CN201128094Y - Dry method edge grinding machine for pottery brick - Google Patents
Dry method edge grinding machine for pottery brick Download PDFInfo
- Publication number
- CN201128094Y CN201128094Y CNU2007201789636U CN200720178963U CN201128094Y CN 201128094 Y CN201128094 Y CN 201128094Y CN U2007201789636 U CNU2007201789636 U CN U2007201789636U CN 200720178963 U CN200720178963 U CN 200720178963U CN 201128094 Y CN201128094 Y CN 201128094Y
- Authority
- CN
- China
- Prior art keywords
- dry method
- method edge
- facing attachment
- ceramic brick
- grinding machine
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses a ceramic brick dry-method edge grinding machine, which comprises a beam. An adobe gearing is arranged on the beam, and the left and the right sides of the beam are provided with a kibbling mechanism, a thick chamfer angle device, a refining mill and a refining chamfer angle device in sequence along the feed direction of adobe gearing. Through the product manufactured by the ceramic brick dry-method edge grinding machine, not only the collapse glaze generated when grinding can be completely trimmed, but also the productivity effect is high, thereby being widely applied to the manufacture of the ceramic brick dry-method edge grinding machine.
Description
Technical field
The utility model relates to a kind of machined machinery that is used for the finishing of ceramic brick edge polisher, the grinding of brick chamfering, particularly a kind of ceramic brick dry method edge polisher.
Background technology
The ceramic brick dry method edge polisher of technology comprises the edge polisher main body that is provided with adobe transmission system, beam device, facing attachment and some bistriques now, and described bistrique, facing attachment set gradually by the adobe direction of feed.Beam device is used to support parts such as bistrique and chamfering, and adobe enters grinding area under the effect of transmission system, finish once complete process by bistrique, facing attachment.Existing dry method edging technology generally adopts the angle that is produced when roughly grinding after grinding and the correct grinding finishing again to peripheral grinding to green brick edge to carry out grinding dressing and is commonly called as chamfering.Collapse glaze owing to the green brick edge grinding time, produce, and the amount of chamfering so can't all trim collapsing glaze, causes product quality to descend usually about 0.2mm.
Summary of the invention
In order to overcome the deficiencies in the prior art, the ceramic brick dry method edge polisher that provides a kind of quality of production good is provided the purpose of this utility model.
The technical scheme that its technical problem that solves the utility model adopts is:
A kind of ceramic brick dry method edge polisher, it comprises crossbeam, and crossbeam is provided with the adobe transmission device, and the left and right sides of described crossbeam is disposed with corase grind mechanism, thick facing attachment, correct grinding mechanism, smart facing attachment along the direction of feed of adobe transmission device;
As a modification of the embodiment above, described corase grind mechanism and correct grinding mechanism are made up of the driven by motor emery wheel;
As the further improvement to above-mentioned embodiment, described thick facing attachment and smart facing attachment are to be the air pressure floating installation that 30~60 degree are provided with.
The beneficial effects of the utility model are: this product increases by one group of thick facing attachment between corase grind mechanism and correct grinding mechanism, when this product carries out grinding to green brick edge, thick facing attachment can carry out chamfering about 1mm to adobe, and the glaze that collapses that makes corase grind cut generation is all handled, and then 30~60 degree chamfering refine grindings about the 1mm that thick facing attachment is produced by some groups of correct grinding mechanisms are intact, carry out the refine chamfering by smart facing attachment again, the product of making by the utility model, produce during not only with grinding and collapse glaze and all trim, and the production efficiency height, thereby be widely used in the making of ceramic brick dry method edge polisher.
Description of drawings
The utility model is described in further detail below in conjunction with drawings and Examples.
Fig. 1 is a structural representation of the present utility model.
The specific embodiment
With reference to Fig. 1, a kind of ceramic brick dry method edge polisher, it comprises crossbeam 1, and crossbeam 1 is provided with adobe transmission device 2, and the left and right sides of described crossbeam 1 is disposed with corase grind mechanism 3, thick facing attachment 4, correct grinding mechanism 5, smart facing attachment 6 along the direction of feed of adobe transmission device 2; Described corase grind mechanism 3 and correct grinding mechanism 5 drive emery wheel 72 by motor 71 and form; Described thick facing attachment 4 and smart facing attachment 6 are for being the air pressure floating installation of 30~60 ° of settings.
The corase grind mechanism 3 of this product is made up of four groups of rough grinding wheels; and correct grinding mechanism 5 is made up of three groups of finishing wheels; actual needs are installed certainly; also can use the emery wheels more than two groups or five groups to combine; so as long as it reaches technique effect of the present utility model with essentially identical means, all should belong to protection domain of the present utility model in a word.
This product increases by one group of thick facing attachment 4 between corase grind mechanism 3 and correct grinding mechanism 5, when this product carries out grinding to green brick edge, thick facing attachment 4 can carry out chamfering about 1mm to adobe, and the glaze that collapses that makes corase grind cut generation is all handled, and then 30~60 degree chamfering refine grindings about the 1mm that thick facing attachments 4 is produced by some groups of correct grinding mechanisms 5 are intact, carry out the refine chamfering by smart facing attachment 6 again, the product of making by the utility model, produce during not only with grinding and collapse glaze and all trim, and the production efficiency height, thereby be widely used in the making of ceramic brick dry method edge polisher.
Claims (3)
1. ceramic brick dry method edge polisher, it is characterized in that: comprise crossbeam (1), crossbeam (1) is provided with adobe transmission device (2), and the left and right sides of described crossbeam (1) is disposed with corase grind mechanism (3), thick facing attachment (4), correct grinding mechanism (5), smart facing attachment (6) along the direction of feed of adobe transmission device (2).
2. a kind of ceramic brick dry method edge polisher according to claim 1 is characterized in that: described corase grind mechanism (3) and correct grinding mechanism (5) drive emery wheel (72) by motor (71) and form.
3. a kind of ceramic brick dry method edge polisher according to claim 1 is characterized in that: described thick facing attachment (4) and smart facing attachment (6) are for being the air pressure floating installation that 30~60 degree are provided with.