CN1693409A - 高渗透密闭液的制作方法 - Google Patents

高渗透密闭液的制作方法 Download PDF

Info

Publication number
CN1693409A
CN1693409A CN 200510043323 CN200510043323A CN1693409A CN 1693409 A CN1693409 A CN 1693409A CN 200510043323 CN200510043323 CN 200510043323 CN 200510043323 A CN200510043323 A CN 200510043323A CN 1693409 A CN1693409 A CN 1693409A
Authority
CN
China
Prior art keywords
resin
agent
sealing liquid
high penetrating
penetrating sealing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200510043323
Other languages
English (en)
Inventor
宿官礼
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200510043323 priority Critical patent/CN1693409A/zh
Publication of CN1693409A publication Critical patent/CN1693409A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种用于石油勘探开发中钻井密闭取心使用的密闭液的制作方法。本发明的技术方案的原料组成包括增塑剂、树脂、封堵剂、乳化剂组成,并按50~80∶3~20∶10~40∶5~18的重量配比。其中:增塑剂是邻苯二甲酸二酯,树脂是聚乙烯或聚氯乙烯树脂,封堵剂是碳酸钙、有机土、磺化沥青或油溶性树脂,乳化剂是固体乳化剂。制备方法是,在60℃~170℃温度下使树脂均匀溶解在原材料增塑剂中;然后依次将封堵剂、乳化剂均匀分散其中,即得密闭液。本发明与现有技术相比有以下优点:具有原材料来源广泛、产品性能稳定、贮存期较长,抗温性好,温度范围-27℃~170℃、取心井段较深、无毒、密闭效果好等优点。

Description

高渗透密闭液的制作方法
一、技术领域
本发明涉及一种用于石油勘探开发中钻井密闭取心使用的密闭液的制作方法。
二、背景技术
中国专利《高效密闭液》(专利申请号93119352)是采用原油中的稠油作为基本原料,在常温下加入硫酸磺化搅拌均匀而成,使用该密闭液取心给油饱和度的测定及油气显示测井解释会有影响,温度升高到100℃后密闭液粘度较低,对于高渗透或有较大缝隙的地层取心密闭效果变差。
三、发明内容:
本发明是针对现有的高效密闭液存在的上述缺陷,提供一种高渗透密闭液的制作方法。
本发明的技术方案的原料组成包括增塑剂、树脂、封堵剂、乳化剂组成,并按50~80∶3~20∶10~40∶5~18的重量配比。其中:增塑剂是邻苯二甲酸二酯,树脂是聚乙烯或聚氯乙烯树脂,封堵剂是碳酸钙、有机土、磺化沥青或油溶性树脂,乳化剂是固体乳化剂。
制备方法是,在60℃~170℃温度下使树脂均匀溶解在原材料增塑剂中;然后依次将封堵剂、乳化剂均匀分散其中,即得密闭液。
本发明与现有技术相比有以下优点:具有原材料来源广泛、产品性能稳定、贮存期较长,抗温性好,温度范围-27℃~170℃、取心井段较深、无毒、密闭效果好等优点。
四、附图说明:无。
五、具体实施方式
将邻苯二甲酸二酯70千克加入到反应釜中,将其均匀加热到120℃后,边搅拌边将10千克聚乙烯或聚氯乙烯树脂均匀加入其中,继续保持120℃温度下搅拌6小时,使树脂均匀溶解在邻苯二甲酸二酯中;然后停止加热,在继续搅拌的情况下,依次均匀加入25千克封堵剂(碳酸钙、有机土、磺化沥青或油溶性树脂的一种)、12千克固体乳化剂搅拌后制得密闭液。

Claims (2)

1、一种高渗透密闭液的制作方法,其特征是:原料组成包括增塑剂、树脂、封堵剂、乳化剂组成,并按50~80∶3~20∶10~40∶5~18的重量配比,在60℃~170℃温度下使树脂均匀溶解在原材料增塑剂中;然后依次将封堵剂、乳化剂均匀分散其中,即得密闭液。
2、根据权利要求1所述的高渗透密闭液的制作方法,其特征是所述的:增塑剂是邻苯二甲酸二酯,树脂是聚乙烯或聚氯乙烯树脂,封堵剂是碳酸钙、有机土、磺化沥青或油溶性树脂,乳化剂是固体乳化剂。
CN 200510043323 2005-04-14 2005-04-14 高渗透密闭液的制作方法 Pending CN1693409A (zh)