Embodiment
For further disclosing technical scheme of the present invention, existing combination is implemented to be described in further detail:
Embodiment 1: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the technical hydrochloric acid (volume percent) of discarded slurry volume 1.5% (31% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the chlorinated lime (weight/volume percent) that adds discarded slurry volume 0.2% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in poly water glass (weight/volume percent) the absorption discarded slurry of discarded slurry volume 2% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 2: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the industrial sulphuric acid (volume percent) of discarded slurry volume 0.8% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the hydrogen peroxide (volume percent) that adds discarded slurry volume 0.1% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in Tai-Ace S 150 (weight/volume percent) the absorption discarded slurry of discarded slurry volume 0.5% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 3: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 1.3% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 0.2% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in alum (weight/volume percent) the absorption discarded slurry of discarded slurry volume 0.5% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 4: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 0.7% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the chlorinated lime (weight/volume percent) that adds discarded slurry volume 0.2% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in gypsum (weight/volume percent) the absorption discarded slurry of discarded slurry volume 2% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 5: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 0.5% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the chlorinated lime (weight/volume percent) that adds discarded slurry volume 0.2% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in magnesium oxide (weight/volume percent) the absorption discarded slurry of discarded slurry volume 2% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 6: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the technical hydrochloric acid (volume percent) of discarded slurry volume 12% (31% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the chlorinated lime (weight/volume percent) that adds discarded slurry volume 1% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in poly water glass (weight/volume percent) the absorption discarded slurry of discarded slurry volume 11% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 7: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the industrial sulphuric acid (volume percent) of discarded slurry volume 5% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the hydrogen peroxide (volume percent) that adds discarded slurry volume 1% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in poly water glass (weight percent) the absorption discarded slurry of discarded slurry volume 2% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 8: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 2.5% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 2.5% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in alum (weight/volume percent) the absorption discarded slurry of discarded slurry volume 12% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 9: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 2.5% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 2.5% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in gypsum (weight/volume percent) the absorption discarded slurry of discarded slurry volume 45% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 10: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 2.5% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 2.5% in stirring are removed or are reduced organic content in the discarded slurry, reduce COD
CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in magnesium oxide (weight/volume percent) the absorption discarded slurry of discarded slurry volume 15% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 11: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add technical hydrochloric acid and the sodium hydroxide in the discarded slurry and the yellow soda ash of the industrial sulphuric acid (volume percent), 0.5% (31% concentration) of discarded slurry volume 5% (98% concentration), the metal ion in the complexing mud;
B, the chlorinated lime (weight/volume percent) that adds discarded slurry volume 0.2% in stirring, 1% clorox (weight/volume percent) is removed or reduce organic content in the discarded slurry, reduces COD
CrAnd colourity, remove the sulfide in the mud;
C, the alum (weight/volume percent) that adds discarded slurry volume 2% in stirring, the moisture content in 30% gypsum (weight/volume percent) the absorption discarded slurry, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent, form powdery or blocks of solid to exosmosis.
Embodiment 12: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in industrial ethanedioic acid (weight/volume percent), 0.8% (31% concentration) technical hydrochloric acid of discarded slurry volume 2% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 1% in stirring, 0.8% chlorinated lime (weight/volume percent) is removed or reduce organic content in the discarded slurry, reduces COD
CrAnd colourity, remove the sulfide in the mud;
C, the Tai-Ace S 150 (weight/volume percent) that adds discarded slurry volume 5% in stirring, the moisture content in 8% magnesium oxide (weight/volume percent) the absorption discarded slurry, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent to exosmosis, form powdery or blocks of solid.
Embodiment 13: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in suction pit, stir to add in the industrial sulphuric acid of industrial ethanedioic acid (weight/volume percent), 0.6% (98% concentration) of discarded slurry volume 1% (98% concentration) and sodium hydroxide and yellow soda ash in the discarded slurry, the metal ion in the complexing mud;
B, the hydrogen peroxide (volume percent) that adds discarded slurry volume 0.5% in stirring, 0.8% chlorinated lime (weight percent) is removed or reduce organic content in the discarded slurry, reduces COD
CrAnd colourity, remove the sulfide in the mud;
C, the Tai-Ace S 150 (weight/volume percent) that adds discarded slurry volume 6% in stirring, the moisture content in 6% poly water glass (weight/volume percent) the absorption discarded slurry, destroy the emulsion balance of discarded slurry, change mud property, stop pollutent to exosmosis, form powdery or blocks of solid.