90%左右,同时也缩短了只有大木材才能砍伐使用的市场规律,缩短了木材的砍伐周期,拓宽了小口径木材的应用领域,极大地提高了其经济和社会效益。

Description

小口径梯形集成材技术领域本实用新型涉及一种建筑材料的集成材,具体说是一种小口径梯形集成材。 背景技术现在用于集成材的木材,在其幼龄期常常砍伐,这些数量大、胸径小、强度差、体积不 稳定的低质材,过去用于作为细木板材的板芯,因为要按照小口径锯解,所以木材的利用率 很低, 一般在60%左右,浪费极大,甚至有些小木材都被弃置不用;本实用新型提供一种小口径梯形集成材,采用锯切面为梯形的小口径锯解方法,出材率大大提高, 一般可以达到90% 左右,同吋也縮短了只有大木材才能砍伐使用的市场规律,縮短了木材的砍伐周期,拓宽了 小口径木材的应用领域,极大地提高了其经济和社会效益。 实用新型内容本实用新型的所要解决的技术问题是针对现有技术不足之处,提供小口径梯形集成材, 解决现有技术集成材浪费木材,利用率不高,应用领域不广的缺陷。本实用新型解决其技术问题所采用的技术方案是:小口径梯形集成材,具有梯形断面的 两层以上的小口径梯形板材通过工业胶热压在一起。本实用新型的小口径梯形集成材和现有技术相比,具有以下有益效果-本实用新型小口径梯形集成材各个小口径梯形板材通过工业胶热压在一起,梯形截面小 段小口径锯解,不仅可以节约木材,充分利用小口径木材,而且集合热压在一起的集成材强 度还比以前有所改善。采用锯切面为梯形的小口径锯解方法,出材率大大提高, 一般可以达 到90%左右,同时也缩短了只有大木材才能砍伐使用的市场规律,縮短了木材的砍伐周期, 拓宽了小口径木材的应用领域,极大地提高了其经济和社会效益。 附图说明附图1为小口径梯形集成材的单独一层板材的结构示意图;附图2为小口径梯形集成材的若干层板材结合在一起的结构示意图;附图3、 4、 5为小口径梯形集成材的锯解结构示意图。图中:A、板材;B、集成材;1、梯形断面;2、小口径梯形集成材。具体实施方式接下来参照说明书附图对本实用新型的小口径梯形集成材作以下详细地说明。 本实用新型的小口径梯形集成材,具有梯形断面的两层以上的小口径梯形板材通过工业胶热压在一起。各个小口径梯形板材通过工业胶热压在一起,梯形截面小段小口径锯解,不仅可以节约 木材,充分利用小口径木材,而且集合热压在一起的集成材强度还比以前有所改善。

Claims (1)

1、小口径梯形集成材,其特征在于:具有梯形断面的两层以上的小口径梯形板材通过工业胶热压在一起。
CNU200820126412XU 2008-06-27 2008-06-27 小口径梯形集成材 Expired - Lifetime CN201217882Y (zh)