CN201042739Y - 连铸中间包手动快换滑动水口 - Google Patents

连铸中间包手动快换滑动水口 Download PDF

Info

Publication number
CN201042739Y
CN201042739Y CNU2007200205346U CN200720020534U CN201042739Y CN 201042739 Y CN201042739 Y CN 201042739Y CN U2007200205346 U CNU2007200205346 U CN U2007200205346U CN 200720020534 U CN200720020534 U CN 200720020534U CN 201042739 Y CN201042739 Y CN 201042739Y
Authority
CN
China
Prior art keywords
slide gate
brick
continuous casting
stirrup
nozzle brick
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU2007200205346U
Other languages
English (en)
Inventor
郁善会
杨丙礼
孙甲玉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZIBO XINNAIDA REFRACTORY MATERIAL CO Ltd
Original Assignee
ZIBO XINNAIDA REFRACTORY MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZIBO XINNAIDA REFRACTORY MATERIAL CO Ltd filed Critical ZIBO XINNAIDA REFRACTORY MATERIAL CO Ltd
Priority to CNU2007200205346U priority Critical patent/CN201042739Y/zh
Application granted granted Critical
Publication of CN201042739Y publication Critical patent/CN201042739Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种连铸中间包手动快换滑动水口,使用在炼钢厂连铸中间包上,有水口砖主体,其特征在于水口砖内孔镶嵌有氧化锆内衬;水口砖外壁设有钢箍。氧化锆内衬直接接触高温流体,抗侵蚀性好,使用寿命长,水口砖外壁的钢箍显著提高了水口砖的整体强度,避免了水口砖炸裂,安全可靠,保证了正常生产。

Description

连铸中间包手动快换滑动水口
技术领域
本实用新型涉及一种改进的连铸中间包手动快换滑动水口,使用在炼钢厂连铸中间包上。
背景技术
随着钢铁冶炼与连铸水平的不断提高,高效连铸发展迅猛,快换水口解决了目前小方坯多炉连浇的难题,实现了中包寿命与水口寿命同步。目前国内小方坯连铸有很大比例采用的是定径水口浇铸,定径水口的使用寿命要低于中间包的包衬寿命,于是出现了用定径水口快速更换装置,来解决这个问题,使用相互匹配的上、下滑动水口,使用过程中,主要用于更换下水口,当下水口经使用扩径后,在不断流的情况下更换至另一个待用下水口,完成水口的快换操作。自然,水口的结构、质量直接影响着水口的使用寿命,现有的水口抗侵蚀性差,容易脱落,使用寿命短,而且整体强度弱,易发生炸裂事故,影响正常生产。
实用新型内容
本实用新型的目的在于提供一种改进的连铸中间包手动快换滑动水口,抗侵蚀性好,使用寿命长,而且整体强度大,避免炸裂,安全可靠,保证正常生产。
本实用新型所述的连铸中间包手动快换滑动水口,有水口砖主体,其水口砖内孔镶嵌有氧化锆内衬。
氧化锆内衬(也称锆芯)热震稳定性好,抗侵蚀、耐冲刷,氧化锆内衬与高温流体接触,可大大延长水口砖的使用寿命。氧化锆内衬设计为整体结构,提高整体强度,可单独成型制作,然后整体嵌装在水口砖内孔中。
在水口砖外壁设钢箍,增加水口砖的整体强度,避免炸裂。水口砖与钢箍成型在一起,构成整体结构,增强整体性。将钢箍的内壁设凹槽,使钢箍和水口砖之间相互嵌入,增强整体强度。
水口有上水口和下水口,两者配合使用,两者之间有配合的平面。上水口有上水口砖,上水口砖内孔镶嵌有氧化锆内衬,上水口砖外壁设钢箍;下水口有下水口砖,下水口砖内孔镶嵌有氧化锆内衬,下水口砖外壁设钢箍。
本实用新型连铸中间包手动快换滑动水口,在水口砖内孔镶嵌氧化锆内衬,由氧化锆内衬直接接触高温流体,抗侵蚀性好,使用寿命长,水口砖外壁的钢箍显著提高了水口砖的整体强度,避免了水口砖炸裂,安全可靠,保证了正常生产。
附图说明
图1、本实用新型上水口结构示意图。
图2、本实用新型下水口结构示意图。
图3、本实用新型中的钢箍结构示意图。
图中:1、上水口砖  2、氧化锆内衬  3、粘结层  4、钢箍  5、下水口砖  6、氧化锆内衬  7、粘结层  8、钢箍  9、凹槽。
具体实施方式
下面结合实施例附图对本实用新型作进一步说明。
如图1所示,本实用新型所述的连铸中间包手动快换滑动水口,为上水口,上水口砖1内孔镶嵌有氧化锆内衬2,氧化锆内衬2为整体结构,由粘结层3与上水口砖1粘结,上水口砖1外壁设有钢箍4,钢箍4的内壁上设有凹槽,上水口砖1与钢箍4成型在一起构成整体结构。
如图2所示,本实用新型所述的连铸中间包手动快换滑动水口,为下水口,下水口砖5内孔镶嵌有氧化锆内衬6,氧化锆内衬6为整体结构,由粘结层7与下水口砖5粘结,下水口砖5外壁设有钢箍8,钢箍8的内壁上设有凹槽9,下水口砖5与钢箍8成型在一起构成整体结构。
上水口砖和下水口砖上的钢箍可以相同,也可以不同。
使用时,上下水口配合使用。

Claims (5)

1.一种连铸中间包手动快换滑动水口,有水口砖主体,其特征在于水口砖内孔镶嵌有氧化锆内衬。
2.根据权利要求1所述的连铸中间包手动快换滑动水口,其特征在于氧化锆内衬为整体结构。
3.根据权利要求1或2所述的连铸中间包手动快换滑动水口,其特征在于水口砖外壁设有钢箍。
4.根据权利要求3所述的连铸中间包手动快换滑动水口,其特征在于水口砖与钢箍为成型在一起的整体结构。
5.根据权利要求4所述的连铸中间包手动快换滑动水口,其特征在于钢箍的内壁上设有凹槽。
CNU2007200205346U 2007-04-07 2007-04-07 连铸中间包手动快换滑动水口 Expired - Fee Related CN201042739Y (zh)