CN1954962A - 螺纹钢筋锚杆柱头螺栓冷镦挤成型方法 - Google Patents
螺纹钢筋锚杆柱头螺栓冷镦挤成型方法 Download PDFInfo
- Publication number
- CN1954962A CN1954962A CN 200510100482 CN200510100482A CN1954962A CN 1954962 A CN1954962 A CN 1954962A CN 200510100482 CN200510100482 CN 200510100482 CN 200510100482 A CN200510100482 A CN 200510100482A CN 1954962 A CN1954962 A CN 1954962A
- Authority
- CN
- China
- Prior art keywords
- upsetting squeeze
- roofbolt
- reinforcing bar
- shaping method
- twisted steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种螺纹钢筋锚杆柱头螺栓冷镦挤成型方法,它包括如下步骤:将螺纹钢筋根据技术要求按锚杆尺寸用树脂砂轮切割机下料,下料后的尺寸规格,按照实际镦挤模套匹配;将钢筋工件用手工输入镦挤模套内;启动液压机,按照需要的技术参数将钢筋工件镦挤成型;镦挤成型的螺纹钢筋锚杆柱头,直接用滚丝机进行套丝等,采用以上方法的工艺螺纹的最小底径均大于母材的截面面积,经冷挤压后,大大的提高了材料的强度,本方法生产的锚杆柱头螺栓,强度高,使用中不容易折断,成本低廉,提高了工程质量,加快了工程进度,节省了能源。
Description
技术领域
本发明涉及一种螺纹钢筋锚杆柱头螺栓冷镦挤成型方法。
背景技术
钢筋螺纹锚杆是矿井、涵洞、隧道等地下施工、工程、支护必备之工艺工装,由于目前公知的技术为采用车削工艺,在车床上将工件经过车削、套丝、热处理等工序成型,这种方式工艺落后,设备陈旧,在实际生产中由于产品强度不够,经常造成锚杆头从钢筋螺纹与柱头螺栓根部折断的现象,对工程质量、工程进度造成影响,同时也是对资源造成莫大的浪费。
发明创造的内容
本发明的目的即在于针对上述不足,提供一种螺纹钢筋锚杆柱头螺栓冷镦挤成型方法,应用本方法生产的锚杆柱头螺栓,强度高,使用中不容易折断,提高了工程质量,加快了工程进度,节省了能源。
本发明的技术方案如下所述:
一种螺纹钢筋锚杆柱头螺栓冷镦挤成型方法,包括如下步骤:
1)、将螺纹钢筋根据技术要求按锚杆尺寸用树脂砂轮切割机下料,下料后的尺寸规格,按照实际镦挤模套匹配;
2)、将钢筋工件用手工输入镦挤模套内;
3)、启动液压机,按照需要的技术参数将钢筋工件镦挤成型;
4)、镦挤成型的螺纹钢筋锚杆柱头,直接用滚丝机进行套丝,滚压柱头螺检;
5)、将滚压好柱头螺栓输出备用。
根据以上工艺步骤的本发明,其有益效果在于,采用以上方法的工艺螺纹的最小底径均大于母材的截面面积,经冷挤压后,大大的提高了材料的强度,即可以将直径细的螺纹钢筋锚杆柱头,镦挤成粗的螺纹钢筋锚杆柱头,本方法生产的锚杆柱头螺栓,强度高,使用中不容易折断,成本低廉,提高了工程质量,加快了工程进度,节省了能源。
实施方式
下面结合实施例对本发明详细加以说明:
一种螺纹钢筋锚杆柱头螺栓冷镦挤成型方法,包括如下步骤:
1)、将螺纹钢筋根据技术要求按锚杆尺寸用树脂砂轮切割机下料,下料后的尺寸规格,按照实际镦挤模套匹配;
2)、将钢筋工件用手工输入镦挤模套内;
3)、启动液压机,按照需要的技术参数将钢筋工件镦挤成型;
4)、镦挤成型的螺纹钢筋锚杆柱头,直接用滚丝机进行套丝,滚压柱头螺栓;
5)、将滚压好柱头螺栓输出备用。
Claims (5)
- 一种螺纹钢筋锚杆柱头螺栓冷镦挤成型方法,其特征在于,包括如下步骤:1)、将螺纹钢筋根据技术要求按锚杆尺寸用树脂砂轮切割机下料,下料后的尺寸规格,按照实际镦挤模套匹配;
- 2)、将钢筋工件用手工输入镦挤模套内;
- 3)、启动液压机,按照需要的技术参数将钢筋工件镦挤成型;
- 4)、镦挤成型的螺纹钢筋锚杆柱头,直接用滚丝机进行套丝,滚压柱头螺栓;
- 5)、将滚压好柱头螺栓输出备用。