CN1706606A - Making process of wooden curtain blade with stereo surface grains - Google Patents

Making process of wooden curtain blade with stereo surface grains Download PDF

Info

Publication number
CN1706606A
CN1706606A CN 200510040011 CN200510040011A CN1706606A CN 1706606 A CN1706606 A CN 1706606A CN 200510040011 CN200510040011 CN 200510040011 CN 200510040011 A CN200510040011 A CN 200510040011A CN 1706606 A CN1706606 A CN 1706606A
Authority
CN
China
Prior art keywords
dimensional line
manufacture method
louver lamina
timber
wooden louver
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200510040011
Other languages
Chinese (zh)
Inventor
邹卫良
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HUATONG INDOOR DECORATION FABRIC CO Ltd CHANGSHU
Original Assignee
HUATONG INDOOR DECORATION FABRIC CO Ltd CHANGSHU
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HUATONG INDOOR DECORATION FABRIC CO Ltd CHANGSHU filed Critical HUATONG INDOOR DECORATION FABRIC CO Ltd CHANGSHU
Priority to CN 200510040011 priority Critical patent/CN1706606A/en
Publication of CN1706606A publication Critical patent/CN1706606A/en
Pending legal-status Critical Current

Abstract

The present invention belongs to the field of making process of special wooden product, and the making process of wooden curtain blade with stereo surface grains includes selecting timber, cutting, cutting into sheet, surface smoothening, forming stereo grains on the surface, coating to raise texture and painting. The present invention features connecting short timber to meet length requirement; adhering decorating paper with stereo grains onto the sheet to form stereo grains; and edging and chamfering of the sheet before coating and painting. The present invention can form beautiful wooden curtain blade.

Description

The surface has the manufacture method of the wooden louver lamina of three-dimensional line
Technical field
The invention belongs to the manufacture method of extraordinary woodwork, especially a kind of surface has the manufacture method of the wooden louver lamina of three-dimensional line.
Background technology
In the manufacture method of the disclosed louver lamina surface three-dimensional of Chinese patent Granted publication CN1112986c wood grain, the background that forms this patented technology scheme is done detailed narration, promptly the existing disadvantage of the louver lamina in the prior art has been done objective analysis, evaluation.The one, pointed out to show that decorative pattern, the pattern on the louver lamina shows as plane decorative pattern, pattern, cause style appearance sharp keen, extremely pull and lose aesthetic feeling, and can produce and the inharmonic sensation of interior space layout; The 2nd, pointed out that plastic cement or PU foaming blade can cause second environmental pollution in discarded back, and also can't incorporate general indoor layout for people's visual effect, not durable easily aging distortion because of not perishable; The 3rd, analyzed people and liked with the reason of wood materials as louver lamina, but point out simultaneously, because blade surface is level and smooth plane, so texture, aesthetic feeling are reduced significantly, though can be at its surface engraving three-dimensional pattern, can spend a large amount of human and material resources, time and uneconomical.
In view of this, CN1112986C has visualized a unique technical proposal that is intended to overcome aforementioned disadvantages, according to the instruction of this patented technology scheme, can make decorative pattern on the wooden blade have various variation, show outstanding aesthetic feeling, texture, saving human and material resources, improve working (machining) efficiency.But the applicant finds to have following shortcoming: the one, and method had not both directly instructed people how to save timber to greatest extent, did not allow people be realized the enlightenment that how reasonably or dexterously utilizes timber yet.Because timber is a kind of resource of preciousness, as wooden product production industry, saving timber resources is a factor that can not be ignored, otherwise can cause unreasonable waste and increase production cost to resource.For example, when will be with the curtain sheet of a collection of scale (custom claim fixed sign indicating number) timber processing Len req, the length of timber general unlikely rightly with the desired curtain leaf length of people or consistent with the length multiple of curtain sheet, therefore tend to occur remaining timber part.Even this remaining timber part (custom claims stub segment on the industry) can also be used to process curtain sheet in a narrow margin, so equally also can exist and can't avoid nubbin, because in the processing of reality, often require material peaceful long not short.Also have, self parameter of timber is more, for example: when certain root timber exists two ends to conform to quality requirements, when yet there are blemishes in the middle part, if then can bring disaster to the use length at two ends when rejecting the middle part, if not rejecting then to influence product quality, often cause the waste of all houses of a house thus in order to ensure product quality; The 2nd, to material alternative condition harshness, as described in its specification, select timber kind according to required wood grain, and done more detailed explaining, select in the timber kind step: need the wood grain of blade (curtain sheet) to select the torrid zone, subtropical zone or level land tree growing at least, otherwise then select frigid zone or high mountain tree growing; The 3rd, many, the artificial consumption of complex process, equipment input is big, as enlightenment by its specification, rectangular thin slice is formed the blasting treatment of wood grain with sand-blasting machine, before sandblast, stick the stencil paper of different pattern prior to blade surface, the stencil paper place forms the decorative pattern of some protrusions so that be sticked on the blade, after sandblast finishes, remove stencil paper; The 4th, because there is unavoidable aberration in timber itself, even therefore the step 5 of introducing by this patented method is carried out application, japanning is handled and still can't be covered aberration, and it is influenced to cause aesthetic feeling, the texture of curtain sheet exactly because of the existence of aberration.
Summary of the invention
Task of the present invention be to provide a kind of and embody the convenience of making the best use of everything, embodying selection to select common timber commonly used for use to save timber effectively, with the simple and saving equipment input of technology and save the surface of consuming artificial amount, demonstrating fully aesthetic feeling and texture with effective color difference eliminating and have the manufacture method of the wooden louver lamina of three-dimensional line.
Task of the present invention is finished like this, a kind of surface has the manufacture method of the wooden louver lamina of three-dimensional line, it comprise select timber, severing, open laminate, to the bright and clean processing of sheet surface, the sheet surface after the bright and clean processing is given three-dimensional line, is used the application, the japanning that increase finished product aesthetic feeling and texture then and handle, characteristics are: through severing, short material to discontented foot length degree carries out finger, opens the strip thin slice of making the required form size again; It is described that to give three-dimensional line be two surfaces that the three-dimensional decorative pattern facial tissue that will have relief wood grain pastes thin slice; Before handling the thin slice after pasting three-dimensional decorative pattern facial tissue is being carried out deburring, chamfered prior to described application, japanning.
Finger of the present invention is that the material that does not satisfy Len req that will occur because of the rejecting flaw in the severing process is engaged with each other.
Finger of the present invention is that the material that will cut out the surplus residue remnant in the severing process is engaged with each other.
Joint of the present invention is to dock with interdigital form between the material.
Joint of the present invention is to dock with the tenon form between the material.
Timber of the present invention is cheap timber.
Cheap timber of the present invention is pine.
Pine of the present invention is any one in pinus sylvestris var. mongolica, Korean pine, the kahikatea.
Stickup of the present invention is that adhesive is pasted, and adhesive is coated on the thin slice.
Adhesive of the present invention is avirulent strong adhesive, and its proportion is 1, PH is 4.5, solid content is 49%, viscosity is 25000cps.
Compared with the prior art said method disclosed by the invention has following strong point: 1. can save timber by finger, demonstrate fully and make the best use of everything; 2. owing to the strong three-dimensional decorative pattern facial tissue of third dimension with wood grain is the wide in range product of easily purchasing of selectivity on the market, it is pasted on the thin slice as curtain blade pioneeringly, can make the fastidious property of the raw material selection of thin slice is able to amiableization; 3. need not drop in addition and be intended to for form protruding the special equipment of decorative pattern, pattern on the thin slice, have that technology is easy, the equipment less investment, save artificial, working (machining) efficiency is high; 4. because what adopt is to paste the decorations means, there is not the sorrow of tedious goods aberration, the aesthetic feeling and the texture that blade table is revealed cause to the greatest extent.
Description of drawings
Fig. 1 is the flow diagram of the inventive method.
Fig. 2 is the described finger schematic diagram of the inventive method.
Fig. 3 is the partial structurtes stereogram of the resulting product of the inventive method.
Fig. 4 is by the resulting wooden louver lamina schematic diagram of finger wood shown in Figure 2.
The specific embodiment
Obtain by Fig. 3, product shown in Figure 4 by step shown in Figure 1.
The first step: pinus sylvestris var. mongolica that buy from market and after super-dry is handled is carried out severing, and general severing becomes square bar, and the shape of square bar is by shown in Figure 2, exists the part of oil sac to clip on material when severing, promptly rejects the oil sac part;
Second step: the square bar that cutting into two exact halves has no progeny meets length is directly opened by the multi-disc machine and is laminated 1, and the square bar that can not reach Len req is carried out finger, the concrete mode of finger adopts woodwork processing industry interdigital joint commonly used or the indented joint mode as shown in Figure 2 that joggle closes or other similarly is easy to know by inference to engage, used equipment is the air-pump type finger joint machine in the joint technology, this finger joint machine also is the habitual and woodworking machinery equipment that generally all have of woodwork processing industry, dip in the glue finger, or brush coating finger, the pinus sylvestris var. mongolica that is used for finger is not limited only to the odd pinus sylvestris var. mongolica of this batch severing, can also be with the previous surplus remnant of using, thereby can grasp flexibly, use to demonstrate fully and make the best use of everything and save timber resources to greatest extent;
The 3rd step: wooden the opening with the multi-disc machine of camphor tree behind finger laminated 1, and the thickness of thin slice 1 is decided according to needing;
The 4th step: reach polishing all around and, make the surface of thin slice 1 reach slippery, clean to the wood chip cleaning with the surface of polishing machine to thin slice 1;
The 5th step: the three-dimensional decorative pattern facial tissue of buying on the market 2 with relief wood grain 21 is pasted on the both side surface of thin slice 1, specifically be to adopt gluing-labelling machine of commonly using in the furniture production industry to finish, the limit is applied to adhesive by glue spreader the both sides of thin slice 1, the limit is pasted by Sticking roller, wherein: adhesive adopts the cohesive force of the no any toxicity meet FDA (U.S. food and medicine association) clause 21CFR175.105 strong and have an adhesive of good waterproof effect, for example adopting the product type by the production and sales of Changshu, Chinese Jiangsu adhesive Co., Ltd is the BFRNF5# adhesive, and the proportion of this adhesive is 1, PH is 4.5, solid content is 49%, viscosity is 25000cps (surface viscosity: centipoise<international unit 〉);
The 6th step: carry out deburring, chamfered, so-called deburring is to exceed the surplus paper of the surface range of thin slice 1 when pasting to repair and remove, so-called chamfering is four week formation camber abgles with thin slice 1, so both be beneficial to attractive in appearance, be beneficial to again the protection three-dimensional decorative pattern facial tissue 2 occur in the bight of thin slice 1 alice, the shelling and so on situation;
The 7th step: the lateral margin japanning that the both sides of thin slice 1 promptly is not pasted with three-dimensional decorative pattern facial tissue 2, japanning is advisable with thin slice 1 whole folded japanning, and the lacquer look should be consistent with the color of the three-dimensional decorative pattern facial tissue 2 of paste, if in order to keep on improving, so, also can impose wiping, waxing to lacquer painting.
Can embody a three-dimensional line that mixes as day become in the surface that obtains of step in one's power by the foregoing description by Fig. 3, wooden louver lamina shown in Figure 4.Though the present invention has only exemplified employing appearance pine, be not difficult to know by inference identical reason with Korean pine, kahikatea.In addition, as long as Fig. 3, the three-dimensional decorative pattern facial tissue 2 with relief wood grain 21 shown in Figure 4 are changed, just can be according to the wooden louver lamina of the three-dimensional line that needs the acquisition different-style.

Claims (10)

1, a kind of surface has the manufacture method of the wooden louver lamina of three-dimensional line, it comprise select timber, severing, open laminate, to the bright and clean processing of sheet surface, the sheet surface after the bright and clean processing is given three-dimensional line, is used the application, the japanning that increase finished product aesthetic feeling and texture then and handle, it is characterized in that through severing, short material to discontented foot length degree carries out finger, opens the strip thin slice of making the required form size again; It is described that to give three-dimensional line be two surfaces that the three-dimensional decorative pattern facial tissue that will have relief wood grain pastes thin slice; Before handling the thin slice after pasting three-dimensional decorative pattern facial tissue is being carried out deburring, chamfered prior to described application, japanning.
2, surface according to claim 1 has the manufacture method of the wooden louver lamina of three-dimensional line, it is characterized in that described finger is that the material that does not satisfy Len req that will occur because of the rejecting flaw in the severing process is engaged with each other.
3, surface according to claim 1 has the manufacture method of the wooden louver lamina of three-dimensional line, it is characterized in that described finger is that the material that will cut out the surplus residue remnant in the severing process is engaged with each other.
4, have the manufacture method of the wooden louver lamina of three-dimensional line according to claim 2 or 3 described surfaces, it is characterized in that described joint is to dock with interdigital form between the material.
5, have the manufacture method of the wooden louver lamina of three-dimensional line according to claim 2 or 3 described surfaces, it is characterized in that described joint is to dock with the tenon form between the material.
6, surface according to claim 1 has the manufacture method of the wooden louver lamina of three-dimensional line, it is characterized in that described timber is cheap timber.
7, surface according to claim 6 has the manufacture method of the wooden louver lamina of three-dimensional line, it is characterized in that described cheap timber is pine.
8, surface according to claim 7 has the manufacture method of the wooden louver lamina of three-dimensional line, it is characterized in that described pine is any one in pinus sylvestris var. mongolica, Korean pine, the kahikatea.
9, surface according to claim 1 has the manufacture method of the wooden louver lamina of three-dimensional line, it is characterized in that described stickup is that adhesive is pasted, and adhesive is coated on the thin slice.
10, surface according to claim 9 has the manufacture method of the wooden louver lamina of three-dimensional line, it is characterized in that described adhesive is avirulent powerful binder, and its proportion is 1, PH is 4.5, solid content is 49%, viscosity is 25000cps.
CN 200510040011 2005-05-12 2005-05-12 Making process of wooden curtain blade with stereo surface grains Pending CN1706606A (en)