CN100418647C - Method for treating waste mud of drilling well by harmless process - Google Patents

Method for treating waste mud of drilling well by harmless process Download PDF

Info

Publication number
CN100418647C
CN100418647C CNB2006100220083A CN200610022008A CN100418647C CN 100418647 C CN100418647 C CN 100418647C CN B2006100220083 A CNB2006100220083 A CN B2006100220083A CN 200610022008 A CN200610022008 A CN 200610022008A CN 100418647 C CN100418647 C CN 100418647C
Authority
CN
China
Prior art keywords
mud
discarded slurry
volume
weight
addition
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CNB2006100220083A
Other languages
Chinese (zh)
Other versions
CN1944280A (en
Inventor
廖中健
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NANCHONG ZHENGDA INSTITUTE OF CHEMICAL ENGINEERING
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB2006100220083A priority Critical patent/CN100418647C/en
Publication of CN1944280A publication Critical patent/CN1944280A/en
Application granted granted Critical
Publication of CN100418647C publication Critical patent/CN100418647C/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The innocent treating process of waste drilling mud includes the following steps: 1. adding industrial hydrochloric acid, sulfuric acid and/or oxalic acid into waste drilling mud through stirring in a mud pit to neutralize sodium hydroxide and sodium carbonate and complex metal ion; 2. adding oxidant bleaching powder, hydrogen peroxide and/or sodium hypochlorite through stirring to eliminate or reduce organic matter content, lower CODCr and chroma and eliminate sulfide; and 3. adding adsorbent polysodium silicate, aluminum sulfate, gypsum powder and/or magnesia through stirring to adsorb water, destroy emulsion balance of mud, alter mud performance, block outward penetration of pollutant and form solid. The present invention has relatively low treatment cost.

Description

A kind for the treatment of waste mud of drilling well by harmless process
Technical field
The present invention relates to a kind of processing method of drilling well discarded slurry, relate in particular to a kind for the treatment of waste mud of drilling well by harmless process.
Background technology
The drilling well discarded slurry is a kind of discarded object of industrial gas oil exploitation, usually be to retain in for a long time in the mud pit of drilling well field or buried in underground through the general back of handling, these methods are not owing to do harmless treatment, need take a large amount of soils, the severe contamination atmosphere, soil, groundwater resources cause the huge wasting of resources.Though some domestic after eighties oil gas fields adopt cement-based solidified method, lime base curing, the organic polymer curing is handled discarded slurry, but still has following problem:
1, in the acid of acid of no use or capacity and NaOH in the discarded slurry and sodium carbonate, make the leachate pH value of solidfied material be strong basicity, and As time goes on NaOH and sodium carbonate do not degrade, and the alkaline pollution source are embedded in the mud pit in well site for a long time or buried in underground;
2, the organic matter in the discarded slurry, sulfide is thoroughly handled, and makes the chemical oxygen demand cod of leachate CrVery high, sometimes up to more than the 500mg/L, and it is dark especially to leach color, is brown or yellow green, and extension rate is hundreds of times, and also there is potential safety hazard in a large amount of leachings of sulfide simultaneously;
Though 3 some seal up for safekeeping, As time goes on, after confining bed destroyed, environmental pollution existed in the same old way;
4, disposal cost is higher, makes the easier selection of operator adopt simple natural air drying, simply buries mode, causes more serious environmental pollution.
Summary of the invention
The objective of the invention is to for not enough a kind for the treatment of waste mud of drilling well by harmless process, solution disposal cost height, the environmental pollution problems of providing of prior art is provided.
Method of the present invention realizes by following steps:
A, in mud pit, stir to add in hydrochloric acid or sulfuric acid or the oxalic acid at least a industrial acids and NaOH in the discarded slurry and sodium carbonate, the metal ion in the complexing mud;
B, add at least a oxidant in bleaching powder or hydrogen peroxide or the clorox in stirring and remove or reduce content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
Add the moisture content at least a adsorbents adsorb discarded slurry in poly sodium metasilicate or aluminum sulfate or alum or land plaster or the magnesia in C, the stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
The addition of said 31% technical hydrochloric acid is that the addition of 0.5~12%, 98% industrial sulphuric acid of percent by volume is that the addition of 0.5~8%, 98% industrial ethanedioic acid of percent by volume is 0.3~2.5% of a weight/volume percent.
The addition of said bleaching powder is 0.2~1% of a weight/volume percent, and the addition of hydrogen peroxide is 0.1~1% of a percent by volume, and the addition of clorox is 0.2~2.5% of a weight/volume percent.
The addition of said aluminum sulfate is 0.5~15% of a weight/volume percent, the addition of poly sodium metasilicate is 2~11% of a weight/volume percent, the addition of alum is 0.5~12% of a weight/volume percent, the addition of gypsum is 2~45% of a weight/volume percent, and magnesian addition is 2~15% of a weight/volume percent.
A kind for the treatment of waste mud of drilling well by harmless process of the present invention, according to the feature of discarded slurry own, adopt chemically treated method, with lower expense the harmful substance in the mud is handled one by one, made the leachate (by the preparation of GB5086 regulation) of drilling well discarded slurry solidfied material reach the GB8978-1996 integrated wastewater discharge standard.Discarded object after the processing is equivalent to the Chemical Physics performance of pan soil after a period of time.One deck planting soil is covered on the surface, or discarded object mixes by a certain percentage with planting soil, can satisfy the requirement of plant growth fully.Reached solution discarded slurry disposal cost height fully, the goal of the invention of problem of environmental pollution.The field trial result of use is as follows:
Well location Lotus flower 1-1 Mound Xi16Jing Chi63Jing
The mud that uses during drilling well Polymer is water base Poly-sulphur mud Polymer is water base
Testing result after the processing Up to standard Up to standard Up to standard
The specific embodiment
For further disclosing technical scheme of the present invention, existing combination is implemented to be described in further detail:
Embodiment 1: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the technical hydrochloric acid (percent by volume) of discarded slurry volume 1.5% (31% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the bleaching powder (weight/volume percent) that adds discarded slurry volume 0.2% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in poly sodium metasilicate (weight/volume percent) the absorption discarded slurry of discarded slurry volume 2% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 2: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the industrial sulphuric acid (percent by volume) of discarded slurry volume 0.8% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the hydrogen peroxide (percent by volume) that adds discarded slurry volume 0.1% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in aluminum sulfate (weight/volume percent) the absorption discarded slurry of discarded slurry volume 0.5% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 3: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 1.3% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 0.2% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in alum (weight/volume percent) the absorption discarded slurry of discarded slurry volume 0.5% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 4: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 0.7% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the bleaching powder (weight/volume percent) that adds discarded slurry volume 0.2% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in gypsum (weight/volume percent) the absorption discarded slurry of discarded slurry volume 2% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 5: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 0.5% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the bleaching powder (weight/volume percent) that adds discarded slurry volume 0.2% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in magnesia (weight/volume percent) the absorption discarded slurry of discarded slurry volume 2% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 6: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the technical hydrochloric acid (percent by volume) of discarded slurry volume 12% (31% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the bleaching powder (weight/volume percent) that adds discarded slurry volume 1% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in poly sodium metasilicate (weight/volume percent) the absorption discarded slurry of discarded slurry volume 11% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 7: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the industrial sulphuric acid (percent by volume) of discarded slurry volume 5% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the hydrogen peroxide (percent by volume) that adds discarded slurry volume 1% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in poly sodium metasilicate (percentage by weight) the absorption discarded slurry of discarded slurry volume 2% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 8: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 2.5% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 2.5% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in alum (weight/volume percent) the absorption discarded slurry of discarded slurry volume 12% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 9: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 2.5% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 2.5% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in gypsum (weight/volume percent) the absorption discarded slurry of discarded slurry volume 45% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 10: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the industrial ethanedioic acid (weight/volume percent) of discarded slurry volume 2.5% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 2.5% in stirring are removed or are reduced content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
C, add the moisture content in magnesia (weight/volume percent) the absorption discarded slurry of discarded slurry volume 15% in stirring, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 11: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add technical hydrochloric acid and the NaOH in the discarded slurry and the sodium carbonate of the industrial sulphuric acid (percent by volume), 0.5% (31% concentration) of discarded slurry volume 5% (98% concentration), the metal ion in the complexing mud;
B, the bleaching powder (weight/volume percent) that adds discarded slurry volume 0.2% in stirring, 1% clorox (weight/volume percent) is removed or reduce content of organics in the discarded slurry, reduces COD CrAnd colourity, remove the sulfide in the mud;
C, the alum (weight/volume percent) that adds discarded slurry volume 2% in stirring, the moisture content in 30% gypsum (weight/volume percent) the absorption discarded slurry, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant, form powdery or blocks of solid to exosmosis.
Embodiment 12: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in industrial ethanedioic acid (weight/volume percent), 0.8% (31% concentration) technical hydrochloric acid of discarded slurry volume 2% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the clorox (weight/volume percent) that adds discarded slurry volume 1% in stirring, 0.8% bleaching powder (weight/volume percent) is removed or reduce content of organics in the discarded slurry, reduces COD CrAnd colourity, remove the sulfide in the mud;
C, the aluminum sulfate (weight/volume percent) that adds discarded slurry volume 5% in stirring, the moisture content in 8% magnesia (weight/volume percent) the absorption discarded slurry, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant to exosmosis, form powdery or blocks of solid.
Embodiment 13: the step of the drilling well discarded slurry being carried out method for innocent treatment is as follows:
A, in mud pit, stir to add in the industrial sulphuric acid of industrial ethanedioic acid (weight/volume percent), 0.6% (98% concentration) of discarded slurry volume 1% (98% concentration) and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
B, the hydrogen peroxide (percent by volume) that adds discarded slurry volume 0.5% in stirring, 0.8% bleaching powder (percentage by weight) is removed or reduce content of organics in the discarded slurry, reduces COD CrAnd colourity, remove the sulfide in the mud;
C, the aluminum sulfate (weight/volume percent) that adds discarded slurry volume 6% in stirring, the moisture content in 6% poly sodium metasilicate (weight/volume percent) the absorption discarded slurry, destroy the emulsion balance of discarded slurry, change mud property, stop pollutant to exosmosis, form powdery or blocks of solid.

Claims (4)

1. treating waste mud of drilling well by harmless process, its concrete steps are as follows:
(1) in mud pit, stir to add in hydrochloric acid or sulfuric acid or the oxalic acid at least a industrial acids and NaOH and sodium carbonate in the discarded slurry, the metal ion in the complexing mud;
(2) add at least a oxidant in bleaching powder or hydrogen peroxide or the clorox in stirring and remove or reduce content of organics in the discarded slurry, reduce COD CrAnd colourity, remove the sulfide in the mud;
(3) add the moisture content at least a adsorbents adsorb discarded slurry in poly sodium metasilicate or aluminum sulfate or alum or land plaster or the magnesia in the stirring, the adhesive solidification discarded slurry stops pollutant to exosmosis, forms powdery or blocks of solid.
2. according to the said a kind for the treatment of waste mud of drilling well by harmless process of claim 1, it is characterized in that: the addition of said 31% technical hydrochloric acid is 0.5~12% of a percent by volume, the addition of 98% industrial sulphuric acid is that the addition of 0.5~8%, 98% industrial ethanedioic acid of percent by volume is 0.3~2.5% of a weight/volume percent.
3. according to the said a kind for the treatment of waste mud of drilling well by harmless process of claim 1, it is characterized in that: the addition of said bleaching powder is 0.2~1% of a weight/volume percent, the addition of hydrogen peroxide is 0.1~1% of a percent by volume, and the addition of clorox is 0.2~2.5% of a weight/volume percent.
4. according to the said a kind for the treatment of waste mud of drilling well by harmless process of claim 1, it is characterized in that: the addition of said aluminum sulfate is 0.5~15% of a weight/volume percent, the addition of poly sodium metasilicate is 2~11% of a weight/volume percent, the addition of alum is 0.5~12% of a weight/volume percent, the addition of gypsum is 2~45% of a weight/volume percent, and magnesian addition is 2~15% of a weight/volume percent.
CNB2006100220083A 2006-09-30 2006-09-30 Method for treating waste mud of drilling well by harmless process Active CN100418647C (en)