CN201211695Y - Solid-wood composite board - Google Patents
Solid-wood composite board Download PDFInfo
- Publication number
- CN201211695Y CN201211695Y CNU2008200530883U CN200820053088U CN201211695Y CN 201211695 Y CN201211695 Y CN 201211695Y CN U2008200530883 U CNU2008200530883 U CN U2008200530883U CN 200820053088 U CN200820053088 U CN 200820053088U CN 201211695 Y CN201211695 Y CN 201211695Y
- Authority
- CN
- China
- Prior art keywords
- solid
- board
- solid wood
- composite board
- core
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses a solid batten composite board and aims at overcoming the defects that the prior core-board has low intensity, weak shearing resistance, more lumbers discarded during the processing, low utilization ratio of lumbers, high cost, and the like. Solid battens discarded during the core-board processing are used to be made into the solid batten composite board with two layers of panels and a middle layer of gusset. The utility model takes the solid battens discarded during the core-board processing as raw materials to be processed to be the composite board needed for decorating houses, and the solid batten composite board has high intensity, strong shearing resistance and low cost.
Description
Technical field
The utility model relates to a kind of composite plate with timber processing, is specially a kind of solid wood bar composite plate.
Background technology
Existing core-board with timber processing is a three-decker, and the gusset in middle level is thick 1.4cm solid wood plate, plays the skeleton stabilization, and other two-layer panels are the wooden skin of thickness 1-1.2mm of stripping down from log.The core-board and the process thereof of veneer decoration gained have following weak point like this, and the one, intensity is little, and shearing resistance is little; The 2nd, its process has produced a large amount of little solid wood bars, and is not enough to the utilization rate of timber, and waste is big, the cost height of production board.
The utility model content
The purpose of this utility model will overcome above-mentioned deficiency exactly, provides a kind of little solid wood bar that abandons in the existing procedure for processing lumber-core board that can utilize to be processed into the intensity height, and shearing resistance is strong, solid wood bar composite plate with low cost.
For achieving the above object, the technical solution of the utility model is, this solid wood bar composite plate comprises two deck panels and be sandwiched in therebetween gusset that described panel and gusset are pieced together system by the solid wood bar and formed.Described panel is not to be the wooden skin of 1-1.2mm with existing thickness, but thickness is greater than the solid wood bar of 1-1.2mm; Described gusset is not to be 1.4cm solid wood plate with existing thickness, but is the solid wood bar of thickness greater than 1.5mm, and these materials all can obtain from the waste material of existing core-board processing.
Described solid wood bar is for 10cm is long at least, 1cm is wide, 1.5mm is thick.
As further improvement of the utility model, described solid wood bar is long 20-60cm, wide 2-6cm, thick 2.5-6mm.
Compare with existing similar technical products, gusset of the present utility model and panel have utilized the little solid wood bar that abandons in the existing procedure for processing lumber-core board, not only turn waste into wealth, and have improved the utilization rate of timber, reduced the cost of raw material, add that glue consumption has reduced 50%, the finished product market price is high by 5%, and only pipe processing wage has increased by 2/3, but integrated cost has descended 6%, and the production board intensity height that is processed into, shearing resistance is strong, and integrated quality is good.
Description of drawings
This accompanying drawing is the utility model cross section structure schematic diagram.
Among the figure, 1. gusset, 2. panel.
The specific embodiment
As shown in the figure, the utility model solid wood bar composite plate comprises with the solid wood bar and pieces together two deck panels [2] of system and be sandwiched in therebetween gusset [1], gusset [1] and the used solid wood bar of panel [2] are at least long 10cm, wide 1cm, thick 1.5mm, generally select for use long 20-60cm, wide 2-6cm, thick 2.5-6mm for well from the waste material of existing core-board processing.
Claims (3)
1, a kind of solid wood bar composite plate comprises two deck panels [2] and is sandwiched in therebetween gusset [1], it is characterized in that, described panel [2] and gusset [1] are pieced together system by the solid wood bar and formed.
2, solid wood bar composite plate according to claim 1 is characterized in that, described solid wood bar is for 10cm is long at least, 1cm is wide, 1.5mm is thick.
3, solid wood bar composite plate according to claim 2 is characterized in that, described solid wood bar is long 20-60cm, wide 2-6cm, thick 2.5-6mm.